# US 2003/0070937 A1 · Cells for the electrowinning of aluminium having dimensionally stable metal-based anodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0070937 A1
- Document ID: US20030070937A1
- Status: Published application
- Kind: A1
- Application number: 10/303,285
- Filed: 2002-11-25
- Published: 2003-04-17
- Earliest claimed: 2001-01-29
- Assignees: Moltech Invent S.A.
- Inventors: Jean-Jacques Duruz; Vittorio De Nora; Olivier Crottaz
- Web page: https://patentgrep.com/patent/US20030070937A1

## CPC

- C25C 3/06: of aluminium
- C25C 3/12: Anodes
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR

## Abstract

A cell for the electrowinning of aluminium comprising one or more anodes (10), each having a metal-based anode substrate, for instance comprising a metal core (11) covered with an metal layer 12, an oxygen barrier layer (13), one or more intermediate layers (14; 14A, 14B) and an iron layer (15). The anode substrate is covered with an electrochemically active transition metal oxide layer, in particular an iron oxide-based outside layer (16) such as a hematite-based layer, which remains dimensionally stable during operation in a cell by maintaining in the electrolyte a sufficient concentration of iron species and dissolved alumina. The cell operating temperature is sufficiently low so that the required concentration of iron species in the electrolyte (5) is limited by the reduced solubility of iron species in the electrolyte at the operating temperature, which consequently limits the contamination of the product aluminium by iron to an acceptable level. The iron oxide-based layer (16) is usually an applied coating or an oxidised surface of a substrate (11, 12, 13, 14, 15), the surface (15) of which contains iron.

## Claims

### Claim 1

A cell for the electrowinning of aluminium by the electrolysis of alumina dissolved in a molten fluoride-containing electrolyte, comprising one or more anodes, each having a metal-based substrate and an electrochemically-active iron oxide-based outside layer, in particular a hematite-based layer, which remains dimensionally stable by maintaining in the electrolyte a sufficient concentration of iron species and dissolved alumina, the cell operating temperature being sufficiently low so that the required concentration of iron species in the electrolyte is limited by the reduced solubility of iron species in the electrolyte at the operating temperature, which consequently limits the contamination of the product aluminium by iron to an acceptable level.

### Claim 2 (depends on 1)

The cell of claim 1, wherein the iron oxide-based outside layer is either an applied layer or obtainable by oxidising the surface of the anode substrate which contains iron.

### Claim 3 (depends on 2)

The cell of claim 2, wherein the anode substrate comprises a plurality of layers carrying the iron oxide-based layer.

### Claim 4 (depends on 3)

The cell of claim 3, wherein the anode substrate comprises an electrically conductive core layer covered with an oxygen barrier layer coated with at least one intermediate layer carrying the iron oxide-based layer.

### Claim 5 (depends on 4)

The cell of claim 4, wherein the oxygen barrier layer contains at least one oxide selected from chromium, niobium and nickel oxide.

### Claim 6 (depends on 4)

The cell of claim 4, wherein the intermediate layer contains copper, or copper and nickel, and/or their oxides.

### Claim 7 (depends on 1)

The cell of claim 1, wherein the anode substrate comprises at least one metal, an alloy, an intermetallic compound or a cermet.

### Claim 8 (depends on 7)

The cell of claim 7, wherein the anode substrate comprises at least one of nickel, copper, cobalt, chromium, molybdenum, tantalum, iron, and their alloys or intermetallic compounds, and combinations thereof.

### Claim 9 (depends on 8)

The cell of claim 8, wherein the anode substrate comprises an alloy consisting of 10 to 30 weight % of chromium, 55 to 90% of at least one of nickel, cobalt or iron, and 0 to 15% of aluminium, titanium, zirconium, yttrium, hafnium or niobium.

### Claim 10 (depends on 8)

The cell of claim 8, wherein the anode substrate contains an alloy of iron and at least one alloying metal selected from nickel, cobalt, molybdenum, tantalum, niobium, titanium, zirconium, manganese and copper.

### Claim 11 (depends on 10)

The cell of claim 10, wherein the substrate alloy comprises 30 to 70 weight % iron and 30 to 70 weight % nickel.

### Claim 12 (depends on 10)

The cell of claim 10, wherein the substrate alloy comprises an alloy of iron and cobalt.

### Claim 13 (depends on 1)

The cell of claim 1, wherein the operating temperature of the electrolyte is above 700° C., preferably between 820° C. and 870° C.

### Claim 14 (depends on 1)

The cell of claim 1, wherein the electrolyte contains NaF and AlF3 in a weight ratio NaF/AlF3 from 0.7 to 0.85.

