A thermoplastic molding composition comprising components A, B, C and D, and also, where appropriate, E, F, G and H, the entirety of which gives 100% by weight:
- a) from 1 to 97.5% by weight of at least one aromatic polycarbonate A,
- b) from 1 to 97.5% by weight of at least one graft polymer B made from
- b1) from 40 to 80% by weight of a graft base made from an elastomeric polymer B1 based on alkyl acrylates having from 1 to 8 carbon atoms in the alkyl radical, on ethylene-propylene, on dienes or on siloxanes, and having a glass transition temperature below 0° C.,
- b2) from 20 to 60% by weight of a graft B2 made from
- b21) from 60 to 95% by weight of styrene or of substituted styrenes B21 of the formula I
- 5
- where R is C1-C8-alkyl or hydrogen and R1 is C1-C8-alkyl and n is 1, 2 or 3, or a mixture of these, and
- b22) from 5 to 40% by weight of at least one unsaturated nitrile B22,
- c) from 1 to 97.5% by weight of at least one thermoplastic copolymer C made from
- c1) from 60 to 85% by weight of styrene or of substituted styrenes C1 of the formula I, or mixtures of these compounds, and
- c2) from 15 to 40% by weight of at least one unsaturated nitrile C2,
- d) from 0.5 to 25% by weight of a mixture D made from, based on component D,
- d1) from 5 to 95% by weight of at least one particulate mineral filler D1, and
- d2) from 5 to 95% by weight of fibrous fillers D2, where at least 50% by weight of the fibrous fillers have a length of at least 50 μm,
- e) from 0 to 10% by weight of at least one copolymer E made from at least two different alkyl, aromatic or alkylaromatic esters of acrylic acid or of methacrylic acid,
- f) from 0 to 25% by weight of at least one thermoplastic polyester F,
- g) from 0 to 2% by weight of at least one low-molecular-weight organic acid G,
- h) from 0 to 25% by weight of at least one halogen-free phosphorus compound H,
- i) from 0 to 45% by weight of other additives I.