# US 2003/0010064 A1 · Method of producing optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2003/0010064 A1
- Document ID: US20030010064A1
- Status: Published application
- Kind: A1
- Application number: 10/203,010
- Filed: 2002-08-05
- Published: 2003-01-16
- Earliest claimed: 2000-12-05
- Inventors: Kazuya Kuwahara; Ichiro Tsuchiya
- Web page: https://patentgrep.com/patent/US20030010064A1

## CPC

- C03C 13/04: Fibre optics, e.g. core and clad fibre compositions (light guides G02B6/00)
- C03C 25/00: Surface treatment of fibres or filaments made from glass, minerals or slags
- C03C 25/60: by diffusing ions or metals into the surface
- C03C 25/607: in the gaseous phase
- C03C 25/628: Atoms
- G02B 6/03627: {arranged - +}
- G02B 6/02261: {Dispersion compensating fibres, i.e. for compensating positive dispersion of other fibres}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method of making an optical fiber employing a wavelength in an infrared region as a wavelength band in use is provided, in which an optical fiber 1 is exposed to an atmosphere containing hydrogen at a concentration of 0.05 vol % but not higher than 4.0 vol % after being drawn and taken up with a bobbin 2 before being put into use, whereas the hydrogen treatment temperature is lower than 50° C., preferably 30° C. or lower, more preferably at room temperature, whereby the increase in loss caused by hydrogen is small even when the optical fiber is used in a wide band, so that the optical fiber can be made efficiently and safely with an optimal hydrogen treatment.

## Claims

### Claim 1

A method of making an optical fiber employing a wavelength in an infrared region as a wavelength band in use, said method comprising the step of exposing said optical fiber to an atmosphere containing hydrogen at a concentration of at least 0.05 vol % but not higher than 4.0 vol % after said optical fiber is drawn and taken up with a bobbin before being put into use.

### Claim 2 (depends on 1)

A method of making an optical fiber according to claim 1, wherein said hydrogen-containing atmosphere has a temperature lower than 50° C.

### Claim 3 (depends on 2)

A method of making an optical fiber according to claim 2, wherein said hydrogen-containing atmosphere has a temperature of 30° C. or lower.

### Claim 4 (depends on 1, 2, 3)

A method of making an optical fiber according to one of claims 1 to 3, wherein transmission loss at a wavelength of 1.24 μm yields a difference of at least 0.005 dB/km between before and after the exposure to said hydrogen-containing atmosphere.

### Claim 5 (depends on 1, 2, 3, 4)

A method of making an optical fiber according to one of claims 1 to 4, wherein said optical fiber is one having a core part doped with a high concentration of germanium such that a center core part exhibits a relative refractive index difference Δn of at least 1% with respect, to a cladding.