# US 2003/0050707 A1 · Novel cermets and molten metal infiltration method and process for their fabrication

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0050707 A1
- Document ID: US20030050707A1
- Status: Published application
- Kind: A1
- Application number: 08/829,034
- Filed: 1997-03-31
- Published: 2003-03-13
- Earliest claimed: 1997-03-31
- Inventors: RICHARD L. LANDINGHAM
- Web page: https://patentgrep.com/patent/US20030050707A1

## CPC

- C04B 41/009: {characterised by the material treated}
- A61L 27/427: {of other specific inorganic materials not covered by A61L27/422 or A61L27/425}
- A61L 31/128: {containing other specific inorganic fillers not covered by A61L31/126 or A61L31/127}
- C04B 41/5133: {with a composition mainly composed of one or more of the refractory metals}
- C04B 41/88: Metals
- C22C 1/1021: {the preform being ceramic}
- C22C 1/1036: {starting from a melt}
- A61F 2/28: Bones
- A61F 2/30: Joints
- A61F 2002/30968: {Sintering}
- A61F 2310/00185: based on metal oxides
- A61F 2310/00191: containing beryllium oxide
- A61F 2310/00203: containing alumina or aluminium oxide
- A61F 2310/00251: containing hafnia or hafnium oxide
- A61F 2310/00263: based on metal borides
- A61F 2310/00299: based on metal nitrides
- A61F 2310/00311: containing aluminium nitride
- C04B 2111/00836: {for medical or dental applications}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)

## Abstract

Cermet comprising ceramic and metal components and a molten metal infiltration method and process for fabrication thereof. The light weight cermets having improved porosity, strength, durability, toughness, elasticity fabricated from presintered ceramic powder infiltrated with a molten metal or metal alloy. Alumina titanium cermets biocompatible with the human body suitable for bone and joint replacements.

## Claims

### Claim 1

A cermet comprising a ceramic powder presintered into a porous ceramic matrix and infiltrated with a molten metal or metal alloy.

### Claim 2 (depends on 1)

The cermet of claim 1 wherein the ceramic powder is selected from the group consisting of aluminum oxide, beryllium oxide, zirconium oxide, hafnium oxide, vanadium oxide, aluminum nitride, beryllium nitride, zirconium nitride, hafnium nitride, vanadium nitride, aluminum boride, beryllium borate, zirconium boride, hafnium boride, vanadium boride, aluminum silicate, zirconium silicate, hafnium silicate, vanadium silicate, beryllium silicate and a mixture thereof.

### Claim 3 (depends on 2)

The cermet of claim 2 wherein the infiltrating metal or metal alloy is selected from the group consisting of titanium, aluminum, magnesium, nickel, lithium, copper, iron, silicon, manganese, cobalt, molybdenum, niobium, zirconium, calcium and their combination.

### Claim 4 (depends on 3)

The cermet of claim 3 wherein the metal or metal alloy is infiltrated into a ceramic powder presintered into a porous ceramic matrix at a temperature higher than is the melting point of the infiltrating metal or metal alloy.

### Claim 5 (depends on 4)

The cermet of claim 4 wherein the ceramic powder is aluminum oxide having particle sizes from about 10 to about 50 microns.

### Claim 6 (depends on 5)

The cermet of claim 5 wherein the aluminum oxide has particle sizes about 10 microns.

### Claim 7 (depends on 6)

The cermet of claim 6 wherein the aluminum oxide is presintered into the porous ceramic matrix at temperature from about 1450° C. to about 1550° C. and infiltrated with molten titanium alloy at temperature lower than 1450° C.

### Claim 8 (depends on 7)

The cermet of claim 7 wherein the porous ceramic matrix has about zero to about 50 degrees wetting angle.

### Claim 9 (depends on 8)

The cermet of claim 8 wherein the particle sizes of the presintered porous ceramic matrix are about the same as the particle sizes of the ceramic powder used.

### Claim 10 (depends on 9)

The cermet of claim 9 wherein the metal alloy is binary, ternary or quaternary alloy selected from alloys shown in Table 1.

### Claim 11

A bone implant fabricated from a cermet comprising a ceramic powder presintered into a porous ceramic matrix and infiltrated with a molten metal or metal alloy.

### Claim 12 (depends on 11)

The implant of claim 11 wherein the ceramic powder is selected from the group consisting of aluminum oxide, zirconium oxide, hafnium oxide, vanadium oxide, aluminum nitride, zirconium nitride, hafnium nitride, vanadium nitride, aluminum boride, zirconium boride, hafnium boride, vanadium boride, aluminum silicate, zirconium silicate, hafnium silicate, vanadium silicate, beryllium oxide, beryllium nitride, beryllium borate, beryllium silicate and a mixture thereof.

