3,4-alkylenedioxy-thiophene copolymers
AssigneeAgfa-Gevaert
InventorsBert Groenendaal, Frank Louwet
Life of this patent
Estimating the term…
Loading patent…
AssigneeAgfa-Gevaert
InventorsBert Groenendaal, Frank Louwet
Estimating the term…
An aqueous dispersion of a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion; a preparation process therefor; its use for coating; a printing ink containing the aqueous dispersion; an electro-conductive layer containing a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof; and an antistatic layer containing a copolymer of at least one 3,4-alkylenedioxy-thiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof.
An aqueous dispersion of a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion.
A chemical polymerization process for preparing an aqueous dispersion of a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion comprising the steps of:
A process using an aqueous dispersion of a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion for coating an object.
An electroconductive layer containing copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof.
An antistatic layer containing a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof.
Dependencies are inferred from the claim text.