### Claim 15 (depends on 1)

The cell of claim 1, wherein the concentration of alumina dissolved in the electrolyte is below 8 weight %, preferably between 2 weight % and 6 weight %.

### Claim 16 (depends on 1)

The cell of claim 1, comprising means for intermittently or continuously feeding iron species into the electrolyte to maintain an amount of iron species in the electrolyte preventing the dissolution of the iron oxide-based anode layer.

### Claim 17 (depends on 16)

The cell of claim 16, wherein the means for feeding iron species feeds iron metal and/or an iron compound.

### Claim 18 (depends on 17)

The cell of claim 17, wherein the means for feeding iron species feeds iron oxide, iron fluoride, iron oxyfluoride and/or an iron-aluminium alloy.

### Claim 19 (depends on 16)

The cell of claim 16, wherein the means for feeding iron species is arranged to periodically feed the iron species together with alumina into the electrolyte.

### Claim 20 (depends on 16)

The cell of claim 16, wherein the means for feeding iron species is a sacrificial electrode continuously feeding the iron species into the electrolyte.

### Claim 21 (depends on 20)

The cell of claim 20, wherein the sacrificial electrode is connected to a current supply arranged to apply a voltage which is lower than the voltage of oxidation of oxygen O— and supply a current controlling and/or promoting the dissolution of the sacrificial electrode into the electrolyte.

### Claim 22 (depends on 1)

The cell of claim 1, comprising an aluminium-wettable cathode.

### Claim 23 (depends on 22)

The cell of claim 22, comprising a drained cathode.

### Claim 24 (depends on 1)

The cell of claim 1, which is in a bipolar configuration.

### Claim 25 (depends on 1)

The cell of claim 1, comprising means to improve the circulation of the electrolyte between the anodes and facing cathodes and/or means to facilitate dissolution of alumina in the electrolyte.

### Claim 26 (depends on 1)

An anode which can be maintained dimensionally stable in a cell for the electrowinning of aluminium according to claim 1, having a metal-based substrate comprising at least one metal, an alloy, an intermetallic compound or a cermet, the substrate being covered with an iron oxide-based outside layer, in particular a hematite-based layer, which is electrochemically active for the oxidation of oxygen ions into molecular oxygen.

### Claim 27 (depends on 26)

The anode of claim 26, wherein the iron oxide-based outside layer is either an applied layer or obtainable by oxidising the surface of the anode substrate which contains iron.

### Claim 28 (depends on 27)

The anode of claim 27, wherein the iron oxide-based layer comprises a dense iron oxide outer portion, a microporous intermediate iron oxide portion and an inner portion containing iron oxide and a metal from the surface of the anode substrate.

### Claim 29 (depends on 27)

The anode of claim 27, wherein the anode substrate comprises a plurality of layers carrying the iron oxide-based layer.

### Claim 30 (depends on 29)

The anode of claim 29, wherein the anode substrate comprises an electrically conductive core layer covered with an oxygen barrier layer coated with at least one intermediate layer carrying the iron oxide-based layer.

### Claim 31 (depends on 30)

The anode of claim 30, wherein the oxygen barrier layer contains at least one oxide selected from chromium, niobium and nickel oxide.

### Claim 32 (depends on 30)

The anode of claim 30, wherein the intermediate layer contains copper, or copper and nickel, and/or their oxides.

### Claim 33 (depends on 26)

The anode of claims 26, wherein the anode substrate comprises at least one of nickel, copper, cobalt, chromium, molybdenum, tantalum, iron, and their alloys or intermetallic compounds, and combinations thereof.

### Claim 34 (depends on 33)

The anode of claim 33, wherein the anode substrate comprises an alloy consisting of 10 to 30 weight % of chromium, 55 to 90% of at least one of nickel, cobalt or iron, and 0 to 15% of aluminium, titanium, zirconium, yttrium, hafnium or niobium.

### Claim 35 (depends on 33)

The anode of claim 33, wherein the anode substrate contains an alloy of iron and at least one alloying metal selected from nickel, copper, cobalt, chromium, molybdenum, tantalum, iron, and their alloys or intermetallic compounds, and combinations thereof.

### Claim 36 (depends on 33)

The anode of claim 33, wherein the alloy substrate comprises 30 to 70 weight % iron and 30 to 70 weight % nickel.

### Claim 37 (depends on 33)

The anode of claim 33, wherein the substrate alloy comprises an alloy of iron and cobalt.

### Claim 38 (depends on 26)

A bipolar electrode which comprises on its anodic side an anode according to claim 26.

