# US 2003/0201038 A1 · Methods of manufacturing hot-dip galvanized hot-rolled and cold-rolled steel sheets excellent in strain age hardening property

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0201038 A1
- Document ID: US20030201038A1
- Status: Published application
- Kind: A1
- Application number: 10/428,881
- Filed: 2003-05-02
- Published: 2003-10-30
- Earliest claimed: 2000-04-07
- Assignees: Kawasaki Steel Corporation, a corporation of Japan
- Inventors: Saiji Matsuoka; Tetsuo Shimizu; Kei Sakata; Osamu Furukimi
- Web page: https://patentgrep.com/patent/US20030201038A1

## CPC

- C22C 38/16: containing copper
- C21D 8/0226: {Hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/40: Plates; Strips
- C21D 1/185: {from an intercritical temperature}
- C21D 8/0236: {Cold rolling}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- Y10T 428/12799: Next to Fe-base component [e.g., galvanized]
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a steel sheet having a chemical composition comprising 0.15% or less C, 2.0% or less Si, 3.0% or less Mn, P, S, Al and N in adjusted amounts, from 0.5 to 3.0% Cu, or one or more of Cr, Mo and W in a total amount of 2.0% or less, and having a composite structure comprising ferrite and martensite having an area ratio of 2% or more. The steel sheet is in the form of a high-strength hot-rolled steel sheet, a high-strength cold-rolled steel sheet, or a hot-dip galvanized steel sheet. There is thus available a steel sheet excellent in press-formability and in strain age hardening property as represented by a ΔTS of 80 MPa or more.

## Claims

### Claim 1

A steel sheet excellent in press-formability and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more, comprising a structure having ferrite phase as a main phase forming a composite structure with a secondary phase containing martensite phase in an area ratio of 2% or more.

### Claim 2 (depends on 1)

A steel sheet according to claim 1, which is a hot-rolled steel sheet.

### Claim 3 (depends on 2)

A steel sheet according to claim 2, comprising, in weight percentage:
19 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less, Cu: from 0.5 to 3.0%,
and the balance Fe and incidental impurities.

### Claim 4 (depends on 3)

A steel sheet according to claim 3, containing, in weight percentage, one or more selected from the following groups A to C, in addition to the above-mentioned chemical composition:
group A: Ni: 2.0% or less;
group B: one or two of Cr and Mo: 2.0% or less in total; and
group C: one or more of Nb, Ti and V: 0.2% or less in total.

### Claim 5 (depends on 2)

A steel sheet according to claim 2, having a chemical composition comprising, in weight percentage:
20 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02%, or less Al: 0.1% or less, N: 0.02% or less,
one or more selected from the group consisting of from 0.05 to 2.0% Mo, from 0.05 to 2.0% Cr and from 0.05 to 2.0% W, 2.0% or less in total, and the balance Fe and incidental impurities.

### Claim 6 (depends on 5)

A steel sheet according to claim 5, further comprising, in addition to the above-mentioned chemical composition, in weight percentage, one or more selected from the group consisting of Nb, Ti, and V, 2.0% or less in total.

### Claim 7

A manufacturing method of a steel sheet excellent in press-formability and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more, comprising the steps, when hot-rolling a steel slab having a chemical composition comprising, in weight percentage:
21 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less, and Cu: from 0.5 to 3.0%,
into a hot-rolled steel sheet having a prescribed thickness, carrying out said hot rolling with a finish rolling end temperature FDT of the Ar3 transformation point or more, then after the completion of the finish rolling, cooling the hot-rolled steel sheet to a temperature region from the (Ar3 transformation point) to the (Ar1 transformation point) at a cooling rate of 5° C./second or more, air-cooling or slowly cooling the sheet within said temperature region for a period of from 1 to 20 seconds, then cooling the sheet again at a cooling rate of 5° C./second or more, and coiling the sheet at a temperature of 550° C. or below.

### Claim 8 (depends on 7)

A manufacturing method of a hot-rolled steel sheet according to claim 7, containing, in addition to said chemical composition in weight percentage, one or more selected from the following groups A to C:
group A: Ni: 2.0% or less;
group B: one or two of Cr and Mo: 2.0% or less in total; and
group C: one or more of Nb, Ti and V: 0.2% or less in total.

