# US 2003/0068872 A1 · Laser annealing method and laser annealing device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0068872 A1
- Document ID: US20030068872A1
- Status: Published application
- Kind: A1
- Application number: 10/025,322
- Filed: 2001-12-18
- Published: 2003-04-10
- Earliest claimed: 1995-10-25
- Assignees: Semiconductor Energy Laboratory Co., Ltd., a Japanese corporation
- Inventors: Naoto Kusumoto; Toru Takayama; Masato Yonezawa
- Web page: https://patentgrep.com/patent/US20030068872A1

## CPC

- H10P 72/0454: {surrounding a central transfer chamber}
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3806: {using crystallisation-enhancing elements}
- H10P 14/3816: {Pulsed laser beam}
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H10P 72/0471: {comprising at least one ion or electron beam chamber}
- H10D 86/0251: {characterised by increasing the uniformity of device parameters}
- Y10S 438/905: Cleaning of reaction chamber
- Y10S 438/906: Cleaning of wafer as interim step
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A laser-annealing method includes the steps of a first step of cleaning a non-monocrystal silicon film formed on a substrate, and a second step of laser-annealing the non-monocrystal silicon film in an atmosphere containing oxygen therein, wherein the first and second steps are conducted continuously without being exposed to the air. Also, a laser-annealing device includes a cleaning chamber, and a laser irradiation chamber, wherein a substrate to be processed is transported between the cleaning chamber and the laser irradiation chamber without being exposed to the air.

## Claims

### Claim 1

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of a semiconductor film; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in a nitrogen atmosphere.

### Claim 2 (depends on 1)

A method according to claim 1, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 3 (depends on 1)

A method according to claim 1, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 4

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of said semiconductor film;
preheating said semiconductor film; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in a nitrogen atmosphere.

### Claim 5 (depends on 4)

A method according to claim 4, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 6 (depends on 4)

A method according to claim 4, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 7

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of said semiconductor film;
preheating said semiconductor film in an atmosphere containing oxygen and nitrogen; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in a nitrogen atmosphere.

### Claim 8 (depends on 7)

A method according to claim 7, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 9 (depends on 7)

A method according to claim 7, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 10

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of said semiconductor film;
preheating said semiconductor film to form an oxide film on a surface of said semiconductor film; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in a nitrogen atmosphere.

### Claim 11 (depends on 10)

A method according to claim 10, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 12 (depends on 10)

A method according to claim 10, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 13

A method for manufacturing a semiconductor device comprising the steps of:
forming a crystalline semiconductor film over a substrate;
cleaning a surface of said crystalline semiconductor film; and
applying a laser beam to said crystalline semiconductor film to improve crystallinity of said crystalline semiconductor film in a nitrogen atmosphere.

### Claim 14 (depends on 13)

A method according to claim 13, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 15 (depends on 13)

A method according to claim 13, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 16

A method for manufacturing a semiconductor device comprising the steps of:
forming a crystalline semiconductor film over a substrate;
cleaning a surface of said crystalline semiconductor film;
preheating said crystalline semiconductor film; and
applying a laser beam to said crystalline semiconductor film to improve crystallinity of said crystalline semiconductor film in a nitrogen atmosphere.

### Claim 17 (depends on 16)

A method according to claim 16, wherein said cleaning is performed by using HF aqueous solution or an aqueous solution containing HF and H2O2.

### Claim 18 (depends on 16)

A method according to claim 16, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 19

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of said semiconductor film;
forming an oxide film on a surface of said semiconductor film; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in the air.

### Claim 20 (depends on 19)

A method according to claim 19, wherein said laser beam is a linear laser beam.

### Claim 21 (depends on 19)

A method according to claim 19, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 22 (depends on 19)

A method according to claim 19, wherein said oxide film has a thickness of 20-40 Å.

### Claim 23

A method for manufacturing a semiconductor device comprising the steps of:
forming a semiconductor film over a substrate;
cleaning a surface of said semiconductor film by using HF aqueous solution or an aqueous solution containing HF and H2O2;
forming an oxide film on a surface of said semiconductor film; and
applying a laser beam to said semiconductor film to form a crystalline semiconductor film in the air.

### Claim 24 (depends on 23)

A method according to claim 23, wherein said laser beam is a linear laser beam.

### Claim 25 (depends on 23)

A method according to claim 23, wherein said laser beam has an energy density of 100 to 500 mJ/cm2.

### Claim 26 (depends on 23)

A method according to claim 23, wherein said oxide film has a thickness of 20-40 Å.