# US 2003/0068490 A1 · Phthalate polyester polyol-based compositions and high dimensionally stable all water-blown spray polyurethane foam produced therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0068490 A1
- Document ID: US20030068490A1
- Status: Published application
- Kind: A1
- Application number: 10/173,070
- Filed: 2002-06-17
- Published: 2003-04-10
- Earliest claimed: 2001-06-15
- Inventors: Warren A. Kaplan
- Web page: https://patentgrep.com/patent/US20030068490A1

## CPC

- C08G 18/26: of lead
- C08G 18/281: {Monocarboxylic acid compounds}
- C08G 18/4018: {Mixtures of compounds of group C08G18/42 with compounds of group C08G18/48}
- C08G 18/4211: {derived from aromatic dicarboxylic acids and dialcohols}
- C08G 18/4213: {from terephthalic acid and dialcohols}
- C08G 18/5021: {having nitrogen}
- C08G 2110/0025: rigid
- C08G 2110/005: < 50kg/m3
- C08G 2110/0083: prepared using water as the sole blowing agent
- Y10T 428/28: Web or sheet containing structurally defined element or component and having an adhesive outermost layer
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to methods and compositions for preparing all water blown spray polyurethane foams by reacting a polyisocyanate with a polyol blend. The polyol methods and compositions of the invention comprises a polyol component, water, a cell opening agent and a diluent. Polyurethane foams prepared according to the invention meet the physical and processing requirements stipulated by the industry.

## Claims

### Claim 1

A method for preparing a polymeric foam comprising urethane units and having an open-cell content sufficient to resist shrinkage, the method comprising reacting an aromatic polymeric isocyanate with a polyol blend at an NCO/OH index of from about 85-125, where the polyol blend comprises:
(a) from about 20% to about 90% by weight of the blend of a polyol formulation comprising a polyester polyol, a polyether polyol, a Mannich-type polyol, or mixtures thereof;
(b) a blowing agent;
(c) a cell opening agent which is a divalent metal salt of a fatty acid; and
(d) from about 0.05% to about 50% by weight of the blend of a diluent or mixture of diluents.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the polyol formulation comprises from about 25%-75% by weight of a polyester polyol or a mixture of polyester polyols.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the polyester polyol has an OH value of from about 150 to about 350 and a molecular weight of from about 350 to 700.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the polyol blend comprises from about 0.05%-3% by weight of the blend of a cell opening agent.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the polyol blend comprises from about 3.5-50% by weight of the blend of a diluent.

### Claim 6 (depends on 3)

A method according to claim 3, where the blend comprises from about 28-80% by weight of a polyester polyol.

### Claim 7 (depends on 6)

A method according to claim 6 wherein the diluent comprises tris-isopropylchlorophosphate, alkoxylated nonyl phenol, propylene carbonate, an alkyl ester of a monobasic acid, a dialkyl ester of a dibasic acid, or mixtures thereof.

### Claim 8 (depends on 7)

A method according to claim 7 wherein the polyol blend further comprises up to about 5% by weight of an acid based on the weight of the polyol blend.

### Claim 9 (depends on 7)

A method according to claim 7 wherein the polyol blend further comprises a surfactant.

### Claim 10 (depends on 7)

A method according to claim 7, wherein the polyol blend comprises from about 0.05%-1.5% by weight of the cell opening agent, based on the weight of the blend.

### Claim 11 (depends on 10)

A method according to claim 10, wherein the cell opening agent has a softening point of from about 100-180° C.

### Claim 12 (depends on 11)

A method according to claim 11, wherein the aromatic polymeric isocyanate is a polymethylene polyphenyl isocyanate.

### Claim 13 (depends on 1)

A method according to claim 1, wherein the blowing agent comprises water.

### Claim 14 (depends on 1)

A method according to claim 1, wherein the polyol blend comprising the cell opening agent is a stable dispersion.

### Claim 15 (depends on 1)

A polyurethane foam prepared according to the method of claim 1 having an in-place density of from about 2.0 to 3.5 lbs./ft3.

