# US 2003/0083003 A1 · Polishing pads and manufacturing methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0083003 A1
- Document ID: US20030083003A1
- Status: Published application
- Kind: A1
- Application number: 10/020,081
- Filed: 2001-12-11
- Published: 2003-05-01
- Earliest claimed: 2001-10-29
- Inventors: Thomas E. West JR.; Donald P. Dietz
- Web page: https://patentgrep.com/patent/US20030083003A1

## CPC

- B24B 37/24: characterised by the composition or properties of the pad materials
- B24D 11/001: {Manufacture of flexible abrasive materials}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)

## Abstract

Disclosed is a method of manufacturing polymer materials having properties that are determined by selected process conditions. The properties can be modified for a variety of applications. Exemplary applications are pads for chemical mechanical planarization of substrates and pads for polishing substrates. One embodiment of the method includes the steps of providing a polymer sheet having a substrate contacting area, heating the area a sufficient amount, and applying a sufficient amount of mechanical pressure to the area during at least a portion of the heating step to achieve the desired properties for the material.

## Claims

### Claim 1

A method of manufacturing a pad for polishing a substrate, the method comprising the steps of:
a) providing a polymer sheet having a substrate contacting area;
b) heating the area a sufficient amount; and
c) applying mechanical pressure greater than 1500 psi (10.3 megapascals) to the area during at least a portion of the heating step.

### Claim 2 (depends on 1)

The method of claim 1 further comprising the steps of:
d) cooling the polymer sheet; and
e) providing a sufficient amount of mechanical pressure to the sheet during at least part of the cooling step.

### Claim 3 (depends on 1)

The method of claim 1 wherein the polymer sheet comprises a thermoplastic polymer.

### Claim 4 (depends on 1)

The method of claim 1 wherein the polymer sheet comprises a non-woven felt impregnated with a thermoplastic polymer.

### Claim 5 (depends on 3)

The method of claim 3 wherein the step of heating the polymer sheet a sufficient amount comprises heating to temperatures greater than about 300 degrees F. (149 degrees C.).

### Claim 6 (depends on 4)

The method of claim 4 wherein the step of heating the polymer sheet a sufficient amount comprises heating to temperatures greater than about 300 degrees F. (149 degrees C.).

### Claim 7 (depends on 3)

The method of claim 3 wherein the step of heating the polymer sheet a sufficient amount comprises heating to temperatures in the range of about 300 degrees F. (149 degrees C.) to about 450 degrees F. (232 degrees C.).

### Claim 8 (depends on 4)

The method of claim 4 wherein the step of heating the polymer sheet a sufficient amount comprises heating to temperatures in the range of about 300 degrees F. (149 degrees C.) to about 450 degrees F. (232 degrees C.).

### Claim 9 (depends on 4)

The method of claim 4 wherein the thermoplastic polymer comprises polyurethane and the step of heating the polymer sheet a sufficient amount comprises heating to a temperature of about 400 degrees F. (204 degrees C.).

### Claim 10 (depends on 1)

The method of claim 1 wherein step c comprises compressing the polymer sheet to a predetermined thickness.

### Claim 11

A method of manufacturing a pad for polishing a substrate, the method comprising the steps of:
providing a polymer sheet comprising a non-woven felt impregnated with a thermoplastic polymer, the sheet having a density less than about 0.7 grams per cubic centimeter, the sheet having a substrate contacting area;
heating the area a sufficient amount and contemporaneously applying a sufficient amount of mechanical pressure to the area so that the density of the sheet increases to greater than about 0.7 grams per cubic centimeter.

### Claim 12 (depends on 11)

The method of claim 11 wherein the mechanical pressure compresses the polymer sheet to a predetermined thickness.

### Claim 13 (depends on 11)

The method of claim 11 wherein the mechanical pressure compresses the polymer sheet to a density greater than about 0.9 grams per cubic centimeter.

### Claim 14 (depends on 11)

The method of claim 11 wherein the mechanical pressure compresses the polymer sheet to a density of about 1 gram per cubic centimeter.

### Claim 15

A polymer composite comprising a non-woven felt of polymer fibers impregnated with a resin, the composite having a density greater than about 0.70 grams per cubic centimeter, the composite having a Shore D hardness of at least 50.

### Claim 16 (depends on 15)

The composite of claim 15 wherein the resin comprises a polyurethane and the felt comprises polyester.

### Claim 17 (depends on 15)

The composite of claim 15 wherein the density is about 1 gram per cubic centimeter.

### Claim 18 (depends on 16)

The composite of claim 16 wherein the Shore D hardness is greater than about 60.

### Claim 19

A method of making a composite polymeric material, the method comprising the steps of:
providing a non-woven felt impregnated with a polymer resin;
applying heat to the felt and the resin at a temperature in the range of about 358 degrees Fahrenheit (181 degrees C.) to about 450 degrees Fahrenheit (232 degrees C.) and contemporaneously applying a mechanical pressure greater than about 2500 psi (17.2 megapascals);
cooling the felt and the resin; and
providing a sufficient amount of mechanical pressure to the felt and the resin during at least part of the cooling step so as to maintain a planar surface for the felt and the resin.

### Claim 20 (depends on 19)

The method of claim 19 wherein the pressure is about 2900 psi (20 megapascals).