# US 2003/0077882 A1 · Method of forming strained-silicon wafer for mobility-enhanced MOSFET device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0077882 A1
- Document ID: US20030077882A1
- Status: Published application
- Kind: A1
- Application number: 09/912,736
- Filed: 2001-07-26
- Published: 2003-04-24
- Earliest claimed: 2001-07-26
- Assignees: Taiwan Semiconductor Manfacturing Company, Ltd.
- Inventors: Wong-Cheng Shih; Wenchi Ting
- Web page: https://patentgrep.com/patent/US20030077882A1

## CPC

- H10P 14/3251: {consisting of three or more layers}
- H10D 30/0516: {of FETs having PN heterojunction gates}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3822: {Controlling the interface between substrate and epitaxial layer, e.g. by ion implantation followed by annealing}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of fabricating a strained-silicon structure comprising the following steps. A substrate having an insulator layer formed thereover is provided. A silicon-on-insulator layer is formed over the insulator layer. A first SiGe layer is formed over the silicon-on-insulator layer. The first SiGe layer being strained. At least the first SiGe layer is annealed to convert the strained SiGe layer to a relaxed first SiGe layer. A second SiGe layer, having the same composition as the first SiGe layer, is formed over the first SiGe layer. The second SiGe layer being relaxed. An epitaxial silicon layer is grown over the second SiGe layer. The epitaxial silicon layer being strained to complete formation of the strained-silicon structure.

## Claims

### Claim 1

A method of fabricating a strained-silicon structure, comprising the steps of:
providing a substrate having an insulator layer formed thereover;
forming a silicon-on-insulator layer over the insulator layer;
forming a first SiGe layer over the silicon-on-insulator layer; the first SiGe layer being strained;
annealing at least the first strained SiGe layer to convert the strained SiGe layer to a first relaxed SiGe layer;
forming a second SiGe layer having the same composition as the first SiGe layer over the first relaxed SiGe layer; the second SiGe layer being relaxed; and
growing an epitaxial silicon layer over the second relaxed SiGe layer; the epitaxial silicon layer being strained to complete formation of the strained-silicon structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon-on-insulator layer has a thickness of from about 5 to 50 nm; the first SiGe layer has a thickness of from about 100 to 400 nm; the second SiGe layer having a thickness of from about 100 to 400 nm; and the epitaxial silicon layer having a thickness of from about 20 to 80 nm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the silicon-on-insulator layer has a thickness of from about 10 to 45 nm; the first SiGe layer has a thickness of from about 50 to 250 nm; the second SiGe layer having a thickness of from about 50 to 300 nm; and the epitaxial silicon layer having a thickness of from about 30 to 70 nm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the silicon-on-insulator is cleaned before formation of the first SiGe layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the silicon-on-insulator is cleaned with dilute HF acid before formation of the first SiGe layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first and second SiGe layers have the composition Si1-xGex where 0.1<x<0.45.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first and second SiGe layers have the composition Si1-xGex where 0.1<x<0.35.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first SiGe layer is annealed at a temperature of from about 800 to 1100° C. for from about 1 to 20 minutes.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first SiGe layer is annealed at a temperature of from about 850 to 1000° C. for from about 1 to 20 minutes.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first and second SiGe layers are epitaxially grown.

### Claim 11 (depends on 1)

The method of claim 1, including the step of forming a semiconductor structure over the strained-silicon structure.

### Claim 12 (depends on 1)

The method of claim 1, wherein the substrate is a silicon substrate.

### Claim 13 (depends on 1)

The method of claim 1, wherein the substrate is a silicon wafer.

### Claim 14

A method of fabricating a strained-silicon structure, comprising the steps of:
providing a substrate having an insulator layer formed thereover;
forming a silicon-on-insulator layer over the insulator layer;
forming a first Si1-xGex layer over the silicon-on-insulator layer where 0.1<x<0.45; the first Si1-xGex layer being strained;
annealing at least the first Si1-xGex layer to convert the strained Si1-xGex layer to a first relaxed Si1-xGex layer;
forming a second Si1-xGex layer having the same composition as the first Si1-xGex layer over the first Si1-xGex layer; the second Si1-xGex layer being relaxed; and
growing an epitaxial silicon layer over the second Si1-xGex layer; the epitaxial silicon layer being strained to complete formation of the strained-silicon structure.

