# US 2003/0079997 A1 · Method for coating metal surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0079997 A1
- Document ID: US20030079997A1
- Status: Published application
- Kind: A1
- Application number: 10/269,265
- Filed: 2002-10-11
- Published: 2003-05-01
- Earliest claimed: 2001-10-11
- Assignees: Enthone Inc.
- Inventors: Wolf-Dieter Franz
- Web page: https://patentgrep.com/patent/US20030079997A1

## CPC

- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23C 28/023: {only coatings of metal elements only}
- C23C 28/025: {with at least one zinc-based layer}
- C25D 5/42: of light metals
- C25D 11/34: of metals or alloys not provided for in groups C25D11/04 - C25D11/32
- C25D 13/20: Pretreatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method for coating a light metal alloy component to form a protective layer comprising Sn. First, a surface of the light metal alloy component is cleaned and passivated. A layer comprising Zn is formed on the surface, and a layer comprising Sn is deposited. An intermediate layer is preferably deposited between the Zn-containing layer and the Sn containing layer. The Sn-containing layer may additionally be varnished.

## Claims

### Claim 1

A method for coating a metallic surface comprising:
cleaning and passivating a surface of a light metal alloy component;
forming a first layer on the cleaned and passivated surface wherein the first layer comprises Zn; and
forming a second layer which comprises Sn such that the first layer is located between the surface of the light metal alloy component and the second layer.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the cleaning and passivating step comprises:
alkaline degreasing the surface of the light metal alloy component; and
performing an acid treatment of the surface to oxidatively produce a passivation layer on the surface, the acid treatment comprising contacting the surface with a solution which is selected from a group consisting of an acidic solution, a solution comprising the salt of an acid, and combinations thereof.

### Claim 3 (depends on 2)

The method according to claim 2 wherein the light metal alloy comprises Mg.

### Claim 4 (depends on 3)

The method according to claim 3 wherein the acid treatment step comprises:
contacting the surface of the light metal alloy component with a weak acidic solution; and
contacting the surface with a strong acidic solution which comprises fluoride ions.

### Claim 5 (depends on 4)

The method according to claim 4 wherein the light metal alloy has a Mg composition of at least about 50 weight %.

### Claim 6 (depends on 5)

The method according to claim 5 wherein the weak acidic solution has a pH of from about 3 to about 5.

### Claim 7 (depends on 5)

The method according to claim 5 wherein the weak acidic solution comprises a carboxylic acid and a pyrophosphate.

### Claim 8 (depends on 5)

The method according to claim 5 wherein the strong acidic acid solution has a pH of from about 0.5 to about 2.

### Claim 9 (depends on 5)

The method according to claim 5 wherein the strong acidic acid solution comprises phosphoric acid and ammonium bifluoride.

### Claim 10 (depends on 5)

The method according to claim 5 wherein the weak acidic solution has a pH of from about 3 to about 5 and the strong acidic acid solution has a pH of from about 0.5 to about 2.

### Claim 11 (depends on 5)

The method according to claim 5 wherein the weak acidic solution comprises a carboxylic acid and a pyrophosphate and wherein the strong acidic acid solution comprises phosphoric acid and ammonium bifluoride.

### Claim 12 (depends on 5)

The method according to claim 5 wherein the weak acidic solution has a pH of from about 3 to about 5 and comprises a carboxylic acid and a pyrophosphate and wherein the strong acidic acid solution has a pH of from about 0.5 to about 2 and comprises phosphoric acid and ammonium bifluoride.

### Claim 13 (depends on 2)

The method according to claim 2 wherein the light metal alloy comprises Al.

### Claim 14 (depends on 13)

The method according to claim 13 wherein the acid treatment step comprises contacting the surface of the light metal alloy component with a strong oxidizing solution.

### Claim 15 (depends on 14)

The method according to claim 14 wherein the light metal alloy has an Al composition of at least about 60 weight %.

### Claim 16 (depends on 15)

The method according to claim 15 wherein the strong oxidizing solution comprises an oxidizer selected from the group consisting of nitric acid, peroxomonosulfuric acid, and a persulfate solution.

### Claim 17 (depends on 1)

The method according to claim 1 wherein the cleaning and passivating of the surface of the light metal alloy component comprises:
anodically connecting the surface to an electrical source; and
contacting the surface with a solution which comprises phosphoric acid and an alcohol.

### Claim 18 (depends on 17)

The method according to claim 17 wherein the light metal alloy comprises a metal selected from the group consisting of Mg, Si, and combinations thereof.

### Claim 19 (depends on 18)

The method according to claim 18 wherein the light metal alloy has a Mg composition of at least about 50 weight %.

### Claim 20 (depends on 18)

The method according to claim 18 wherein the light metal alloy has a Si composition of at least about 0.1 weight %.

### Claim 21 (depends on 18)

The method according to claim 18 wherein the cleaning and passivating step comprises contacting the anodically connected surface with a solution that comprises phosphoric acid and fluoride ions.

### Claim 22 (depends on 17)

The method according to claim 17 wherein the light metal alloy comprises Al.

### Claim 23 (depends on 22)

The method according to claim 22 wherein the light metal alloy has an Al composition of at least about 60 weight %.

### Claim 24 (depends on 22)

The method according to claim 22 wherein the cleaning and passivating step comprises contacting the surface of the light metal alloy component with an aqueous oxidation agent.

### Claim 25 (depends on 1)

The method according to claim 1 wherein the first layer is formed by chemical metal plating.

