# US 2003/0076217 A1 · Polymeric PTC device capable of returning to its initial resistance after overcurrent protection

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0076217 A1
- Document ID: US20030076217A1
- Status: Published application
- Kind: A1
- Application number: 10/045,973
- Filed: 2002-01-10
- Published: 2003-04-24
- Earliest claimed: 2001-10-12
- Assignees: Ceratech Corporation
- Inventors: Kyoung-Ri Park; Byoung-Su Jin; Sang-Joon Sung; Yu-Seok Kim; Seoung-Jung Ryu
- Web page: https://patentgrep.com/patent/US20030076217A1

## CPC

- H01C 17/06586: {composed of organic material}
- H01C 7/027: {consisting of conducting or semi-conducting material dispersed in a non-conductive organic material}
- H01C: RESISTORS

## Abstract

A polymeric positive temperature coefficient (PTC) thermistor having a particular crystalline structure to allow the resistivity of the crystalline polymer to return to its approximate original level after an overcurrent is applied thereto. Subjecting a polymer to cross-linking, heating the cross-linked polymer at a temperature of a melting point of the polymer or above the melting point of the polymer, and re-crystallizing the heated polymer forms the particular crystalline structure. By doing so, the cross-linking rate of the crystalline polymer is maximized, and the size of the crystals in the crystalline polymer is minimized. Also, the polymer layer having electrodes thereon are cut into units of a desired size before setting and/or hardening thereof, to minimize to formation of irregularities such as stress fractures, microscopic cracks, and the like.

## Claims

### Claim 1

A polymeric positive temperature coefficient (PTC) device comprising:
a composite polymer having a conductive substance dispersed therein; and
at least one pair of electrodes electrically connected with the composite polymer,
the composite polymer having a particular crystalline structure formed by subjecting the composite polymer to cross-linking, heating the cross-linked polymer at a temperature approximately at or above a melting point of a polymer material, and re-crystallizing the heated polymer.

### Claim 2 (depends on 1)

The device of claim 1, wherein a resistance of the composite polymer returns to its approximate original level after an overcurrent is applied thereto.

### Claim 3 (depends on 1)

The device of claim 1, wherein the composite polymer has an initial resistance, and a subsequent resistance after receiving an overcurrent being approximately equal to the initial resistance, due to the particular crystalline structure of the polymer.

### Claim 4 (depends on 1)

The device of claim 1, wherein the composite polymer comprises a polymer material, a conductive filler material, and at least one other additive.

### Claim 5 (depends on 4)

The device of claim 4, wherein the polymer material is selected from a group comprising polyethylene, co-polymer of polyethylene, polypropylene, ethyl/propylene co-polymer, polybutadiene, acrylate, acrylic ethylene co-polymer, and polyvinylidene fluoride, or any combination thereof.

### Claim 6 (depends on 4)

The device of claim 4, wherein the conductive filler material is selected from a group comprising nickel powder, gold powder, copper powder, silver coated copper powder, metal alloy powder, carbon black, carbon powder, and graphite, or any combination thereof.

### Claim 7 (depends on 4)

The device of claim 4, wherein the other additive includes a non-conductive filler material selected from a group comprising an anti-oxidizing agent, salt restrainer, stabilizer, anti-ozonizing agent, cross-linking agent, and dispersant, or any combination thereof.

### Claim 8 (depends on 1)

The device of claim 1, wherein the polymeric PTC device is a polymeric PTC thermistor.

### Claim 9 (depends on 1)

The device of claim 1, further comprising an insulator encapsulating the composite polymer while exposing a portion of the electrodes.

### Claim 10

A polymer thermistor having a positive temperature coefficient of resistivity comprising:
a composite polymer having a conductive substance dispersed therein; and
at least one pair of electrodes electrically connected with the composite polymer,
the composite polymer having a particular crystalline structure formed by cross-linking the composite polymer and heating the cross-linked composite polymer at a temperature approximately at or greater than a melting temperature of a polymer material to maximize a cross-linking rate of crystals therein, and by cooling the heated polymer for approximately no more than five minutes to minimize a size of the crystals.

### Claim 11

A method of forming a polymeric positive temperature coefficient (PTC) device, the method comprising:
providing a composite polymer layer;
forming at least one pair of electrodes on an upper surface and a lower surface the polymer layer to obtain an intermediate structure;
dividing the intermediate structure into samples of a desired size;
subjecting the samples to cross-linking; and
re-crystallizing the samples to form a polymeric positive temperature coefficient (PTC) device.

### Claim 12 (depends on 11)

The method of claim 11, further comprising a step of first heating processing the samples prior to cross-linking.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first heat processing comprises a step of heating at a temperature that is approximately between a melting point of the polymer layer to 100° C. above the melting point of the polymer layer, and a step of relatively slow cooling at about room temperature.

### Claim 14 (depends on 11)

The method of claim 11, further comprising a step of second heat processing the samples after cross-linking.

### Claim 15 (depends on 14)

The method of claim 14, wherein the second heat processing comprises a step of heating at a temperature that is approximately between a melting point of the polymer to 100° C. above the melting point of the polymer layer, and a step of relatively rapid cooling at a temperature that is approximately between room temperature to 0° C. for no more than five minutes.

### Claim 16 (depends on 11)

The method of claim 11, wherein the composite polymer layer comprises a polymer material, a conductive filler material, and at least one other additive.

### Claim 17 (depends on 11)

The method of claim 11, wherein the cross-linking is achieved by irradiating the samples and/or performing chemical cross-linking.

### Claim 18 (depends on 17)

The method of claim 17, wherein the irradiating is performed by an electron beam.

### Claim 19 (depends on 11)

The method of claim 11, wherein the re-crystallizing is performed by cooling the samples to minimize a size of the crystals.

### Claim 20 (depends on 11)

The method of claim 11, wherein the formed polymeric PTC device is a polymeric PTC thermistor.