### Claim 39 (depends on 26)

A method of manufacturing an anode according to claim 26, said method comprising forming an iron oxide-based outside layer, in particular a hematite-based layer, on a metal-based anode substrate made of at least one metal, an alloy, an intermetallic compound or a cermet either by oxidising the anode surface of the substrate which contains iron, or by coating the iron oxide-based layer onto the substrate.

### Claim 40 (depends on 39)

The method of claim 39, wherein the iron oxide-based layer is formed chemically or electrochemically on the anode substrate.

### Claim 41 (depends on 39)

The method of claim 39, wherein the iron oxide-based layer is applied as a colloidal and/or polymeric slurry, and dried and/or heat treated.

### Claim 42 (depends on 41)

The method of claim 41, wherein the colloidal and/or polymeric slurry comprises at least one of alumina, ceria, lithia, magnesia, silica, thoria, yttria, zirconia, tin oxide and zinc oxide.

### Claim 43 (depends on 39)

The method of claim 39, wherein the iron oxide-based layer is formed by arc or plasma spraying iron oxide or iron onto the anode substrate followed by an oxidation treatment.

### Claim 44 (depends on 39)

The method of claim 39, wherein the iron oxide-based layer is formed, or consolidated, by heat treating an anode substrate, the surface of which contains iron and/or iron oxide, in an oxidising gas at a temperature above the operating temperature of the cell in which the anode is to be inserted.

### Claim 45 (depends on 44)

The method of claim 44, wherein the anode substrate is heat treated at a temperature of 950° C. to 1250° C.

### Claim 46 (depends on 43)

The method of claim 43, wherein the anode substrate is heat treated in air or in oxygen.

### Claim 47 (depends on 39)

The method of claim 39, wherein the iron oxide-based layer is formed on an anode substrate comprising a plurality of layers.

### Claim 48 (depends on 47)

The method of claim 47, wherein the anode substrate is made by forming on a core layer an oxygen barrier layer which is coated with at least one intermediate layer and the iron oxide-based outside layer, said oxygen barrier layer being formed before or after application of the intermediate layer(s).

### Claim 49 (depends on 48)

The method of claim 48, wherein the oxygen barrier layer is formed by applying a coating onto the core layer before application of the intermediate layer(s) or by surface oxidation of the core layer before or after application of the intermediate layer(s).

### Claim 50 (depends on 49)

The method of claim 49, wherein the oxygen barrier layer and/or the intermediate layer is/are formed by slurry application of a precursor.

### Claim 51 (depends on 49)

The method of claim 49, wherein the oxygen barrier layer and/or the intermediate layer is/are formed by arc or plasma spraying oxides thereof, or by arc or plasma spraying metals and forming the oxides by heat treatment.

### Claim 52 (depends on 26, 39)

The method of claim 39, for reconditioning an anode according to claim 26 whose iron oxide-based layer is damaged, the method comprising clearing at least the damaged parts of the iron oxide-based layer from the anode substrate and then reconstituting at least the iron oxide-based layer.

### Claim 53 (depends on 1)

A method of producing aluminium in a cell according to claim 1, the cell comprising an anode having a metal-based anode substrate and an iron oxide-based outside layer, in particular a hematite-based layer, which is electrochemically active for the oxidation of oxygen ions into molecular oxygen, said method comprising keeping the anode dimensionally stable during electrolysis by maintaining a sufficient concentration of iron species and dissolved alumina in the electrolyte, and operating the cell at a sufficiently low temperature so that the required concentration of iron species in the electrolyte is limited by the reduced solubility of iron species in the electrolyte at the operating temperature, which consequently limits the contamination of the product aluminium by iron to an acceptable level.

### Claim 54 (depends on 53)

The method of claim 53, wherein the cell is operated at an electrolyte temperature above 700° C., preferably between 820° C. and 870° C.

### Claim 55 (depends on 53)

The method of claim 53, wherein the cell is operated with an electrolyte containing NaF and AlF3 in weight ratio NaF/AlF3 from 0.7 to 0.85.

### Claim 56 (depends on 53)

The method of claim 53, wherein the amount of dissolved alumina contained in the electrolyte is maintained is below 8 weight %, preferably between 2 weight % and 6 weight %.

### Claim 57 (depends on 53)

The method of claim 53, wherein the amount of dissolved iron preventing dissolution of the iron oxide-based anode layer is such that the product aluminium is contaminated by no more than 2000 ppm iron, preferably by no more than 1000 ppm iron, and even more preferably by no more than 500 ppm iron.

