# US 2003/0077460 A1 · Supported tungsten carbide material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0077460 A1
- Document ID: US20030077460A1
- Status: Published application
- Kind: A1
- Application number: 09/966,047
- Filed: 2001-09-28
- Published: 2003-04-24
- Earliest claimed: 2000-09-29
- Assignees: Osram Sylvania Inc.
- Inventors: Joel B. Christian; Tuan A. Dang; Robert G. Mendenhall
- Web page: https://patentgrep.com/patent/US20030077460A1

## CPC

- C04B 41/009: {characterised by the material treated}
- B01J 21/04: Alumina
- B01J 21/18: Carbon
- B01J 27/22: Carbides
- C04B 41/4584: {Coating or impregnating of particulate or fibrous ceramic material (C04B20/10, C04B35/628 take precedence)}
- C04B 41/81: Coating or impregnation
- C04B 2111/0081: {as catalysts or catalyst carriers}
- Y10T 428/25: Web or sheet containing structurally defined element or component and including a second component containing structurally defined particles
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- Y10T 428/31641: Next to natural rubber, gum, oil, rosin, wax, bituminous or tarry residue
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A supported tungsten carbide material is provided. The material has a unique structure as defined by its x-ray diffraction pattern and consists of extremely small crystallites on the order of about 15 to about 30 angstroms in size. The tungsten carbide material is supported on a high-surface-area support to allow for a greater number of active sites for catalysis. The support consists preferably of a high-surface-area carbon.

## Claims

### Claim 1

A supported tungsten carbide material comprising: a high-surface-area support and a tungsten carbide material; the high-surface-area support being comprised of carbon or alumina; the tungsten carbide being present on the surface of the high-surface-area support and comprising tungsten and carbon, the tungsten carbide material having an x-ray diffraction pattern containing a primary x-ray diffraction peak and first and second secondary x-ray diffraction peaks, the primary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 2.39±0.02 Å, the first secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.496±0.007 Å and a relative peak height of 25% to 40% of the peak height of the primary x-ray diffraction peak, and the second secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.268±0.005 Å and a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 2 (depends on 1)

The supported tungsten carbide material of claim 1 wherein ratio of peak height of the first secondary x-ray diffraction peak to the peak height of the second x-ray diffraction peak is from 0.65 to 0.80.

### Claim 3 (depends on 1)

The supported tungsten carbide material of claim 1 wherein ratio of peak height of the first secondary x-ray diffraction peak to the peak height of the second x-ray diffraction peak is from 0.69 to 0.75.

### Claim 4 (depends on 1)

The supported tungsten carbide material of claim 1 wherein the composition of the material is represented by the general formula WC1−x where x is from 0 to 0.5.

### Claim 5 (depends on 1)

The supported tungsten carbide material of claim 1 wherein the material has crystallite sizes of about 15 Å to about 30 Å.

### Claim 6 (depends on 5)

The supported tungsten carbide material of claim 5 wherein ratio of peak height of the first secondary x-ray diffraction peak to the peak height of the second x-ray diffraction peak is from 0.65 to 0.80.

### Claim 7 (depends on 6)

The supported tungsten carbide material of claim 6 wherein ratio of peak height of the first secondary x-ray diffraction peak to the peak height of the second x-ray diffraction peak is from 0.69 to 0.75.

### Claim 8

A supported tungsten carbide material comprising: a high-surface-area support and a tungsten carbide material; the high-surface-area support being comprised of carbon or alumina; the tungsten carbide being present on the surface of the high-surface-area support and comprising tungsten and carbon, the tungsten carbide material comprising tungsten and carbon, the material having a CuKα1 x-ray diffraction pattern consisting of a primary x-ray diffraction peak and first and second secondary x-ray diffraction peaks, the primary peak having a 2-theta reflection angle of 37.3 to 37.9 degrees, the first secondary peak having a 2-theta reflection angle of 61.7 to 62.3 degrees, the second secondary peak having a 2-theta reflection angle of 74.5 to 75.1 degrees, and wherein the ratio of the peak height of the first secondary peak to the peak height of the second secondary peak is from 0.65 to 0.80.

### Claim 9 (depends on 8)

The supported tungsten carbide material of claim 8 wherein the first secondary peak has a relative peak height of 25% to 40% of the peak height of the primary x-ray diffraction peak and the second secondary x-ray diffraction peak has a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 10 (depends on 9)

The supported tungsten carbide material of claim 9 wherein the ratio of the peak height of the first secondary peak to the peak height of the second secondary peak is from 0.69 to 0.75.

### Claim 11 (depends on 8)

The supported tungsten carbide material of claim 8 wherein the composition of the material is represented by the general formula WC1−x where x is from 0 to 0.5.

### Claim 12 (depends on 8)

The supported tungsten carbide material of claim 8 wherein the material has crystallite sizes of about 15 Å to about 30 Å.

### Claim 13 (depends on 12)

The supported tungsten carbide material of claim 12 wherein the first secondary peak has a relative peak height of 25% to 40% of the peak height of the primary x-ray diffraction peak and the second secondary x-ray diffraction peak has a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 14 (depends on 13)

The supported tungsten carbide material of claim 13 wherein the ratio of the peak height of the first secondary peak to the peak height of the second secondary peak is from 0.69 to 0.75.

### Claim 15

A method for forming a supported tungsten carbide material comprising: forming a mixture of a tungsten precursor and a high-surface area support; and, heating the mixture to a temperature from about 500° C. to about 800° C. in an atmosphere containing a hydrocarbon gas and, optionally, hydrogen gas for a time sufficient to convert the tungsten precursor to the tungsten carbide material.

