Method of manufacturing a motor vehicle antivibration device comprising a metal insert for bonding to elastomer
AssigneeHutchinson
InventorsAndre Girard, Victor Zarife
Life of this patent
Estimating the term…
Abstract
A method of manufacturing an antivibration device for motor vehicles, the device comprising at least one metal insert having at least one fixing surface bonded to an elastomer, the method including a cleaning step during which the fixing surface is scanned with a laser beam that is sufficiently powerful to eliminate the impurities present on said surface.
Claims13
1/ A method of manufacturing an antivibration device for motor vehicles, the device comprising at least one metal insert itself having at least one fixing surface bonded to an elastomer, the method comprising the following steps:
- a step of cleaning the fixing surface;
- a coating step during which the fixing surface is covered in at least one layer of fixing material for making a bond between the insert and the elastomer, said material being based on rubber;
- and
- a step of molding the elastomer onto the insert;
- wherein the cleaning step is performed dry and comprises laser treatment which consists in scanning the fixing surface with a laser beam of sufficient power to eliminate the impurities present on said fixing surface.
2/ A method according to claim 1, in which during the cleaning step, the laser beam delivers energy to the fixing surface at a mean density per unit area lying in the range 0.5 J/cm2 to 20 J/cm2.
3/ A method according to claim 1, in which a pulse laser is used.
4/ A method according to claim 1, in which the fixing surface is scanned by the laser beam at a treatment speed of at least 2 cm2/s.
5/ A method according to claim 1, in which a laser is used selected from excimer lasers emitting in the ultraviolet and YAG lasers emitting in the infrared.
6/ A method according to claim 1, in which the insert is made of steel.
7/ A method according to claim 1, in which during the cleaning step the laser beam is used to deliver sufficient energy to the fixing surface of the metal insert to eliminate all traces of corrosion on said fixing surface.
8/ A method according to claim 1, in which the cleaning step is followed by a passivation step.
9/ A method according to claim 1, in which the cleaning step is followed directly by the coating step.
10/ A method according to claim 9, in which the coating step is implemented sufficiently quickly after the cleaning step to avoid any trace of corrosion reappearing on the fixing surface.
11/ A method according to claim 10, in which the coating step is implemented less than 24 hours after the end of the cleaning step.
12/ A method according to claim 1, in which during the cleaning step the laser beam is used to deliver sufficient energy to the fixing surface to etch said fixing surface to a small extent.
13/ A method according to claim 1, in which the elastomer is rubber.