### Claim 58 (depends on 53)

The method of claim 53, wherein iron species are intermittently or continuously fed into the electrolyte to maintain the amount of iron species in the electrolyte which prevents at the operating temperature the dissolution of the anode iron oxide-based layer.

### Claim 59 (depends on 58)

The method of claim 58, wherein the iron species are fed in the form of iron metal and/or an iron compound.

### Claim 60 (depends on 59)

The method of claim 59, wherein the iron species are fed into the electrolyte in the form of iron oxide, iron fluoride, iron oxyfluoride and/or an iron-aluminium alloy.

### Claim 61 (depends on 60)

The method of claim 60, wherein the iron species are periodically fed into the electrolyte together with alumina.

### Claim 62 (depends on 58)

The method of claim 58, wherein a sacrificial electrode continuously feeds the iron species into the electrolyte.

### Claim 63 (depends on 62)

The method of claim 62, comprising applying a voltage which is lower than the voltage of oxidation of oxygen O— and supplying an electric current to the sacrificial electrode to control and/or promote the dissolution of the sacrificial electrode into the electrolyte.

### Claim 64 (depends on 63)

The method of claim 63, comprising adjusting the electric current supplied to the sacrificial electrode so that it corresponds to a current necessary for the dissolution of the required amount of iron species into the electrolyte replacing the iron which is cathodically reduced and not otherwise compensated.

### Claim 65 (depends on 53)

The method of claim 53, for producing aluminium on an aluminium-wettable cathode.

### Claim 66 (depends on 65)

The method of claim 65, wherein the produced aluminium continuously drains from said aluminium-wettable cathode.

### Claim 67 (depends on 24, 53)

The method of claim 53, for producing aluminium in a bipolar cell according to claim 24, comprising passing an electric current from the surface of the terminal cathode to the surface of the terminal anode as ionic current in the electrolyte and as electronic current through the bipolar electrodes, thereby electrolysing the alumina dissolved in the electrolyte to produce aluminium on each cathode surface and oxygen on each anode surface.

### Claim 68 (depends on 53)

The method of claim 53, comprising circulating the electrolyte between the anodes and facing cathodes thereby improving dissolution of alumina into the electrolyte and/or improving the supply of dissolved alumina under the active surfaces of the anodes.

### Claim 69 (depends on 1)

A cell component which can be maintained dimensionally stable in a cell for the electrowinning of aluminium according to claim 1, having an iron oxide-based outside layer, in particular a hematite-based layer, which is electrochemically active for the oxidation of oxygen ions into molecular oxygen.

### Claim 70 (depends on 69)

The cell component of claim 69, wherein the hematite-based layer covers a metal-based substrate comprising at least one metal, an alloy, an intermetallic compound or a cermet.

### Claim 71

A cell for the electrowinning of aluminium by the electrolysis of alumina dissolved in a molten fluoride-containing electrolyte, comprising one or more anodes, each having a metal-based substrate and an electrochemically-active transition metal oxide-based outside layer which remains dimensionally stable by maintaining in the electrolyte a sufficient concentration of dissolved alumina and transition metal species which are present as one or more corresponding transition metal oxides in the electrochemically-active layer, the cell operating temperature being sufficiently low so that the required concentration of transition metal species in the electrolyte is limited by the reduced solubility thereof in the electrolyte at the operating temperature, which consequently limits the contamination of the product aluminium to an acceptable level by the transition metal(s) present as one or more corresponding transition metal oxides in the electrochemically-active layer.

### Claim 72 (depends on 71)

The cell of claim 71, wherein the electrochemically-active layer is made of an oxidised nickel-cobalt alloy which remains dimensionally stable by maintaining in the electrolyte a sufficient concentration of nickel and/or cobalt species.

### Claim 73 (depends on 72)

The cell of claim 72, wherein the cobalt nickel atomic ratio is in the range of 2 to 2.7.

### Claim 74 (depends on 71)

A method of producing aluminium in a cell according to claim 71, comprising an anode having a metal-based anode substrate and an electrochemically-active transition metal oxide-based outside layer, said method comprising keeping the anode dimensionally stable during electrolysis by maintaining a sufficient concentration of dissolved alumina and transition metal species which are present as one or more corresponding transition metal oxides in the electrochemically-active layer, and operating the cell at a sufficiently low temperature so that the required concentration of transition metal species in the electrolyte is limited by the reduced solubility thereof in the electrolyte at the operating temperature, which consequently limits the contamination of the product aluminium to an acceptable level by the transition metal(s) present as one or more corresponding transition metal oxides in the electrochemically-active layer.