# US 2003/0203573 A1 · Semiconductor device including trench with at least one of an edge of an opening and a bottom surface being round

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0203573 A1
- Document ID: US20030203573A1
- Status: Published application
- Kind: A1
- Application number: 10/436,084
- Filed: 2003-05-13
- Published: 2003-10-30
- Earliest claimed: 1994-02-04
- Assignees: Mitsubishi Denki Kabushiki Kaisha
- Inventors: Katsumi Nakamura; Tadaharu Minato; Shuuichi Tominaga; Katsuomi Shiozawa
- Web page: https://patentgrep.com/patent/US20030203573A1

## CPC

- H10D 30/657: {having substrates comprising insulating layers, e.g. SOI-LDMOS transistors}
- H10D 12/01: Manufacture or treatment
- H10D 12/021: {of gated diodes, e.g. field-controlled diodes [FCD]}
- H10D 12/038: {having a recessed gate, e.g. trench-gate IGBTs}
- H10D 12/211: {Gated diodes}
- H10D 12/421: {on insulating layers or insulating substrates, e.g. thin-film IGBTs}
- H10D 12/481: {having gate structures on slanted surfaces, on vertical surfaces, or in grooves, e.g. trench gate IGBTs}
- H10D 18/655: {produced by insulated gate structures}
- H10D 30/025: {of vertical IGFETs (of VDMOS H10D30/0291; of vertical TFTs H10D30/0318)}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/63: Vertical IGFETs (H10D30/66 {, H10D30/6728, H10D30/689, H10D30/693} take precedence)
- H10D 30/64: Double-diffused metal-oxide semiconductor [DMOS] FETs
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/127: {of cellular field-effect devices, e.g. multicellular DMOS transistors or IGBTs}
- H10D 64/513: {within recesses in the substrate, e.g. trench gates, groove gates or buried gates}
- H10D 84/0105: {the built-in components being field-effect devices}
- H10P 90/1906: {Preparing SOI wafers}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/041: {of isolation regions comprising polycrystalline semiconductor materials}
- H10W 10/061: {using SOI processes together with lateral isolation, e.g. combinations of SOI and shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10W 10/40: Isolation regions comprising polycrystalline semiconductor materials
- H10D 62/8325: {Silicon carbide}
- H10D 64/516: {the thicknesses being non-uniform}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

There is disclosed a method of fabricating a semiconductor device which includes the steps of forming a trench (4), and repeating the formation and removal of an oxide film (a sacrificial oxide film) twice to provide a rounded configuration (5b) of an opening portion of the trench (4) and a rounded configuration (6b) of a bottom thereof and to draw defects in a semiconductor layer into a silicon oxide film (8), reducing the defects adjacent the inner wall of the trench (4), whereby electric field concentration on a gate is prevented and the mobility of carriers in channels is improved for an improvement in characteristic, particularly an on-state voltage, of a power device. (FIG. 5)

## Claims

### Claim 1

A method of fabricating a semiconductor device, comprising the steps of:
(a) anisotropically etching a substrate made of semiconductor to form a trench extending in a direction of the thickness of said substrate;
(b) performing a first thermal oxidation to form a first sacrificial oxide film in said trench;
(c) removing said first sacrificial oxide film;
(d) performing a second thermal oxidation to form a second sacrificial oxide film in said trench after said step (c);
(e) removing said second sacrificial oxide film;
(f) forming an insulating film comprising a part of a control electrode in said trench after said step (e); and
(g) filling said trench to form said control electrode opposed to said substrate through said insulating film comprising said part of said control electrode.

### Claim 2 (depends on 1)

The method of claim 1, wherein
said second thermal oxidation is performed in a water-containing atmosphere, and
said first thermal oxidation is performed at a first temperature higher than a second temperature at which said second thermal oxidation is performed.

### Claim 3 (depends on 2)

The method of claim 2, wherein
said first temperature is not less than 1000° C.

### Claim 4

A method of fabricating a semiconductor device, comprising the steps of:
(a) anisotropically etching a substrate made of semiconductor to form a trench having an aspect ratio of from 2 to 30 and extending in a direction of the thickness of said substrate;
(b) performing a thermal oxidation in an atmosphere of oxygen at a temperature not less than 1000° C. to form in said trench a sacrificial oxide film having a thickness one-tenth to three-tenths the size of an opening portion of said trench;
(c) removing said sacrificial oxide film;
(d) forming an insulating film comprising a part of a control electrode in said trench after said step (c); and
(e) filling said trench to form said control electrode opposed to said substrate through said insulating film comprising said part of said control electrode.

### Claim 5

A method of fabricating a semiconductor device, comprising the steps of:
(a) anisotropically etching a substrate made of semiconductor to form a trench extending in a direction of the thickness of said substrate;
(b) performing a thermal oxidation to form a sacrificial oxide film in said trench;
(c) removing said sacrificial oxide film;
(d) oxidizing an inside of said trench at an atmosphere of oxygen at a temperature not less than 1000° C. to form an insulating film comprising a part of a control electrode after said step (c); and
(e) filling said trench to form said control electrode opposed to said substrate through said insulating film comprising said part of said control electrode.

