# US 2003/0082086 A1 · Removal of thiothionylfluoride from sulfur tetrafluoride

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0082086 A1
- Document ID: US20030082086A1
- Status: Published application
- Kind: A1
- Application number: 10/016,034
- Filed: 2001-11-01
- Published: 2003-05-01
- Earliest claimed: 2001-11-01
- Assignees: Air Products and Chemicals, Inc.
- Inventors: Philip Bruce Henderson
- Web page: https://patentgrep.com/patent/US20030082086A1

## CPC

- C01B 17/4523: {Sulfur tetrafluoride}
- B01J 20/20: comprising free carbon; comprising carbon obtained by carbonising processes
- B01J 20/28064: {being in the range 500-1000 m2/g}
- B01J 20/3416: {of sorbents or filter aids comprising free carbon, e.g. activated carbon}
- B01J 20/3458: {in the gas phase}
- B01J 20/3483: {by thermal treatment not covered by groups B01J20/3441 - B01J20/3475, e.g. by heating or cooling}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A process for removing thiothionylfluoride from a composition containing sulfur tetrafluoride and thiothionylfluoride includes contacting the composition with a high surface area material, such as activated carbon. The process can provide purified sulfur tetrafluoride free of thiothionylfluoride. The high surface area material can be replaced for further processing. Alternatively, the material can be regenerated by contacting it with a gas mixture of oxygen and nitrogen at 150-450° C. and converting the adsorbed elemental sulfur to sulfur dioxide without oxidation of the material.

## Claims

### Claim 1

A process for removing thiothionylfluoride from a composition containing sulfur tetrafluoride and an initial concentration of thiothionylfluoride, said process comprising:
contacting said composition with an activated carbon;
reacting at least a portion of said thiothionylfluoride to form elemental sulfur; and
recovering a purified composition containing said sulfur tetrafluoride and said thiothionylfluoride at a reduced concentration less than said initial concentration.

### Claim 2 (depends on 1)

The process of claim 1, wherein said activated carbon has a surface area of about 800 to about 1000 m2/g.

### Claim 3 (depends on 2)

The process of claim 2, wherein said activated carbon has less oxygen-containing active sites than Westvaco activated carbon.

### Claim 4 (depends on 1)

The process of claim 1, wherein said activated carbon is free of metal oxides.

### Claim 5 (depends on 1)

The process of claim 1, wherein said contacting comprises loading said composition on a bed of said activated carbon in a column.

### Claim 6 (depends on 1)

The process of claim 1, wherein a maximum of 800 grams of said activated carbon are provided per mole of said thiothionylfluoride being reacted.

### Claim 7 (depends on 1)

The process of claim 1, wherein said recovering comprises monitoring signals emitted from an effluent flowing from a bed of said activated carbon and collecting said purified composition as a fraction of said effluent emitting said signals indicative of said sulfur tetrafluoride and contraindicative of said thiothionylfluoride.

### Claim 8 (depends on 7)

The process of claim 7, wherein said signals are monitored by ultraviolet spectroscopy and infrared spectroscopy.

### Claim 9 (depends on 1)

The process of claim 1, wherein said initial concentration of thiothionylfluoride is at least 8% v/v.

### Claim 10 (depends on 1)

The process of claim 1, wherein said reduced concentration is 0 to 0.3% v/v.

### Claim 11 (depends on 1)

The process of claim 1, wherein said purified composition is free of thiothionylfluoride.

### Claim 12 (depends on 1)

The process of claim 1, further comprising activating said activated carbon prior to said contacting by heating a carbonaceous material to at least 150° C. under an inert gas atmosphere for at least 8 hours and cooling to room temperature.

### Claim 13 (depends on 1)

The process of claim 1, further comprising replenishing said activated carbon from which said purified composition is obtained by contacting said activated carbon with a gas mixture containing oxygen and nitrogen to convert elemental sulfur adsorbed on said activated carbon to sulfur dioxide without oxidation of said activated carbon.

### Claim 14 (depends on 13)

The process of claim 13, wherein said gas mixture is air.

### Claim 15 (depends on 14)

The process of claim 14, wherein said air is provided at a temperature of 250-300° C. and an airflow rate is provided so as to maintain an oxidation rate such that a reaction zone temperature does not exceed 400° C.

### Claim 16 (depends on 15)

The process of claim 15, wherein said oxidation rate is 9-1000 μg/min.

### Claim 17 (depends on 1)

The process of claim 1, further comprising replenishing said activated carbon from which said purified composition is obtained by replacing said activated carbon with fresh activated carbon.

### Claim 18

A process for removing thiothionylfluoride from a composition containing sulfur tetrafluoride and an initial concentration of thiothionylfluoride, said process comprising:
contacting said composition with a material having a surface area of at least 400 m2/g, wherein said material is free of metal oxides;
reacting at least a portion of said thiothionylfluoride to form elemental sulfur; and
recovering a purified composition containing said sulfur tetrafluoride and said thiothionylfluoride at a reduced concentration less than said initial concentration.

### Claim 19 (depends on 18)

The process of claim 18, wherein said material is activated carbon.