# US 2003/0203604 A1 · Methods of fabricating layered structure and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0203604 A1
- Document ID: US20030203604A1
- Status: Published application
- Kind: A1
- Application number: 10/400,378
- Filed: 2003-04-01
- Published: 2003-10-30
- Earliest claimed: 2002-04-26
- Assignees: Oki Electric Industry Co., Ltd.
- Inventors: Takehiko Makita
- Web page: https://patentgrep.com/patent/US20030203604A1

## CPC

- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3256: {Microstructure}
- H10P 14/3416: {Nitrides}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a layered structure including a substrate, a first semiconductor layer with a first thermal expansion coefficient αA, and a second semiconductor layer with a second thermal expansion coefficient αB deposited on the first semiconductor layer, wherein αA is greater than αB or smaller than αB, includes: forming the first semiconductor layer, the second semiconductor layer, and a third semiconductor layer with a third thermal expansion coefficient αC in this order on the substrate at a first temperature using a film deposition technique such as MOCVD, thereby forming a structural body including the substrate and the first to third semiconductor layers, wherein αC is greater than αB if αA is greater than αB or αC is smaller than αB if αA is smaller than αB; cooling the structural body to a second temperature, which is lower than the first temperature; and removing the third semiconductor layer from the structural body to expose the second semiconductor layer.

## Claims

### Claim 1

A method of fabricating a layered structure including a substrate, a first semiconductor layer with a first thermal expansion coefficient αA, and a second semiconductor layer with a second thermal expansion coefficient αB deposited on the first semiconductor layer, wherein αA is greater than αB or smaller than αB, said method comprising:
forming the first semiconductor layer, the second semiconductor layer, and a third semiconductor layer with a third thermal expansion coefficient ac in this order on the substrate at a first temperature using a film deposition technique, thereby forming a structural body including the substrate and the first to third semiconductor layers, wherein ac is greater than αB if αA is greater than αB or αC is smaller than αB if αA is smaller than αB;
cooling the structural body to a second temperature, which is lower than the first temperature; and
removing the third semiconductor layer from the structural body to expose the second semiconductor layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the film deposition technique is metal-organic chemical vapor deposition.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising:
forming a buffer layer on the substrate before said forming step of the first semiconductor layer so that the first semiconductor layer is formed on the buffer layer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the third semiconductor layer is made of the same material as the first semiconductor layer.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the first semiconductor layer and the third semiconductor layer are made of GaN, and the second semiconductor layer is made of AlxGa1−xN, where 0<x<1.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the first temperature is within a range of 950° C. to 1150° C. inclusive.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the second temperature is a temperature at which vaporization of atoms of the third semiconductor layer from a surface of the third semiconductor layer stops.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said removing step of the third semiconductor layer is performed using dry etching.

### Claim 9

A method of fabricating a semiconductor device including a layered structure, which includes a substrate, a first semiconductor layer with a first thermal expansion coefficient αA, and a second semiconductor layer with a second thermal expansion coefficient αB deposited on the first semiconductor layer, wherein αA is greater than αB or smaller than αB, said method comprising:
forming the first semiconductor layer, the second semiconductor layer, and a third semiconductor layer with a third thermal expansion coefficient ac in this order on the substrate at a first temperature using a film deposition technique, thereby forming a structural body including the substrate and the first to third semiconductor layers, wherein ac is greater than αB if αA is greater than αB or αC is smaller than αB if αA is smaller than αB;
cooling the structural body to a second temperature, which is lower than the first temperature; and
removing the third semiconductor layer from the structural body to expose the second semiconductor layer.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the film deposition technique is metal-organic chemical vapor deposition.

### Claim 11 (depends on 9)

The method according to claim 9, further comprising:
forming a buffer layer on the substrate before said forming step of the first semiconductor layer so that the first semiconductor layer is formed on the buffer layer.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the third semiconductor layer is made of the same material as the first semiconductor layer.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the first semiconductor layer and the third semiconductor layer are made of GaN, and the second semiconductor layer is made of AlxGa1−xN, where 0<x<1.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the first temperature is within a range of 950° C. to 1150° C. inclusive.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the second temperature is a temperature at which vaporization of atoms of the third semiconductor layer from a surface of the third semiconductor layer stops.

### Claim 16 (depends on 9)

The method according to claim 9, wherein said removing step of the third semiconductor layer is performed using dry etching.

### Claim 17 (depends on 9)

The method according to claim 9, further comprising:
forming a control electrode, a first main electrode, and a second main electrode on the exposed surface of the second semiconductor layer.

### Claim 18 (depends on 9)

The method according to claim 9, further comprising:
forming an insulating layer on the exposed surface of the second semiconductor layer;
forming a control electrode on the insulating layer;
removing a part of the insulating layer to expose a part of the second semiconductor layer; and
forming a first main electrode and a second main electrode on the exposed surface of the second semiconductor layer.

### Claim 19 (depends on 9)

The method according to claim 9, wherein said removing step of the third semiconductor layer is performed so as to remove a part of the third semiconductor layer;
said method further comprising:
forming a first main electrode and a second main electrode on the third semiconductor layer before said removing step of the third semiconductor layer; and
forming a control electrode on the exposed surface of the second semiconductor layer after said removing step of the third semiconductor layer.