### Claim 16 (depends on 1)

A polyurethane foam prepared according to the method of claim 1, wherein the foam comprises from about 0.01 to 1% by weight of a cell opening agent which is a divalent metal salt of a fatty acid, the foam having an open-cell content sufficient to resist shrinkage and exhibiting less than about 5% shrinkage when stored at about 158° F. and about 100% relative humidity for about 28 days.

### Claim 17 (depends on 13)

A polyurethane foam according to claim 13 exhibiting less than about 3% shrinkage when stored at −20° F. for 28 days.

### Claim 18 (depends on 3)

A method according to claim 3, wherein the acid is an alkanoic acid or an alkenoic acid.

### Claim 19 (depends on 1)

A method according to claim 1, wherein the polyol formulation comprises from about 1% to 100% by weight of a diethylene glycol phthalate polyester polyol having an OH value of from about 150 to 350 and comprising
(a) the reaction product of a mixture comprising a phthalic acid compound and a low molecular weight aliphatic diol, and
(b) an optional nonionic surfactant, and
where the diethylene glycol phthalate polyester polyol has a molecular weight of from about 350 to 700.

### Claim 20 (depends on 19)

A method according to claim 19 further comprising up to about 5% by weight of an alkanoic or alkenoic acid based on the weight of the polyol blend.

### Claim 21 (depends on 20)

A method according to claim 20, wherein the alkanoic or alkenoic acid has the formula RCO2H, where R is hydrogen, a straight or branched chain alkyl group having from about 1 to 12 carbon atoms, or a straight or branched chain alkenyl group having from about 2 to 12 carbon atoms.

### Claim 22

A polyol blend suitable for use in a method for preparing a polymeric foam comprising urethane units and having an open-cell content sufficient to resist shrinkage comprising reacting an aromatic polymeric isocyanate with a polyol blend at an NCO/OH index of from about 85-125,
the polyol blend comprising:
(a) from about 20% to about 90% by weight of the blend of a polyol formulation comprising a polyester polyol, a polyether polyol, a Mannich-type polyol, or mixtures thereof;
(b) a blowing agent;
(c) a cell opening agent which is a divalent metal salt of a fatty acid; and
(d) from about 0.05% to about 50% by weight of the blend of a diluent or mixture of diluents.

### Claim 23 (depends on 22)

A blend according to claim 22, where the polyol blend comprises from about 50-85% by weight of a polyol formulation comprising a modified diethylene glycol phthalate polyester polyol having an OH value of about 290-325, an Mannich type polyol having an OH value of 415-435, and diethylene glycol.

### Claim 24 (depends on 23)

A blend according to claim 23, where the blowing agent is water, the cell opener is calcium stearate, and the diluent is selected from the group consisting of tris-isopropylchlorophosphate, an alkoxylated nonyl phenol, propylene carbonate, a monobasic ester, a dibasic ester and mixtures thereof, and
where the blend further comprises a catalyst selected from the group consisting of dimethylethanolamine, dimethylcyclohexylamine, a catalyst which contains about 70% bis(2-dimethylaminoethyl) ether in 30% dipropylene glycol or a mixture thereof; and
a surfactant, where the surfactant comprises an alkoxylated polysiloxane surfactant.

### Claim 25 (depends on 22)

A blend according to claim 22, wherein the polyol blend comprises about
(a) 30-40% by weight of a modified diethylene glycol phthalate polyester polyol having an OH value of about 290-325 and/or a modified diethylene glycol phthalate polyester polyol having an OH value of about 230-250;
(b) 20-30% by weight of an Mannich type polyol having an OH value of 415-435;
(c) 5.5-9% by weight of diethylene glycol
(d) 1-3% by weight of water;
(e) 0.1-1% by weight of the cell opener; and
(f) about 18-34% by weight of the diluent.