### Claim 9 (depends on 7)

A manufacturing method of a hot-rolled steel sheet, according to claim 7, wherein said steel slab has a chemical composition containing, in weight percentage:
22 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less,
and further containing one or more selected from the group consisting of from 0.05 to 2.0% Mo, from 0.05 to 2.0% Cr, and from 0.05 to 2.0% W, 2.0% or less in total.

### Claim 10 (depends on 7, 8, 9)

A manufacturing method of a hot-rolled steel sheet according to any one of claims 7 to 9, wherein all or part of said finish rolling comprises lubrication rolling.

### Claim 11 (depends on 1)

A steel sheet according to claim 1, which is a cold-rolled steel sheet.

### Claim 12 (depends on 11)

A steel sheet according to claim 11, comprising, in weight percentage:
23 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less, Cu: from 0.5 to 3.0%,
and the balance Fe and incidental impurities.

### Claim 13 (depends on 12)

A steel sheet according to claim 12, containing, in weight percentage, one or more selected from the following groups A to C, in addition to the above-mentioned chemical composition:
group: Ni: 2.0% or less;
group B: one or two of Cr and Mo: 2.0% or less in total; and
group C: one or more of Nb, Ti and V: 0.2% or less in total.

### Claim 14 (depends on 11)

A steel sheet according to claim 11, having a chemical composition comprising, in weight percentage:
24 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less,
one or more selected from the group consisting of from 0.05 to 2.0% Mo, from 0.05 to 2.0% Cr and from 0.05 to 2.0% W, 2.0% or less in total, and the balance Fe and incidental impurities.

### Claim 15 (depends on 14)

A steel sheet according to claim 14, further comprising, in addition to the above-mentioned chemical composition, in weight percentage, one or more selected from the group consisting of Nb, Ti and V, 2.0% or less in total.

### Claim 16

A manufacturing method of a cold-rolled steel sheet excellent in press-formability and in strain age hardening property typically represented by a ΔTS of 80 MPa or more, comprising the steps of using a steel slab having a chemical composition containing, in weight percentage:
25 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less, and Cu: from 0.5 to 3.0%
as a material; a hot rolling step of applying hot rolling to said material into a hot-rolled steel sheet; a cold rolling step of applying cold rolling to said hot-rolled steel sheet into a cold-rolled steel sheet; and a recrystallization annealing step of applying recrystallization annealing into a cold-rolled annealed steel sheet; these steps being sequentially applied; wherein said recrystallization annealing is conducted in a ferrite+austenite dual phase region within a temperature range of from Ac1 transformation point to Ac3 transformation point.

### Claim 17 (depends on 16)

A manufacturing method of a cold-rolled steel sheet according to claim 16, containing, in addition to said chemical composition in weight percentage, one or more selected from the following groups A to C:
group A: Ni: 2.0% or less;
group B: one or two of Cr and Mo: 2.0% or less in total; and
group C: one or more of Nb, Ti and V: 0.2% or less in total.

### Claim 18 (depends on 16)

A manufacturing method of a cold-rolled steel sheet according to claim 16, wherein said steel slab has a chemical composition containing, in weight percentage:
26 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less,
and further containing one or more selected from the group consisting of from 0.05 to 2.0% Mo, from 0.05 to 2.0% Cr, and from 0.05 to 2.0% W.

### Claim 19 (depends on 16, 17, 18)

A manufacturing method of a cold-rolled steel sheet according to any one of claims 16 to 18, wherein said hot rolling is conducted under conditions including a heating temperature of said material of 900° C. or more, a finish rolling end temperature of 700° C. or more, and a coiling temperature of 800° C. or below.

### Claim 20 (depends on 16, 17, 18, 19)

A manufacturing method of a cold-rolled steel sheet according to any one of claims 16 to 19, wherein all or part of said hot rolling comprises lubrication rolling.

### Claim 21 (depends on 2, 3, 4, 5, 6)

A hot-dip galvanized steel sheet comprising a hot-dip galvanizing layer or an alloyed hot-dip galvanizing layer formed on the surface of the steel sheet according to any one of claims 2 to 6.