### Claim 26 (depends on 1)

The method according to claim 1 wherein the first layer further comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 27 (depends on 1)

The method according to claim 1 wherein the second layer is formed by electrolytic deposition.

### Claim 28 (depends on 1)

The method according to claim 1 wherein the second layer further comprises a metal selected from the group consisting of Zn, Bi, Pb, and combinations thereof.

### Claim 29 (depends on 1)

The method according to claim 1 further comprising forming an intermediate layer such that the intermediate layer is located between the first layer and the second layer.

### Claim 30 (depends on 29)

The method according to claim 29 wherein the intermediate layer is formed by electrolytic deposition.

### Claim 31 (depends on 29)

The method according to claim 29 wherein the intermediate layer comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 32 (depends on 1)

The method according to claim 1 further comprising depositing varnish layer on the second layer wherein the varnish layer comprises a varnish.

### Claim 33 (depends on 32)

The method according to claim 32 wherein the varnish is a two-component varnish.

### Claim 34 (depends on 32)

The method according to claim 32 further comprising performing a passivating treatment on the second layer prior to depositing the varnish layer.

### Claim 35 (depends on 34)

The method according to claim 34 wherein the passivating treatment comprises an alkaline anodic oxidation.

### Claim 36 (depends on 35)

The method according to claim 35 wherein the passivating treatment comprises contacting the second layer with a solution comprising a compounds selected from the group consisting of phosphates, carbonates, and combinations thereof.

### Claim 37 (depends on 35)

The method according to claim 35 wherein the passivating treatment further comprises a cathodic treatment wherein the second layer is contacted with a solution comprising hexavalent chromium ions.

### Claim 38 (depends on 32)

The method according to claim 32 further comprising removing a portion of the varnish layer to expose a portion of the second layer.

### Claim 39 (depends on 38)

The method according to claim 38 wherein the portion of the varnish layer is removed by bombarding the varnish layer with a laser beam.

### Claim 40 (depends on 39)

The method according to claim 39 wherein the varnish layer is bombarded by the laser beam at least twice to remove the portion of the varnish layer.

### Claim 41

A method for coating a metallic surface comprising:
alkaline degreasing the surface of a light metal alloy component, wherein the light metal alloy component has a Mg composition of at least about 50 weight %;
performing an acid treatment of the surface to oxidatively produce a passivation layer on the surface, the acid treatment comprising:
contacting the surface of the light metal alloy component with a weak acidic solution having a pH of from about 3 to about 5; and
contacting the surface with a strong acidic solution which has a pH of from about 0.5 to about 2 which comprises fluoride ions;
forming a first layer on the cleaned and passivated surface wherein the first layer comprises Zn; and
forming a second layer which comprises Sn such that the first layer is located between the surface of the light metal alloy component and the second layer.

### Claim 42 (depends on 41)

The method according to claim 41 further comprising forming an intermediate layer such that the intermediate layer is located between the first layer and the second layer.

### Claim 43 (depends on 42)

The method according to claim 42 wherein the intermediate layer is formed by electrolytic deposition.

### Claim 44 (depends on 42)

The method according to claim 42 wherein the intermediate layer comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 45

A method for coating a metallic surface comprising:
contacting a surface of a light metal alloy component with an aqueous oxidation agent, wherein the light metal alloy component has an Al composition of at least about 60 weight %;
forming a first layer on the surface wherein the first layer comprises Zn; and
forming a second layer which comprises Sn such that the first layer is located between the surface of the light metal alloy component and the second layer.

### Claim 46 (depends on 45)

The method according to claim 45 further comprising forming an intermediate layer such that the intermediate layer is located between the first layer and the second layer.

### Claim 47 (depends on 46)

The method according to claim 46 wherein the intermediate layer is formed by electrolytic deposition.

### Claim 48 (depends on 46)

The method according to claim 46 wherein the intermediate layer comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 49

A coating for a light metal alloy comprising:
a first layer comprising Zn wherein the first layer is deposited on a surface of the light metal alloy component; and
a second layer comprising Sn,
wherein the first layer is located between the surface of the light metal alloy component and the second layer.

### Claim 50 (depends on 49)

The coating according to claim 49 wherein the light metal alloy comprises Mg.

### Claim 51 (depends on 49)

The coating according to claim 49 wherein the light metal alloy comprises Al.

### Claim 52 (depends on 49)

The coating according to claim 49 wherein the first layer is formed by is formed by chemical metal plating.

### Claim 53 (depends on 49)

The coating according to claim 49 wherein the first layer further comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 54 (depends on 49)

The coating according to claim 49 wherein the second layer is formed by electrolytic deposition.

### Claim 55 (depends on 49)

The coating according to claim 49 wherein the second layer further comprises a metal selected from the group consisting of Zn, Bi, Pb, and combinations thereof.

### Claim 56 (depends on 49)

The coating according to claim 49 further comprising an intermediate layer wherein the intermediate layer is located between the first layer and the second layer.

### Claim 57 (depends on 56)

The coating according to claim 56 wherein the intermediate layer is formed by electrolytic deposition.

### Claim 58 (depends on 56)

The coating according to claim 56 wherein the intermediate layer comprises a metal selected from the group consisting of Cu, Ni, and combinations thereof.

### Claim 59 (depends on 49)

The coating according to claim 49 further comprising a varnish layer which comprises a varnish wherein the second layer is located between the first layer and the varnish layer.