# US 2003/0071304 A1 · Method of forming flash memory having pre-interpoly dielectric treatment layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0071304 A1
- Document ID: US20030071304A1
- Status: Published application
- Kind: A1
- Application number: 10/291,293
- Filed: 2002-11-08
- Published: 2003-04-17
- Earliest claimed: 1999-08-13
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Robert B. Ogle JR.; Arvind Halliyal
- Web page: https://patentgrep.com/patent/US20030071304A1

## CPC

- H10D 64/681: {having a compositional variation, e.g. multilayered}
- H10D 30/6891: {characterised by the shapes, relative sizes or dispositions of the floating gate electrode}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A flash memory structure and its fabrication process, whereby stacks, of a first poly-crystalline silicon material or an amorphous silicon material (polysilicon), are processed for formation of a pre-interpoly dielectric treatment layer over the first polysilicon material. The pre-interpoly dielectric treatment layer being a solid material formed by a chemical reaction formed for purposes of improving the reliability of an interpoly dielectric member and results in changing the capacitor coupling ratio of the flash memory element and allows the use of new power supply and programming voltages. The pre-interpoly dielectric treatment layer is formed by exposing the polysilicon stacks to a selected one of at least three ambient reagent gases. The selected gaseous ambient and exposure of the polysilicon stacks being performed in a fabrication tool such as a batch furnace, a single wafer rapid thermal anneal tool, or a plasma chamber. The reagent gases consist essentially of: (1) nitrous oxide (N2O) and/or nitric oxide (NO), (2) oxygen (O2) and/or water (H2O), and (3) ammonia (NH3). Any one ambient reagent gas may be selected and utilized in any of the foregoing fabrication tools for pre-treating the surface of the first polysilicon stack prior to forming the interpoly dielectric structure member of the flash memory element. The interpoly dielectric member being a stack of silicon dioxide-silicon nitride-silicon dioxide material known as an ONO is thereon subsequently formed.

## Claims

### Claim 1

A flash memory semiconductor apparatus, said apparatus comprising:
a. a semiconductor substrate;
b. at least one region on said substrate member having a silicon dioxide layer;
c. a silicon material deposited over said silicon dioxide layer, said silicon material and said silicon dioxide layer being formed into at least one partial stack portion of a flash memory element, said silicon material formed into said at least one stack portion comprising a first polysilicon layer of said flash memory element;
d. a pre-interpoly dielectric treatment layer, said pre-interpoly dielectric treatment layer being formed over said first polysilicon layer;
e. an interpoly dielectric member, said interpoly dielectric member being formed over said pre-interpoly dielectric treatment layer; and
f. a second polysilicon layer, said second polysilicon layer being formed over said interpoly dielectric member and forming another fabricated stage of said flash memory element.

### Claim 2 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace at an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to two (2) hours in a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of a nitric oxide (NO) and a nitrous oxide (N2O), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar), nitrogen (N2), and oxygen (O2), in a concentration balancing that of the selected at least one reagent gas, at a pressure ranging from 0.1 to 10.0 atmospheres.

### Claim 3 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool at an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to two (2) minutes in a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of nitric oxide (NO) and nitrous oxide (N2O), in a concentration ranging from 1 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar), nitrogen (N2), and oxygen (O2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 4 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a plasma chamber, said chemical reaction comprises treating a surface of said first polysilicon layer in a plasma for a duration ranging from one (1) second to two (2) minutes, said plasma being selected from a plasma group of reagent gases consisting essentially of nitric oxide (NO) plasma and nitrous oxide (N2O) plasma.

### Claim 5 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace at an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to sixty (60) minutes in a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of oxygen (O2) and water (H2O), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas, at a pressure ranging from 0.5 to 10.0 atmospheres.

### Claim 6 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool at an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to one hundred twenty seconds with a gas mixture, and
b. said gas mixture comprising at least one ambient reagent gas selected from a group of reagent gases consisting essentially of oxygen (O2) and water (H2O), in a concentration ranging from 1 to 100 volume % and 0.5 to 80 volume percent, respectively, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 7 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace at an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to one hundred twenty (120) minutes in a gas mixture, and said gas mixture comprising a reagent gas, ammonia (NH3), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas, at a pressure ranging from 0.5 to 10.0 atmospheres.

### Claim 8 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
a. said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool at an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to one hundred twenty (120) seconds in a gas mixture, and
b. said gas mixture comprising a reagent gas, ammonia (NH3), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas stream selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 9 (depends on 1)

A flash memory semiconductor apparatus, as recited in claim 1, wherein:
said pre-interpoly dielectric treatment layer comprises a solid material produced from a chemical reaction in a plasma chamber, said chemical reaction comprises treating a surface of said first polysilicon layer in a reagent gas, ammonia (NH3), plasma for a duration ranging from one (1) second to two (2) minutes.