### Claim 22 (depends on 11, 12, 13, 14, 15)

A hot-dip galvanized steel sheet comprising a hot-dip galvanizing layer or an alloyed hot-dip galvanizing layer formed on the surface of the steel sheet according to any one of claims 11 to 15.

### Claim 23

A manufacturing method of a hot-dip galvanized steel sheet excellent in press-formability, and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more, comprising the steps of using a steel sheet having a chemical composition containing, in weight percentage:
27 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, N: 0.02% or less, and Cu: from 0.5 to 3.0%,
applying annealing comprising heating to a dual phase region of ferrite+austenite within a temperature range of from Ac3 transformation point to Ac1 transformation point to said steel sheet on a line for conducting continuous hot-dip galvanizing, and then, performing a hot-dip galvanizing treatment, thereby forming a hot-dip galvanizing layer on the surface of said steel sheet.

### Claim 24 (depends on 23)

A manufacturing method of a hot-dip galvanized steel sheet according to claim 23, further containing, in weight percentage, in addition to said chemical composition, one or more of the following groups A to C:
group A: Ni: 2.0% or less;
group B: one or two of Cr and Mo, 0.2% or less in total; and
group C: one or more of Nb, Ti and V, 0.2% or less in total.

### Claim 25 (depends on 23)

A manufacturing method of a hot-dip galvanized steel sheet according to claim 23, wherein said steel sheet is replaced by a steel sheet having a chemical composition containing, in weight percentage:
28 C: 0.15% or less, Si: 2.0% or less, Mn: 3.0% or less, P: 0.1% or less, S: 0.02% or less, Al: 0.1% or less, and N: 0.02% or less,
and further comprising one or more selected from the group consisting of from 0.05 to 2.0% Mo, from 0.05 to 2.0% Cr and from 0.05 to 2.0% W, 2.0% or less in total.

### Claim 26 (depends on 23, 24, 25)

A manufacturing method of a hot-dip galvanized steel sheet according to any one of claims 23 to 25, wherein, prior to said annealing, a preheating treatment of heating the sheet at a temperature of 700° C. or more on a continuous annealing line, and then applying a pretreatment comprising a pickling treatment.

### Claim 27 (depends on 23, 24, 25, 26)

A manufacturing method of a hot-dip galvanized steel sheet according to any one of claims 23 to 26, comprising the steps of conducting said hot-dip galvanizing treatment to form a hot-dip galvanizing layer on the surface of the steel sheet, and then, performing an alloying treatment of said hot-dip galvanizing layer.

### Claim 28 (depends on 23, 24, 25, 26, 27)

A manufacturing method of a hot-dip galvanized steel sheet excellent in press-formability, and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more according to any one of claims 23 to 27, wherein said steel sheet is a hot-rolled steel sheet manufactured by hot-rolling the material having said chemical composition under conditions including a heating temperature of 900° C. or more, a finish rolling end temperature of 700° C. or more and a coiling temperature of 800° C. or below, or a cold-rolled steel sheet obtained by cold-rolling said hot-rolled steel sheet.

### Claim 29 (depends on 7, 8, 9, 10)

A manufacturing method of a hot-dip galvanized steel sheet excellent in press-formability and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more, further comprising a step of applying a hot-dip galvanizing treatment to the hot-rolled steel sheet resulting from the manufacturing method of a hot-rolled steel sheet according to any one of claims 7 to 10 to form a hot-dip galvanizing layer on the surface of said hot-rolled steel sheet.

### Claim 30 (depends on 16, 17, 18, 19, 20)

A manufacturing method of a hot-dip galvanized steel sheet excellent in press-formability and in strain age hardening property as typically represented by a ΔTS of 80 MPa or more, further comprising a step of applying a hot-dip galvanizing treatment to the cold-rolled steel sheet resulting from the manufacturing method of a cold-rolled steel sheet according to any of claims 16 to 20 to form a hot-dip galvanizing layer on the surface of said cold-rolled steel sheet.

### Claim 31 (depends on 29, 30)

A manufacturing method of a hot-dip galvanized steel sheet according to any one of claims 29 and 30, further comprising the step of carrying out an alloying treatment after said hot-dip galvanizing treatment.