# US 2003/0077909 A1 · Etching method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0077909 A1
- Document ID: US20030077909A1
- Status: Published application
- Kind: A1
- Application number: 10/277,725
- Filed: 2002-10-23
- Published: 2003-04-24
- Earliest claimed: 2001-10-24
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Nobuhiro Jiwari
- Web page: https://patentgrep.com/patent/US20030077909A1

## CPC

- H10W 20/069: {by forming self-aligned vias or self-aligned contact plugs}
- H10P 50/283: {by chemical means}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The etching method of the present invention for forming a hole having a high aspect ratio in a silicon oxide film formed on a substrate via a silicon nitride film includes the step of performing etching using an etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas.

## Claims

### Claim 1

An etching method for forming a hole having a high aspect ratio in a silicon oxide film formed on a substrate via a silicon nitride film, the method comprising the step of:
performing etching using an etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the etching gas is 20% or more.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the etching gas is 50% or more.

### Claim 4 (depends on 1)

The method of claim 1, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the etching gas is in the range of 50% to 70%.

### Claim 5

An etching method for forming a hole having a high aspect ratio in a laminated film formed on a substrate via a silicon nitride film, the laminated film including a lower layer composed of an impurity-containing silicon oxide film and an upper layer composed of a substantially impurity-free silicon oxide film, the method comprising the steps of:
performing first-stage etching for the upper layer using a first etching gas composed of a mixture of Ar gas, O2 gas and C5F8 gas in a relatively large mixing ratio of the O2 gas to the fluorocarbon gas; and
performing second-stage etching for the lower layer using a second etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas in a relatively small mixing ratio of the O2 gas to the fluorocarbon gas.

### Claim 6 (depends on 5)

The method of claim 5, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the second etching gas is 20% or more.

### Claim 7 (depends on 5)

The method of claim 5, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the second etching gas is 50% or more.

### Claim 8 (depends on 5)

The method of claim 5, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the second etching gas is in the range of 50% to 70%.

### Claim 9

An etching method for forming a second hole having a high aspect ratio in a laminated film formed on a silicon nitride film defining a first hole formed on a substrate, the laminated film including a lower layer composed of an impurity-containing silicon oxide film and an upper layer composed of a substantially impurity-free silicon oxide film, the second hole being made integral with the first hole, the method comprising the steps of
performing first-stage dry etching for the upper layer using a first etching gas composed of a mixture of Ar gas, O2 gas and C5F8 gas in a relatively large mixing ratio of the O2 gas to the fluorocarbon gas;
performing second-stage dry etching for the lower layer using a second etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas in a relatively small mixing ratio of the O2 gas to the fluorocarbon gas; and
removing a residue of the lower layer in the first hole by wet etching.

### Claim 10 (depends on 9)

The method of claim 9, wherein the ratio of the flow rate of the CH2F2 gas to the total flow rate of the C5F8 gas and the CH2F2 gas in the second etching gas is in the range of 20% to 70%.

### Claim 11 (depends on 9)

The method of claim 9, wherein the lower layer is a BPSG film containing 3.7 wt % of boron and 7.0 wt % of phosphorus.