### Claim 6 (depends on 5)

The method of claim 5, wherein
said thermal oxidation in said step (b) is performed in an atmosphere of oxygen at a temperature ranging from 950 to 1100° C.

### Claim 7

A method of fabricating a semiconductor device, comprising the steps of:
(a) anisotropically etching a substrate made of semiconductor to form a trench extending in a direction of the thickness of said substrate;
(b) providing on said substrate a mask having an edge backing away a predetermined distance from an opening portion of said trench;
(c) performing an isotropic dry etching on said substrate by using said mask;
(d) oxidizing an inside of said trench in an atmosphere of steam at a temperature not more than 1000° C. after said step (c); and
(e) filling said trench to form a control electrode opposed to said substrate through said insulating film comprising a part of said control electrode.

### Claim 8 (depends on 7)

The method of claim 7, wherein
said distance is 100 to 400 nm.

### Claim 9 (depends on 7)

The method of claim 7, wherein
said isotropic dry etching is performed by using an O2/CF4 based gas, and a ratio R=O2/CF4 of the gas satisfies 1<R<5.

### Claim 10 (depends on 7)

The method of claim 7, further comprising the steps of:
(f) performing a thermal oxidation to form a sacrificial oxide film in said trench; and
(g) removing said sacrificial oxide film,
said steps (f) and (g) being performed after said step (c) and before said step (d).

### Claim 11 (depends on 10)

The method of claim 10, wherein
said thermal oxidation in said step (f) is performed in an atmosphere of oxygen at a temperature ranging from 950 to 1100° C.

### Claim 12

A method of fabricating a semiconductor device, comprising the steps of:
(a) providing a semiconductor layer on a substrate including an insulating film at least on its surface;
(b) anisotropically etching said semiconductor layer to form a trench extending in a direction of the thickness of said semiconductor layer;
(c) performing a thermal oxidation to form a sacrificial oxide film in said trench;
(d) removing a part of said substrate which lies under said trench and said sacrificial oxide film;
(e) oxidizing an inside of said trench in an atmosphere of oxygen at a temperature not less than 1000° C. to form an isolation oxide film after said step (d); and
(f) filling said trench with a burying material.

### Claim 13

A method of fabricating a semiconductor device, comprising the steps of:
(a) providing a semiconductor layer on a substrate including an insulating film at least on its surface;
(b) anisotropically etching said semiconductor layer to form a trench extending in a direction of the thickness of said semiconductor layer;
(c) removing a predetermined distance of a part of said insulating film on said substrate which lies under said trench to form a recess having a diameter greater than a diameter of said trench;
(d) performing an isotropic dry etching on said semiconductor layer;
(e) oxidizing an inside of said trench in an atmosphere of steam at a temperature not more than 1000° C. to form an isolation oxide film after said step (d); and
(f) filling said trench with a burying material.

### Claim 14 (depends on 13)

The method of claim 13, wherein
an isotropic etching of an oxide film is used in said step (c).

### Claim 15 (depends on 13)

The method of claim 13, wherein
said predetermined distance is 100 to 400 nm.

### Claim 16 (depends on 13)

The method of claim 13, wherein
said isotropic dry etching is performed by using an O2/CF4 based gas, and a ratio R=O2/CF4 of the gas satisfies 1<R<5.

### Claim 17 (depends on 13)

The method of claim 13, further comprising the steps of:
(g) performing a thermal oxidation to form a sacrificial oxide film in said trench; and
(h) removing said sacrificial oxide film,
said steps (g) and (h) being performed after said step (d) and before said step (e).

### Claim 18 (depends on 17)

The method of claim 17, wherein
said thermal oxidation in said step (g) is performed in an atmosphere of oxygen at a temperature ranging from 950 to 1100° C.

### Claim 19

A method of fabricating a semiconductor device, comprising the steps of:
(a) providing a semiconductor layer on a substrate including an insulating film at least on its surface;
(b) anisotropically etching said semiconductor layer to form a trench extending in a direction of the thickness of said semiconductor layer;
(c) performing a thermal oxidation to form a sacrificial oxide film in said trench;
(d) removing a part of said substrate which lies under said trench and said sacrificial oxide film;
(e) forming a polycrystalline semiconductor layer on an inner wall of said trench;
(f) oxidizing said polycrystalline semiconductor layer to form an isolation oxide film; and
(g) filling said trench with a burying material.

### Claim 20

A method of fabricating a semiconductor device, comprising the steps of:
(a) providing a semiconductor layer on a substrate including a semiconductor oxide film;
(b) anisotropically etching said semiconductor layer to form a trench having an aspect ratio of from 2 to 30 and extending in a direction of the thickness of said semiconductor layer;
(c) performing a thermal oxidation in an atmosphere of oxygen at a temperature not less than 1000° C. to form in said trench a sacrificial oxide film having a thickness one-tenth to three-tenths the size of an opening portion of said trench;
(d) removing said sacrificial oxide film;
(e) forming an isolation oxide film in said trench after said step (c); and
(f) filling said trench with a burying material.