# US 2002/0173063 A1 · Method for monolithic integration of multiple devices on an optoelectronic substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0173063 A1
- Document ID: US20020173063A1
- Status: Published application
- Kind: A1
- Application number: 09/821,212
- Filed: 2001-03-29
- Published: 2002-11-21
- Earliest claimed: 2001-03-29
- Assignees: Agere Systems Inc.
- Inventors: Si Hyung Cho; Ronald E. Leibenguth; Abdullah Ougazzaden; Claude L. Reynolds
- Web page: https://patentgrep.com/patent/US20020173063A1

## CPC

- H01S 5/026: Monolithically integrated components, e.g. waveguides, monitoring photo-detectors, drivers (stabilisation of output H01S5/06)
- H01S 5/0265: {Intensity modulators (intra-cavity modulators H01S5/0625)}
- H01S 5/4031: {Edge-emitting structures}
- H01S 5/50: Amplifier structures not provided for in groups H01S5/02 - H01S5/30
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL

## Abstract

The present invention provides a method for monolithic integration of multiple devices on an optoelectronic substrate. The method, in a preferred embodiment, includes forming an active layer having a given wavelength over a substrate. The method further includes forming an N-type doped layer over a portion of the active layer to form first and second active regions within the active layer, the first active region having the given wavelength and the second active region having an altered wavelength different from the given wavelength. In one exemplary embodiment, the conditions used to form the N-type doped layer, for example, dopant concentration, growth rate and temperature, cause the difference in wavelength between the given wavelength and the altered wavelength.

## Claims

### Claim 1

A method for monolithic integration of multiple devices on an optoelectronic substrate, comprising:
forming an active layer having a given wavelength over a substrate; and
forming an N-type doped layer over a portion of the active layer to form first and second active regions within the active layer, the first active region having the given wavelength and the second active region having an altered wavelength different from the given wavelength.

### Claim 2 (depends on 1)

The method as recited in claim 1 further including forming a indium phosphide layer between the active region and the N-type doped layer.

### Claim 3 (depends on 1)

The method as recited in claim 1 further including forming an etch stop layer over an unmasked active region prior to allowing the N-type doped layer to form over the unmasked active region.

### Claim 4 (depends on 3)

The method as recited in claim 3 wherein a masked active region and the unmasked active region have the given wavelength and the method further includes altering the given wavelength of the unmasked active region by the formation of the N-type doped layer to obtain the altered wavelength.

### Claim 5 (depends on 4)

The method as recited in claim 4 wherein altering the given wavelength by the formation of the N-type doped layer includes altering the given wavelength as a function of a growth rate, dopant concentration, temperature or mask geometry used to form the N-type doped layer.

### Claim 6 (depends on 5)

The method as recited in claim 5 wherein altering the given wavelength as a function of a dopant concentration includes altering the given wavelength as a function of a dopant concentration ranging from about 1E18/cm3 to about 4E18/cm3.

### Claim 7 (depends on 4)

The method as recited in claim 4 wherein altering the given wavelength as a function of a temperature includes altering the given wavelength as a function of a temperature ranging from about 600° C. to about 680° C.

### Claim 8 (depends on 4)

The method as recited in claim 4 wherein altering the given wavelength includes altering the given wavelength up to about 0.2 μm.

### Claim 9

A method of manufacturing an optical fiber communication system, comprising:
forming an optical fiber;
forming a transmitter and a receiver connected by the optical fiber; and
forming multiple devices on an optoelectronic substrate, including:
forming an active layer having a given wavelength over a substrate; and
forming an N-type doped layer over a portion of the active layer to form first and second active regions within the active layer, the first active region having the given wavelength and the second active region having an altered wavelength different from the given wavelength.

### Claim 10 (depends on 9)

The method as recited in claim 9 further including forming a indium phosphide layer between the active region and the N-type doped layer.

### Claim 11 (depends on 9)

The method as recited in claim 9 further including forming an etch stop layer over an unmasked active region prior to allowing the N-type doped layer to form over the unmasked active region.

### Claim 12 (depends on 11)

The method as recited in claim 11 wherein a masked active region and the unmasked active region have the given wavelength and the method further includes altering the given wavelength of the unmasked active region by the formation of the N-type doped layer to obtain the altered wavelength.

### Claim 13 (depends on 12)

The method as recited in claim 12 wherein altering the given wavelength by the formation of the N-type doped layer includes altering the given wavelength as a function of a growth rate, dopant concentration, temperature or mask geometry used to form the N-type doped layer.

### Claim 14 (depends on 13)

The method as recited in claim 13 wherein altering the given wavelength as a function of a dopant concentration includes altering the given wavelength as a function of a dopant concentration ranging from about 1E18/cm3 to about 4E18/cm3.

### Claim 15 (depends on 13)

The method as recited in claim 13 wherein altering the given wavelength as a function of a temperature includes altering the given wavelength as a function of a temperature ranging from about 600° C. to about 680° C.

### Claim 16 (depends on 13)

The method as recited in claim 13 wherein altering the given wavelength includes altering the given wavelength up to about 0.2 μm.

### Claim 17 (depends on 9)

The method recited in claim 9 wherein the transmitter includes the optoelectronic device.

### Claim 18 (depends on 9)

The method recited in claim 9 wherein the receiver includes the optoelectronic device.

### Claim 19 (depends on 9)

The method recited in claim 9 further including forming a repeater.

### Claim 20 (depends on 9)

The method recited in claim 9 wherein forming multiple devices on an optoelectronic substrate includes forming devices selected from the group consisting of:
lasers,
modulators;
optical amplifiers; and
optical waveguides.