# US 2002/0176042 A1 · Liquid crystal display device and fabricating method thereof, and reworking method of alignment film using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0176042 A1
- Document ID: US20020176042A1
- Status: Published application
- Kind: A1
- Application number: 10/005,867
- Filed: 2001-12-07
- Published: 2002-11-28
- Earliest claimed: 2001-05-24
- Assignees: LG.Philips LCD Co., Ltd.
- Inventors: Kyo Ho Moon; Yong In Park
- Web page: https://patentgrep.com/patent/US20020176042A1

## CPC

- G02F 1/136227: {Through-hole connection of the pixel electrode to the active element through an insulation layer}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 1/133711: {by organic films, e.g. polymeric films}
- C09K 2323/00: Functional layers of liquid crystal optical display excluding electroactive liquid crystal layer characterised by chemical composition
- Y10S 438/906: Cleaning of wafer as interim step
- Y10S 438/963: Removing process residues from vertical substrate surfaces
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A liquid crystal display device includes a substrate, an organic insulating film formed on the substrate, an alignment film having a first etch rate formed on the organic insulating film, and a silicon nitride layer having a second etch rate formed between the alignment film and the organic insulating film, wherein the first etch rate is different from the second etch rate.

## Claims

### Claim 1

A liquid crystal display device, comprising:
a substrate;
an organic insulating film formed on the substrate;
an alignment film having a first etch rate formed on the organic insulating film; and
a silicon nitride layer having a second etch rate formed between the alignment film and the organic insulating film,
wherein the first etch rate is different from the second etch rate.

### Claim 2 (depends on 1)

The device according to claim 1, wherein the alignment film is eliminated by dry-etching during rework processing.

### Claim 3 (depends on 2)

The device according to claim 2, wherein the dry-etching is carried out by using at least one compound gas of SF6, O2, O2+Cl2, and CF4.

### Claim 4 (depends on 3)

The device according to claim 3, wherein a ratio of the compound gas is at least about SF6:O2=1:50.

### Claim 5 (depends on 3)

The device according to claim 3, wherein a ratio of the compound gas is at least about SF6:O2=1:70.

### Claim 6 (depends on 3)

The device according to claim 3, wherein the dry-etching usess a radio frequency power of about 500-1500W.

### Claim 7 (depends on 1)

The liquid crystal display device according to claim 1, wherein the silicon nitride layer includes hydrogen.

### Claim 8 (depends on 1)

The device according to claim 1, further comprising:
a gate line on the substrate;
a data line crossing the gate line;
a gate electrode connected to the gate line;
a gate insulating film covering the gate electrode and the gate line;
a semiconductor layer formed on the gate insulating film;
a source electrode connected to the data line; and
a drain electrode formed away from the source electrode with a channel of a fixed size formed therebetween.

### Claim 9 (depends on 8)

The device according to claim 8, wherein a pixel electrode electrically contacts the drain electrode and overlaps at least one of the data line and the gate line.

### Claim 10

A method of fabricating a liquid crystal display device, comprising the steps of:
forming an organic insulating film on a substrate;
forming an alignment film having a first etch rate on the organic insulating film; and
forming a silicon nitride layer having a second etch rate between the alignment film and the organic insulating film,
wherein the first etch rate is different from the second etch rate.

### Claim 11 (depends on 10)

The method according to claim 10, further including eliminating the alignment film by dry-etching during rework processing.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the dry-etching is carried out by using at least one compound gas of SF6, O2, O2+Cl2, and CF4.

### Claim 13 (depends on 12)

The method according to claim 12, wherein a ratio of the compound gas is at least about SF6:O2=1:50.

### Claim 14 (depends on 12)

The method according to claim 12, wherein a ratio of the compound gas is at least about SF6:O2=1:70.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the dry-etching uses a radio frequency power of about 500-1500W.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the silicon nitride layer includes hydrogen.

### Claim 17 (depends on 10)

The method according to claim 10, further including the steps of:
forming a gate line and a gate electrode on the substrate;
forming a gate insulating film on the gate line, the gate electrode and the substrate;
forming a semiconductor layer on the gate insulating film; and
forming a data line, a source electrode and a drain electrode on the gate insulating film.

### Claim 18 (depends on 17)

The method according to claim 17, further including the step of forming a pixel electrode on the silicon nitride layer to overlap at least one of the data line and the gate line.

### Claim 19

A method of reworking an alignment film of a liquid crystal display device, comprising the steps of:
forming an organic protective film on a substrate;
forming a silicon nitride layer having a first etch rate on the organic protective film;
forming a first alignment film on the silicon nitride layer;
detecting at least one irregularity of the first alignment film formed on the silicon nitride layer;
eliminating the first alignment film with a second etch rate different from the first etch rate of the silicon nitride layer; and
forming a second alignment film on the silicon nitride layer.

### Claim 20 (depends on 19)

The method of according to claim 19, wherein the step of eliminating the first alignment film includes dry-etching during rework processing.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the dry-etching is carried out by using at least one compound gas of SF6, O2, O2+Cl2, and CF4.

### Claim 22 (depends on 21)

The method according to claim 21, wherein a ratio of the compound gas is at least about SF6:O2=1:50.

### Claim 23 (depends on 21)

The method according to claim 21, wherein a ratio of the compound gas is at least about SF6:O2=1:70.

### Claim 24 (depends on 21)

The method according to claim 21, wherein the dry-etching includes a radio frequency power of about 500-1500W.

### Claim 25 (depends on 19)

The method according to claim 19, wherein the silicon nitride layer includes hydrogen.

### Claim 26 (depends on 19)

The method according to claim 19, further including the steps of:
forming a gate line and a gate electrode on the substrate;
forming a gate insulating film on the gate line, the gate electrode and the substrate;
forming a semiconductor layer on the gate insulating film; and
forming a data line, a source electrode and a drain electrode on the gate insulating film.

### Claim 27 (depends on 26)