# US 2003/0069339 A1 · Polybutylene terephthalate resin and compositions and molded articles comprising the resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0069339 A1
- Document ID: US20030069339A1
- Status: Published application
- Kind: A1
- Application number: 10/126,406
- Filed: 2002-04-19
- Published: 2003-04-10
- Earliest claimed: 2001-04-24
- Assignees: Mitsubishi Engineering-Plastics Corporation
- Inventors: Kunihiro Takenaka; Ryo Saito; Hidekazu Shoji
- Web page: https://patentgrep.com/patent/US20030069339A1

## CPC

- C08G 63/183: Terephthalic acids
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A polybutylene terephthalate resin having 30 eq/t or less of carboxyl end group, a crystallization temperature in a temperature decrease of 175° C. or higher and an amount of residual tetrahydrofuran of 300 ppm by weight or less; and compositions and molded articles comprising the resin and glass fiber, antioxidants and mold-releasing agents is provided. The polybutylene terephthalate resin can be molded in a short molding cycle, exhibits excellent resistance to hydrolysis and mold-releasing property, causes no corrosion of metals and generates little gas during molding. The compositions and the molded articles exhibit improved impact resistance, stability under heating and oxidation and mold-releasing property and can be advantageously used for members in electric and electronic products and in automobiles.

## Claims

### Claim 1

A polybutylene terephthalate resin having 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min.

### Claim 2 (depends on 1)

A resin according to claim 1, which has an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin.

### Claim 3 (depends on 1)

A resin according to claim 1, which has an amount of residual tetrahydrofuran of 50 to 300 ppm by weight in the polybutylene terephthalate resin.

### Claim 4 (depends on 1)

A resin according to claim 1, which has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in amounts by weight of 1/1.

### Claim 5 (depends on 1)

A resin according to claim 1, which is obtain ed by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 6

A polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the resin.

### Claim 7 (depends on 6)

A resin according to claim 6, which has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 8 (depends on 6)

A resin according to claim 6, which is prepared by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 9

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and glass fiber.

### Claim 10 (depends on 9)

A composition according to claim 9, wherein the polybutylene terephthalate resin has an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin.

### Claim 11 (depends on 9)

A composition according to claim 9, wherein the polybutylene terephthalate resin has an amount of residual tetrahydrofuran of 50 to 300 ppm.

### Claim 12 (depends on 9)

A composition according to claim 9, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in amounts by weight of 1/1.

### Claim 13 (depends on 9)

A composition according to claim 9, wherein the polybutylene terephthalate resin is obtained by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 14 (depends on 9)

A composition according to claim 9, which comprises glass fiber in an amount of 3 to 150 parts by weight per 100 parts by weight of the polybutylene terephthalate resin.

### Claim 15

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and glass fiber.

### Claim 16 (depends on 15)

A composition according to claim 15, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 17 (depends on 15)

A composition according to claim 15, wherein the polybutylene terephthalate resin is a resin produced by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 18

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and phenolic antioxidants.

### Claim 19 (depends on 18)

A composition according to claim 18, which further comprises at least one antioxidant selected from a group consisting of sulfur-based antioxidants and phosphorus-based antioxidants.

### Claim 20 (depends on 18)

A composition according to claim 18, wherein the phenolic antioxidants are hindered phenolic antioxidants.

### Claim 21 (depends on 19)

A composition according to claim 19, wherein the sulfur-based antioxidants are thioether-based antioxidants.

### Claim 22 (depends on 18)

A composition according to claim 18, which has an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin.

### Claim 23 (depends on 18)

A composition according to claim 18, the polybutylene terephthalate resin has an amount of residual tetrahydrofuran of 50 to 300 ppm.

### Claim 24 (depends on 18)

A composition according to claim 18, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 25 (depends on 18)

A composition according to claim 18, wherein the polybutylene terephthalate resin is a resin produced by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 26 (depends on 18)

A composition according to claim 18, which comprises the phenolic antioxidants in an amount of 0.001 to 2 parts by weight per 100 parts by weight of the polybutylene terephthalate resin.

### Claim 27

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and phenolic antioxidants.

### Claim 28 (depends on 27)

A composition according to claim 27, which further comprises at least one antioxidant selected from a group consisting of sulfur-based antioxidants and phosphorus-based antioxidants.

### Claim 29 (depends on 27)

A composition according to claim 27, wherein the phenolic antioxidants are hindered phenolic antioxidants.

### Claim 30 (depends on 28)

A composition according to claim 28, wherein the sulfur-based antioxidants are thioether-based antioxidants.

### Claim 31 (depends on 27)

A composition according to claim 27, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 32 (depends on 27)

A composition according to claim 27, wherein the polybutylene terephthalate resin is a resin produced by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 33

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and a fatty acid ester which has a residue group of a fatty acid having 12 to 36 carbon atoms and a residue group of an alcohol having 1 to 36 carbon atoms.

### Claim 34 (depends on 33)

A composition according to claim 33, which has an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin.

### Claim 35 (depends on 33)

A composition according to claim 33, wherein the polybutylene terephthalate resin has an amount of residual tetrahydrofuran of 50 to 300 ppm.

### Claim 36 (depends on 33)

A composition according to claim 33, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 37 (depends on 33)

A composition according to claim 33, wherein the polybutylene terephthalate resin is a resin produced by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 38 (depends on 33)

A composition according to claim 33, which comprises the fatty acid ester in an amount of 0.01 to 2 parts by weight per 100 parts by weight of the polybutylene terephthalate resin.

### Claim 39

A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and a fatty acid ester which has a residue group of a fatty acid having 12 to 36 carbon atoms and a residue group of an alcohol having 1 to 36 carbon atoms.

### Claim 40 (depends on 39)

A composition according to claim 39, wherein the polybutylene terephthalate resin has an inherent viscosity of 0.5 to 1.5 dl/g as measured at 30° C. in a mixed solvent composed of phenol and 1,1,2,2-tetrachloroethane in relative amounts by weight of 1/1.

### Claim 41 (depends on 39)

A composition according to claim 39, wherein the polybutylene terephthalate resin is a resin produced by continuous polycondensation using terephthalic acid and 1,4-butanediol as main raw materials.

### Claim 42 (depends on 1)

A molded article obtained by molding the polybutylene terephthalate resin described in claim 1.