# US 2003/0083446 A1 · Method of preparation of coupled branched and linear polymer compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0083446 A1
- Document ID: US20030083446A1
- Status: Published application
- Kind: A1
- Application number: 10/305,542
- Filed: 2002-11-26
- Published: 2003-05-01
- Earliest claimed: 2000-03-23
- Assignees: Firestone Polymers, LLC
- Inventors: Mark N. Dedecker
- Web page: https://patentgrep.com/patent/US20030083446A1

## CPC

- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08C 19/44: of polymers containing metal atoms exclusively at one or both ends of the skeleton
- C08F 297/044: {using a coupling agent}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A continuous process for manufacture of a polymer including branched and linear components comprising first polymerizing conjugated diene(s) in the presence of an organometallic initiator to a conversion that is at least 90% complete. A coupling agent is added to obtain a polymer including branched and linear components. The coupling agent is added at a ratio of about 0.3 to about 0.6 coupling equivalents to initiator equivalents.

## Claims

### Claim 1

A process for manufacture of a polymer including branched and linear components comprising polymerizing at least one conjugated diene in the presence of an organometallic initiator of the formula M(R)x, wherein R represents an organic group and M represents a Group I or Group II metal, to a conversion of at least 90% and adding a coupling agent to produce a polymer comprised of branched and linear chains, said coupling agent being added at a ratio of about 0.3 to about 0.6 coupling agent equivalents to initiator equivalents.

### Claim 2 (depends on 1)

The process of claim 1 wherein said at least one conjugated diene monomer comprises 1,3-butadiene.

### Claim 3 (depends on 1)

The process of claim 1 wherein said coupling agent comprises silicon tetrachloride.

### Claim 4 (depends on 1)

The process of claim 1 wherein said organometallic initiator comprises n-butyl-lithium.

### Claim 5 (depends on 1)

The process of claim 1 wherein from about 0.01 to 1.0 phm of organometallic initiator is used.

### Claim 6 (depends on 1)

The process of claim 1 wherein said polymer has a weight average molecular weight between about 150,000 and about 350,000.

### Claim 7 (depends on 1)

The process of claim 1 wherein said polymer has a weight average molecular weight between about 225,000 and about 275,000.

### Claim 8 (depends on 1)

The process of claim 1 further including the addition of a vinyl modifier to said polymer.

### Claim 9 (depends on 2)

The process of claim 2 further including the addition of 1,2-butadiene.

### Claim 10 (depends on 1)

The process of claim 1 further including the addition of water to terminate the coupling reaction.

### Claim 11 (depends on 1)

The process of claim 1 wherein said polymer has a solution viscosity in the range of about 150 to 190 cP (0.15 to 0.19 kg/m.s).

### Claim 12 (depends on 1)

The process of claim 1 wherein said polymer has a Mooney viscosity in the range of about 60 to 85 (ML4).

### Claim 13 (depends on 1)

The process of claim 1 wherein said conversion is at least 99%.

### Claim 14

A polymer prepared by polymerizing at least one conjugated diene in the presence of an organometallic initiator of the formula M(R)x, wherein R represents an organic group and M represents a Group I or Group II metal, to a conversion that is at least 90% complete and adding a coupling agent to produce a polymer comprised of branched and linear chains, said coupling agent being added at a ratio of about 0.3 to about 0.6 coupling agent equivalents to initiator equivalents.

### Claim 15 (depends on 14)

The polymer of claim 14 having a weight average molecular weight between about 225,000 and about 275,000.

### Claim 16 (depends on 14)

The polymer of claim 14 having a Mooney viscosity in the range of about 60 and 85 (ML4).

### Claim 17 (depends on 14)

The polymer of claim 14 having a solution viscosity in the range of about 150 to 190 cP (0.15 to 0.19 kg/m.s).