### Claim 15 (depends on 14)

The method of claim 14, wherein the silicon-on-insulator layer has a thickness of from about 5 to 50 nm; the first Si1-xGex layer has a thickness of from about 100 to 400 nm; the second Si1-xGex layer having a thickness of from about 100 to 400 nm; and the epitaxial silicon layer having a thickness of from about 20 to 80 nm.

### Claim 16 (depends on 14)

The method of claim 14, wherein the silicon-on-insulator layer has a thickness of from about 10 to 45 nm; the first Si1-xGex layer has a thickness of from about 50 to 250 nm; the second Si1-xGex layer having a thickness of from about 50 to 300 nm; and the epitaxial silicon layer having a thickness of from about 30 to 70 nm.

### Claim 17 (depends on 14)

The method of claim 14, wherein the silicon-on-insulator is cleaned before formation of the first Si1-xGex layer.

### Claim 18 (depends on 14)

The method of claim 14, wherein the silicon-on-insulator is cleaned with dilute HF acid before formation of the first Si1-xGex layer.

### Claim 19 (depends on 14)

The method of claim 14, wherein 0.1<x<0.35.

### Claim 20 (depends on 14)

The method of claim 14, wherein the first Si1-xGex layer is annealed at a temperature of from about 800 to 1100° C. for from about 1 to 20 minutes.

### Claim 21 (depends on 14)

The method of claim 14, wherein the first Si1-xGex layer is annealed at a temperature of from about 850 to 1000° C. for from about 1 to 20 minutes.

### Claim 22 (depends on 14)

The method of claim 14, wherein the first and second Si1-xGex layers are epitaxially grown.

### Claim 23 (depends on 14)

The method of claim 14, including the step of forming a semiconductor structure over the strained-silicon structure.

### Claim 24 (depends on 14)

The method of claim 14, wherein the substrate is a silicon substrate.

### Claim 25 (depends on 14)

The method of claim 14, wherein the substrate is a silicon wafer.

### Claim 26

A method of fabricating a strained-silicon structure, comprising the steps of:
providing a substrate having an insulator layer formed thereover;
forming a silicon-on-insulator layer upon the insulator layer; the silicon-on-insulator layer having a thickness of from about 5 to 50 nm;
forming a first Si1-xGex layer upon the silicon-on-insulator layer where 0.1<x <0.45; the first Si1-xGex layer being strained; the first Si1-xGex layer 16 having a thickness of from about 100 to 400 nm;
annealing at least the first Si1-xGex layer to convert the strained Si1-xGex layer to a first relaxed Si1-xGex layer;
forming a second Si1-xGex layer having the same composition as the first Si1-xGex layer upon the first Si1-xGex layer; the second Si1-xGex layer being relaxed; the second Si1-xGex layer having a thickness of from about 100 to 400 nm; and
growing an epitaxial silicon layer upon the second Si1-xGex layer; the epitaxial silicon layer being strained to complete formation of the strained-silicon structure; the epitaxial silicon layer having a thickness of from about 20 to 80 nm.

### Claim 27 (depends on 26)

The method of claim 26, wherein the silicon-on-insulator layer has a thickness of from about 10 to 45 nm; the first Si1-xGex layer has a thickness of from about 50 to 250 nm; the second Si1-xGex layer having a thickness of from about 50 to 300 nm; and the epitaxial silicon layer having a thickness of from about 30 to 70 nm.

### Claim 28 (depends on 26)

The method of claim 26, wherein the silicon-on-insulator is cleaned before formation of the first Si1-xGex layer.

### Claim 29 (depends on 26)

The method of claim 26, wherein the silicon-on-insulator is cleaned with dilute HF acid before formation of the first Si1-xGex layer.

### Claim 30 (depends on 26)

The method of claim 26, wherein 0.1<x<0.35.

### Claim 31 (depends on 26)

The method of claim 26, wherein the first Si1-xGex layer is annealed at a temperature of from about 800 to 1100° C. for from about 1 to 20 minutes.

### Claim 32 (depends on 26)

The method of claim 26, wherein the first Si1-xGex layer is annealed at a temperature of from about 850 to 1000° C. for from about 1 to 20 minutes.

### Claim 33 (depends on 26)

The method of claim 26, wherein the first and second Si1-xGex layers are epitaxially grown.

### Claim 34 (depends on 26)

The method of claim 26, including the step of forming a semiconductor structure over the strained-silicon structure.

### Claim 35 (depends on 26)

The method of claim 26, wherein the substrate is a silicon substrate.

### Claim 36 (depends on 26)

The method of claim 26, wherein the substrate is a silicon wafer.