Golf ball with polysulfide rubber layer
OwnerMichael J. Sullivaninventor
Life of this patent
Estimating the term…
Loading patent…
OwnerMichael J. Sullivaninventor
Estimating the term…
A golf ball with at least one moisture vapor barrier layer is disclosed. In accordance to one aspect of the invention, the moisture vapor barrier layer may comprise a polysulfide rubber Polysulfide rubber may be applied to the golf ball in a liquid form curable at an elevated temperature or at room temperature. The liquid form may be mixed from two or more components prior to being applied to the ball. The liquid form may have water mixed therein before being applied to the ball. Alternatively, the liquid form may be applied to the ball without any additional mixing. The polysulfide rubber may be formed from a solid form that has been heated to a flowable condition and extruded or cast to form the moisture vapor barrier layer. The polysulfide rubber may be dissolved in a solvent and applied to the ball, wherein the solvent is allowed to evaporate or otherwise flashed. The present invention is also directed to a golf ball comprising a layer of moisture vapor barrier with a moisture vapor transmission rate preferably lower than that of the cover. Preferably, the moisture vapor barrier layer comprises a material curable at room temperature. Preferably the moisture vapor barrier layer is a polysulfide rubber that is curable at room temperature.
A golf ball comprising a core, a moisture vapor barrier layer and a cover, wherein the moisture barrier layer has a moisture vapor transmission rate that is lower than that of the cover and wherein the moisture vapor barrier comprises a polysulfide rubber.
The golf ball of claim 27, wherein the additive is selected from a group consisting of curing agents, cure accelerated agents, cure retarding agents, pigments, fillers, deliquescent agents, desiccating agents.
A golf ball comprising a core, a moisture vapor barrier layer and a cover, wherein the moisture barrier layer has a moisture vapor transmission rate that is lower than that of the cover and wherein the moisture vapor barrier layer comprises a material curable at room temperature.
Dependencies are inferred from the claim text.