# US 2003/0200916 A1 · Vapor phase growth method of oxide dielectric film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0200916 A1
- Document ID: US20030200916A1
- Status: Published application
- Kind: A1
- Application number: 10/419,822
- Filed: 2003-04-22
- Published: 2003-10-30
- Earliest claimed: 2002-04-24
- Assignees: NEC Electronics Corporation
- Inventors: Takashi Hase
- Web page: https://patentgrep.com/patent/US20030200916A1

## CPC

- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- C23C 16/409: {of the type ABO3 with A representing alkali, alkaline earth metal or lead and B representing a refractory metal, nickel, scandium or a lanthanide}
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45531: {specially adapted for making ternary or higher compositions}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A vapor phase growth method of an oxide dielectric film for forming an oxide dielectric film having a perovskite crystal structure expressed by ABO3 on a substrate according to the present invention includes a first step of sequentially and alternately supplying an A-site layer element material and a B-site layer element material to grow an atomic layer on the substrate to form an early layer or early core, at a first substrate temperature, and a second step of raising the temperature to a second substrate temperature that is higher than the first substrate temperature to crystallize the early layer or early core formed in the first step and simultaneously supplying both the A-site layer element material and the B-site layer element material to form an ABO3 film.

## Claims

### Claim 1

A vapor phase growth method of an oxide dielectric film for forming an oxide dielectric film having a perovskite crystal structure expressed by ABO3 on a substrate, comprising:
a first step of sequentially and alternately supplying an A-site layer element material and a B-site layer element material to perform atomic layer deposition on said substrate to form an early layer or early core, at a first substrate temperature, and
a second step of raising the temperature to a second substrate temperature that is higher than said first substrate temperature to crystallize the early layer or early core formed in said first step and simultaneously supplying both the A-site layer element material and the B-site layer element material to form an ABO3 film.

### Claim 2 (depends on 1)

The vapor phase growth method of an oxide dielectric film according to claim 1, wherein said oxide dielectric having a perovskite crystal structure expressed by ABO3 is a ferroelectric comprising Pb(ZrxTi1−x)O3 (O<×<1) as a main component.

### Claim 3 (depends on 1)

The vapor phase growth method of an oxide dielectric film according to claim 1, wherein said first substrate temperature is 400° C. or less.

### Claim 4 (depends on 1)

The vapor phase growth method of an oxide dielectric film according to claim 1, wherein said substrate is a metal or a conductive oxide comprising at least one or more selected from Pt, Ir and Ru as a main component.

### Claim 5 (depends on 1)

The vapor phase growth method of an oxide dielectric film according to claim 1, further comprising the step of supplying only the A-site layer element material in advance of said first step to form an A-site layer comprising layers composed of one or more atomic layers.

### Claim 6 (depends on 5)

The vapor phase growth method of an oxide dielectric film according to claim 5, wherein said layers composed of one or more atomic layers is the layers composed of less than 30 atomic layers.

### Claim 7

A vapor phase growth method of an oxide dielectric film for forming an ABO3 film after forming an early layer or early core of A1B1O3 by a major element A1 contained in A and a major element B1 contained in B, on a substrate, when forming an oxide dielectric film having a perovskite crystal structure expressed by ABO3, comprising:
a first step of supplying an A1 source and an oxidant to prepare an A1 oxide layer, at a first substrate temperature where A1B1O3 does not crystallize,
a second step of supplying a B1 source and an oxidant to form one atomic layer of a B1 oxide on the A1 oxide layer, at the same substrate temperature as that in the first step,
a third step of supplying an A1 source and an oxidant to form one atomic layer of an A1 oxide on said B1 oxide layer comprising one atomic layer, at the same substrate temperature as that in the first step, and
a fourth step of subsequently raising the temperature to a second substrate temperature of 500° C. or less, thereby crystallizing the early layer or early core of A1B1O3 formed in said first to third steps and then depositing an ABO3 film.

### Claim 8 (depends on 7)

The vapor phase growth method of an oxide dielectric film according to claim 7, wherein said second and third steps are repeated two or more times.

### Claim 9 (depends on 7)

The vapor phase growth method of an oxide dielectric film according to claim 7, wherein said oxide dielectric having a perovskite crystal structure expressed by ABO3 is a ferroelectric comprising Pb(ZrxTi1−x)O3 (0<×<) as a main component and said A1B1O3 is PbTiO3.

### Claim 10 (depends on 7)

The vapor phase growth method of an oxide dielectric film according to claim 7 wherein said first, second, third and fourth steps are performed by a MOCVD method using a metal organic material.