### Claim 26 (depends on 25)

A blend according to claim 25, where the polyol blend further comprises about
(g) 2.5-4.5% by weight of an amine catalyst; and
(f) 1-3% by weight of the surfactant.

### Claim 27

A polyol blend suitable for use in a method for preparing a polymeric foam comprising urethane units and having an open-cell content sufficient to resist shrinkage comprising reacting an aromatic polymeric isocyanate with a dispersed polyol blend at an NCO/OH index of from about 85-125, the polyol blend comprising:
(a) a polyol formulation comprising
(i) a modified diethylene glycol phthalate polyester polyol having an OH value of about 290-325, or
(ii) a modified diethylene glycol phthalate polyester polyol having an OH value of about 230-250, a Mannich type polyol having an OH value of 415-435, and diethylene glycol;
(b) water;
(c) a cell opener comprising calcium stearate;
(d) a diluent selected from the group consisting of tris-isopropylchlorophosphate, an alkoxylated nonyl phenol, propylene carbonate, a monobasic ester, a dibasic ester and mixtures thereof;
(e) a catalyst selected from the group consisting of dimethylethanolamine, dimethylcyclohexylamine, a catalyst which contains about 70% bis(2-dimethylaminoethyl) ether in 30% dipropylene glycol or a mixture thereof; and
(f) an alkoxylated polysiloxane surfactant.

### Claim 28 (depends on 27)

A polyol blend according to claim 27, comprising, based on the weight of the blend,
about 30-40% by weight of the modified diethylene glycol phthalate polyester polyol having an OH value of about 290-325 and/or the modified diethylene glycol phthalate polyester polyol having an OH value of about 230-250,
from about 20-30% by weight of the Mannich type polyol having an OH value of 415-435,
from about 6-8% by weight of diethylene glycol,
from about 1-3% by weight of water,
from about 0.1-2.5% by weight of the cell opener, and
from about 20-34% by weight of the diluent.

### Claim 29 (depends on 22)

A method according to claim 22, where the polyol blend comprises from about 50-85% by weight of a polyol formulation comprising a modified diethylene glycol phthalate polyester polyol having an OH value of about 230-250, an Mannich type polyol having an OH value of 415-435, and diethylene glycol.

### Claim 30 (depends on 22)

A polyol blend according to claim 22, wherein the diluent is propylene carbonate, an alkoxylated nonyl phenol, tris-isopropylchlorophosphate, monomethyl dipropylene glycol, monomethyl tripropylene glycol, a dibasic ester mixture, or a mixture thereof.

### Claim 31 (depends on 30)

A polyol blend according to claim 30, wherein the diluent is a mixture comprising an alkoxylated nonyl phenol and tris-isopropylchlorophosphate.

### Claim 32 (depends on 22)

A reaction mixture comprising the polyol blend of claim 22 and a polyisocyanate.

### Claim 33 (depends on 32)

A reaction mixture according to claim 32, wherein the polyol blend and polyisocyanate are present in the mixture at a volume ratio of about 1:1.

### Claim 34 (depends on 32)

A spray foam generated by the reaction product of claim 32.

### Claim 35 (depends on 33)

A spray foam according to claim 33, where the foam comprises open celled foam.

### Claim 36 (depends on 37)

A foam according to claim 37, where the foam has a sprayed in-place density of from about 2.0 to 3.5 pcf.

### Claim 37 (depends on 22)

A polyol blend according to claim 22, wherein the modified diethylene glycol phthalate polyester polyol having an OH value of about 290-325 or the modified diethylene glycol phthalate polyester polyol having an OH value of about 230-250 is about 32-33% by weight of the blend, the Mannich type polyol having an OH value of 415-435 is about 21-22% by weight of the blend, the diethylene glycol is about 7-8% by weight of the blend, the water is 1-2% by weight of the blend, the cell opener is about 0.15-2.25% by weight of the blend, the diluent is about 20-35% by weight of the blend, catalyst is about 2.5-4% by weight of the blend, and surfactant is from about 1-3% by weight of the blend.