### Claim 16 (depends on 15)

The method of claim 15 wherein the mixture is formed by dissolving the tungsten precursor to form a tungsten-containing solution, forming a slurry of the high-surface-area support with the tungsten-containing solution, and drying to form the mixture.

### Claim 17 (depends on 15)

The method of claim 15 wherein the tungsten precursor is selected from ammonium metatungstate, ammonium paratungstate, ammonium tungstate, sodium tungstate, or tungsten oxides.

### Claim 18 (depends on 15)

The method of claim 15 wherein the tungsten precursor is ammonium metatungstate or ammonium paratungstate.

### Claim 19 (depends on 15)

The method of claim 15 wherein the hydrocarbon gas is selected from propane, ethane, natural gas, ethylene, acetylene, or a combination thereof.

### Claim 20 (depends on 15)

The method of claim 15 wherein the hydrocarbon gas has a molecular formula containing twelve or less carbon atoms.

### Claim 21 (depends on 19)

The method of claim 19 wherein the hydrocarbon gas is ethane or propane.

### Claim 22 (depends on 15)

The method of claim 15 wherein the tungsten carbide material is cooled in an inert atmosphere and passivated in nitrogen after conversion.

### Claim 23 (depends on 21)

The method of claim 21 wherein the tungsten precursor is ammonium paratungstate.

### Claim 24 (depends on 15)

The method of claim 15 wherein the tungsten carbide material comprises tungsten and carbon and has an x-ray diffraction pattern containing a primary x-ray diffraction peak and first and second secondary x-ray diffraction peaks, the primary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 2.39±0.02 Å, the first secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.496±0.007 Å and a relative peak height of 25% to 40% of the peak height of the primary x-ray diffraction peak, and the second secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.268±0.005 Å and a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 25

A method for forming a supported tungsten carbide material comprising: forming an aqueous solution of ammonium metatungstate, mixing the solution with a high-surface-area support, adjusting the pH of the solution to promote the formation of ammonium paratungstate, allowing the solution to set to form crystals of ammonium paratungstate, separating the solid material from the solution, and drying the solids to form a mixture of ammonium paratungstate and a high-surface area support, heating the mixture to a temperature from about 500° C. to about 800° C. in an atmosphere containing a hydrocarbon gas and, optionally, hydrogen gas for a time sufficient to convert the tungsten precursor to the tungsten carbide material.

### Claim 26 (depends on 25)

The method of claim 25 wherein the hydrocarbon gas is selected from propane, ethane, natural gas, ethylene, acetylene, or a combination thereof.

### Claim 27 (depends on 25)

The method of claim 25 wherein the hydrocarbon gas has a molecular formula containing twelve or less carbon atoms.

### Claim 28 (depends on 26)

The method of claim 26 wherein the hydrocarbon gas is ethane or propane.

### Claim 29 (depends on 25)

The method of claim 25 wherein the tungsten carbide material is cooled in an inert atmosphere and passivated in nitrogen after conversion.

### Claim 30 (depends on 25)

The method of claim 25 wherein the high-surface-area support is a high-surface-area carbon or a high-surface-area alumina.

### Claim 31 (depends on 30)

The method of claim 30 wherein the surface area of the support is at least about 50 m2/g.

### Claim 32 (depends on 31)

The method of claim 31 wherein the surface area of the support is from about 100 m2/g to about 1000 m2/g.

### Claim 33 (depends on 31)

The method of claim 31 wherein the support is a high-surface-area carbon.

### Claim 34 (depends on 33)

The method of claim 33 wherein the hydrocarbon gas is ethane or propane.

### Claim 35 (depends on 25)

The method of claim 25 wherein the tungsten carbide material comprises tungsten and carbon and has an x-ray diffraction pattern containing a primary x-ray diffraction peak and first and second secondary x-ray diffraction peaks, the primary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 2.39±0.02 Å, the first secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.496±0.007 Å and a relative peak height of 25% to 40% of the peak height of the primary x-ray diffraction peak, and the second secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.268±0.005 Å and a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 36

A method for forming a supported tungsten carbide material comprising: forming a mixture of a tungsten precursor selected from ammonium paratungstate or ammonium metatungstate and a high-surface-area support selected from a high-surface-area carbon or a high-surface-area alumina; heating the mixture to a temperature from about 500° C. to about 800° C. in an atmosphere containing a hydrocarbon gas and, optionally, hydrogen gas for a time sufficient to convert the tungsten precursor to the tungsten carbide material; the tungsten carbide material comprising tungsten and carbon; the material having an x-ray diffraction pattern containing a primary x-ray diffraction peak and first and second secondary x-ray diffraction peaks, the primary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 2.39±0.02 Å, the first secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.496±0.007 Å and a relative peak height of 25% to 40% of the peak height of the primary x-ray ray diffraction peak, and the second secondary x-ray diffraction peak having a reflection angle corresponding to a d-spacing of 1.268±0.005 Å and a relative peak height of 35% to 55% of the peak height of the primary x-ray diffraction peak.

### Claim 37 (depends on 36)

The method of claim 36 wherein the hydrocarbon gas is ethane or propane.

### Claim 38 (depends on 36)

The method of claim 36 wherein the surface area of the support is at least about 50 m2/g.

### Claim 39 (depends on 38)

The method of claim 38 wherein the surface area of the support is from about 100 m2/g to about 1000 m2/g.

### Claim 40 (depends on 38)

The method of claim 38 wherein the support is a high-surface-area carbon.

### Claim 41 (depends on 36)

The method of claim 36 wherein the mixture is formed by dissolving the tungsten precursor to form a tungsten-containing solution, forming a slurry of the high-surface-area support with the tungsten-containing solution, and drying to form the mixture.

### Claim 42 (depends on 41)

The method of claim 41 wherein the surface area of the support is at least about 50 m2/g.