### Claim 13 (depends on 12)

The implant of claim 12 wherein the infiltrating metal or metal alloy is selected from the group consisting of titanium, aluminum, magnesium, nickel, lithium, copper, iron, silicon, manganese, cobalt, molybdenum, niobium, zirconium, calcium and their combination.

### Claim 14 (depends on 13)

The implant of claim 13 wherein the ceramic powder is pressed into a near-net shape of the bone implant, presintered into a porous ceramic matrix at a temperature higher than is the melting point of the infiltrating metal or metal alloy and infiltrated with the molten metal or metal alloy at temperature lower than the sintering temperature of the ceramic powder.

### Claim 15 (depends on 14)

The implant of claim 14 wherein the ceramic powder is aluminum oxide having particle sizes from about 10 to about 50 microns presintered into the porous ceramic matrix at temperature from about 1450° C. to about 1550° C. and infiltrated with molten titanium alloy at temperature lower than 1450° C.

### Claim 16 (depends on 15)

The implant of claim 15 wherein the porous ceramic matrix has about zero to about 50 degrees wetting angle.

### Claim 17 (depends on 16)

The implant of claim 16 wherein the particle sizes of the aluminum oxide presintered into a porous ceramic matrix are about the same as the particle sizes of aluminum oxide used.

### Claim 18 (depends on 17)

The implant of claim 17 wherein the metal alloy is binary, ternary or quaternary alloy selected from alloys shown in Table 1 having the melting point lower than 1450° C.

### Claim 19

A process for fabrication of cermets comprising of a ceramic powder infiltrated with a molten metal or metal alloy, said process comprising steps:
(a) presintering a ceramic powder selected from the group consisting of any one or a mixture of aluminum oxide, aluminum nitride, aluminum boride, aluminum silicate, hafnium oxide, hafnium nitride, hafnium boride, hafnium silicate, vanadium oxide, vanadium nitride, vanadium boride, vanadium silicate, beryllium oxide, beryllium nitride, beryllium borate and beryllium silicate at its sintering temperature and proper atmospheres into a porous ceramic matrix of a desired shape;
(b) molten metal infiltrating the matrix of step (a) with a metal selected from the group consisting of titanium, nickel, magnesium, calcium, aluminum, lithium, copper, iron, silicon, manganese, cobalt, molybdenum, niobium, zirconium, and their combination wherein said selected metal having a melting point lower than the sintering temperature of the powder of step (a).

### Claim 20 (depends on 21)

The process of claim 21 wherein additionally a wetting angle of the metal or metal alloy is determined before the compact of step (a) is infiltrated.

### Claim 21 (depends on 20)

The process of claim 20 wherein the wetting angle for the metal and ceramic compact interaction is zero or is not larger than about 60 degrees.

### Claim 22 (depends on 21)

The process of claim 21 wherein the ceramic powder is presintered under vacuum.

### Claim 23 (depends on 22)

The process of claim 22 wherein the molten metal is infiltrated evenly into the ceramic presintered compact.

### Claim 24 (depends on 23)

The process of claim 23 wherein the ceramic powder is aluminum oxide.

### Claim 25 (depends on 24)

The process of claim 24 wherein the aluminum oxide powder has particle sizes from about 10 μ to about 50 μ.

### Claim 26 (depends on 25)

The process of claim 25 wherein the sintering temperature is between 1400° C. and 1660° C.

### Claim 27 (depends on 26)

The process of claim 26 wherein the aluminum oxide has particle sizes about 10 μ.

### Claim 28 (depends on 27)

The process of claim 27 wherein the sintering temperature is about 1500° C.

### Claim 29 (depends on 28)

The process of claim 28 wherein the metal used for molten-metal-infiltration is titanium alloy.

### Claim 30 (depends on 29)

The process of claim 29 wherein the temperature used for titanium alloy is lower than the sintering temperature of the ceramic powder compact.

### Claim 31 (depends on 30)

The process of claim 30 wherein the metal is the titanium alloy selected from the group of binary, ternary and quaternary alloy shown in Table 1.

### Claim 32 (depends on 31)

The process of claim 31 wherein the titanium alloy contains about 20-30% of nickel.

### Claim 33 (depends on 32)

The process of claim 32 wherein the temperature for molten-metal-infiltration is under 1500° C.

### Claim 34 (depends on 33)

The process of claim 33 wherein the ceramic powder additionally contains an additive selected for the group consisting of calcium oxide, magnesium oxide and sulfur present in an amount for about 0.01 to about 1%.