### Claim 10

A method of fabricating a flash memory semiconductor apparatus, said method comprising the steps of:
a. providing a semiconductor substrate;
b. fabricating a silicon dioxide layer on at least one region of said substrate member;
c. depositing a silicon material over said silicon dioxide layer;
d. forming said silicon material and said silicon dioxide layer into at least one partial stack portion of a flash memory element, said silicon material formed into said at least one stack portion comprising a first polysilicon layer of said flash memory element;
e. forming a pre-interpoly dielectric treatment layer over said first polysilicon layer;
f. forming an interpoly dielectric member over said pre-interpoly dielectric treatment layer; and
forming a second polysilicon layer over said interpoly dielectric member.

### Claim 11 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace by heating said polysilicon layer to an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to two (2) hours, exposing said heated first polysilicon layer to a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of a nitric oxide (NO) and a nitrous oxide (N2O), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar), nitrogen (N2), and oxygen (O2), in a concentration balancing that of the selected at least one reagent gas, and pressurizing said batch furnace to a pressure ranging from 0.1 to 10.0 atmospheres.

### Claim 12 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool by heating said polysilicon layer to an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to two (2) minutes, exposing said heated first polysilicon layer to a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of a nitric oxide (NO) and a nitrous oxide (N2O), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar), nitrogen (N2), and oxygen (O2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 13 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
said step of forming pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a plasma chamber, said chemical reaction comprises treating a surface of said first polysilicon layer in a plasma for a duration ranging from one (1) second to two (2) minutes, said plasma being selected from a plasma group consisting of a nitrogen (N2) plasma and a nitrous oxide (N2O) plasma.

### Claim 14 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace by heating said first polysilicon layer to an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to sixty minutes, exposing said heated first polysilicon layer to in a gas mixture, and
b. said gas mixture comprising at least one reagent gas selected from a group of reagent gases consisting essentially of oxygen (O2) and water (H2O), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas, and pressurizing said batch furnace to a pressure ranging from 0.5 to 10.0 atmospheres.

### Claim 15 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool at an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to one hundred twenty (120) seconds, exposing said heated first polysilicon layer to a gas mixture, and
b. said gas mixture comprising at least one ambient reagent gas selected from a group of reagent gases consisting essentially of oxygen (O2) and water (H2O), in a concentration ranging from 1 to 100 volume % and 0.5 to 80 volume percent, respectively, and at least one diluent gas selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 16 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a batch furnace, said chemical reaction comprises treating said first polysilicon layer in said batch furnace by heating said first polysilicon layer to an elevated temperature ranging from 800° C. to 1050° C. for a duration ranging from one (1) minute to one hundred twenty (120) minutes, exposing said heated first polysilicon layer to a gas mixture,
b. said gas mixture comprising a reagent gas, ammonia (NH3), in a concentration ranging from 5 to 100 volume %, and at least one diluent gas stream selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas, and pressurizing said batch furnace to a pressure ranging from 0.5 to 10.0 atmospheres.

### Claim 17 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus, as recited in claim 10, wherein:
a. said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a single wafer RTA tool, said chemical reaction comprises treating said first polysilicon layer in said RTA tool by heating said first polysilicon layer to an elevated temperature ranging from 700° C. to 1150° C. for a duration ranging from one (1) second to one hundred twenty (120) seconds, exposing said heated first polysilicon layer to a gaseous mix,
b. said gas mixture comprising a reagent gas, ammonia (NH3), in a concentration ranging from 1 to 100 volume %, and at least one diluent gas stream selected from a group of diluent gases consisting essentially of argon (Ar) and nitrogen (N2), in a concentration balancing that of the selected at least one reagent gas.

### Claim 18 (depends on 10)

A method of fabricating a flash memory semiconductor apparatus as recited in claim 10, wherein:
said step of forming a pre-interpoly dielectric treatment layer over said first polysilicon layer comprises producing a solid material by a chemical reaction in a plasma chamber, said chemical reaction comprises treating a surface of said first polysilicon layer in a reagent gas plasma, ammonia (NH3), for a duration ranging from one (1) second to two (2) minutes.

### Claim 19

A flash memory semiconductor apparatus, said apparatus comprising:
a. a semiconductor substrate;
b. at least one region on said substrate member having a silicon dioxide layer;
c. a silicon material deposited over said silicon dioxide layer, said silicon material and said silicon dioxide layer being formed into at least one partial stack portion of a flash memory element, said silicon material formed into said at least one stack portion comprising a first polysilicon layer of said flash memory element;
d. a pre-interpoly dielectric treatment layer, said pre-interpoly dielectric treatment layer being formed over said first polysilicon layer;
e. a multi-layered interpoly dielectric member, said multi-layered interpoly dielectric member being formed such that said pre-interpoly dielectric treatment layer facilitates a thickness decrease ranging from 5 to 30 Å for said dielectric member, thereby increasing a capacitor coupling ratio from 5% to 10% and lowering a power supply programming voltage by 2 to 10%; and
f. a second polysilicon layer, said second polysilicon layer being formed over said interpoly dielectric member and forming another fabricated stage of said flash memory element.

### Claim 20 (depends on 19)

A flash memory semiconductor apparatus, as recited in claim 19 wherein:
said multi-layered interpoly dielectric member comprises
a. a top oxide layer of silicon dioxide;
b. a middle nitride layer of silicon nitride; and
c. a bottom oxide layer of silicon dioxide, and
said multi-layered interpoly dielectric member being known as an ONO.