# US 2002/0164842 A1 · Method for manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0164842 A1
- Document ID: US20020164842A1
- Status: Published application
- Kind: A1
- Application number: 10/131,503
- Filed: 2002-04-25
- Published: 2002-11-07
- Earliest claimed: 2001-04-27
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Setsuo Nakajima
- Web page: https://patentgrep.com/patent/US20020164842A1

## CPC

- H10P 14/3816: {Pulsed laser beam}
- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/673: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 86/00: Integrated devices formed in or on insulating or conducting substrates, e.g. formed in silicon-on-insulator [SOI] substrates or on stainless steel or glass substrates
- H10D 86/0225: {using crystallisation-promoting species, e.g. using a Ni catalyst}
- H10D 86/0227: {using structural arrangements to control crystal growth, e.g. placement of grain filters}
- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3806: {using crystallisation-enhancing elements}
- H10P 14/381: {Beam shaping, e.g. using a mask}
- H10P 14/3814: {Continuous wave laser beam}
- H10P 14/382: {Scanning of a beam}
- C03C 2218/32: After-treatment
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A purpose of the invention is to provide a method for leveling a semiconductor layer without increasing the number and the complication of manufacturing processes as well as without deteriorating a crystal characteristic, and a method for leveling a surface of a semiconductor layer to stabilize an interface between the surface of the semiconductor layer and a gate insulating film, in order to achieve a TFT having a good characteristic. In an atmosphere of one kind or a plural kinds of gas selected from hydrogen or inert gas (nitrogen, argon, helium, neon, krypton and xenon), radiation with a laser beam in the first, second and third conditions is carried out in order, wherein the first condition laser beam is radiated for crystallizing a semiconductor film or improving a crystal characteristic; the second condition laser beam is radiated for eliminating an oxide film; and the third condition laser beam is radiated for leveling a surface of the crystallized semiconductor film.

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising:
forming a semiconductor film over an insulating surface;
forming an oxide film on a surface of the semiconductor film; and
radiating the semiconductor film with a laser beam in a first condition, a second condition and a third condition in order under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas,
wherein the laser beam in the first condition has a first energy density, a first wavelength and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 2 (depends on 1)

A method for manufacturing a semiconductor device according to claim 1. the oxide film is formed by contacting the surface of the semiconductor film with a solution or gas containing ozone.

### Claim 3 (depends on 1)

A method for manufacturing a semiconductor device according to claim 1, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 4 (depends on 1)

A method for manufacturing a semiconductor device according to claim 1, the first energy density is 300 to 500 mJ/cm2.

### Claim 5

A method for manufacturing a semiconductor device comprising:
forming a semiconductor film on an insulating surface;
radiating the semiconductor film with a laser beam in a first condition to crystallize the semiconductor film;
forming an oxide film on a surface of the semiconductor film;
radiating the crystallized semiconductor film with a laser beam in a second condition to eliminate the oxide film; and
after radiating with the laser beam in the second condition, radiating the crystallized semiconductor film with a laser beam in a third condition to level a surface of the crystallized semiconductor film,
wherein radiating with the laser beams in the first to third conditions is performed successively under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas;
wherein the laser beam in the first condition has a first energy density, a first wavelength, and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 6 (depends on 5)

A method for manufacturing a semiconductor device according to claim 5, the oxide film is formed by contacting the surface of the semiconductor film with a solution or gas containing ozone.

### Claim 7 (depends on 5)

A method for manufacturing a semiconductor device according to claim 5, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 8 (depends on 5)

A method for manufacturing a semiconductor device according to claim 5, the first energy density is 300 to 500 mJ/cm2.

### Claim 9

A method for manufacturing a semiconductor device comprising:
forming a semiconductor film on an insulating surface;
radiating the semiconductor film with a laser beam in a first condition to crystallize the semiconductor film;
forming an oxide film on a surface of the semiconductor film;
radiating the crystallized semiconductor film with a laser beam in a second condition to eliminate the oxide film; and
after radiating with the laser beam in the second condition, radiating the crystallized semiconductor film with a laser beam in a third condition to make a difference between top and bottom points of a surface of the crystallized semiconductor film 6 nm or less,
wherein radiating with the laser beams in the first to third conditions is performed successively under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas;
wherein the laser beam in the first condition has a first energy density, a first wavelength, and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 10 (depends on 9)

A method for manufacturing a semiconductor device according to claim 9, the oxide film is formed by contacting the surface of the semiconductor film with a solution or gas containing ozone.

### Claim 11 (depends on 9)

A method for manufacturing a semiconductor device according to claim 9, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 12 (depends on 9)

A method for manufacturing a semiconductor device according to claim 9 the first energy density is 300 to 500 mJ/cm2.

### Claim 13

A method for manufacturing a semiconductor device comprising:
forming a semiconductor film on an insulating surface;
radiating the semiconductor film with a laser beam in a first condition;
forming an oxide film on a surface of the crystallized semiconductor film; and
radiating the crystallized semiconductor film with a laser beam in a second condition to eliminate the oxide film;
radiating the crystallized semiconductor film with a laser beam to level a surface of the crystallized semiconductor; a third condition in order in an atmosphere of one kind of gas or a mixed atmosphere of plural kinds of gas, the gas being selected from hydrogen and inert gas,
wherein radiating with the laser beams in the first to third conditions is performed successively under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas;
wherein the laser beam in the first condition has a first energy density, a first wavelength, and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 14 (depends on 13)

A method for manufacturing a semiconductor device according to claim 13, the oxide film is formed by contacting the surface of the semiconductor film with a solution or gas containing ozone.

### Claim 15 (depends on 13)

A method for manufacturing a semiconductor device according to claim 13, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 16 (depends on 13)

A method for manufacturing a semiconductor device according to claim 13, the first energy density is 300 to 500 mJ/cm2.

### Claim 17

A method for manufacturing a semiconductor device comprising:
forming a semiconductor film on an insulating surface;
adding a catalyst element to the semiconductor film;
crystallizing the semiconductor film by a first heating treatment to the semiconductor film added with the catalyst element;
forming an oxide film on a surface of the crystallized semiconductor film;
radiating the semiconductor film with a laser beam in a first condition to improve a crystal characteristic of the crystallized semiconductor film;
radiating the crystallized semiconductor film with a laser beam in a second condition to eliminate the oxide film;
after radiating with the laser beam in the second condition, radiating the crystallized semiconductor film with a laser beam in a third condition to level a surface of the crystallized semiconductor film;
providing a second heat treatment to the crystallized semiconductor film to transport the catalyst element in the crystallized semiconductor film to a gettering site,
wherein radiating with the laser beams in the first to third conditions is performed successively under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas;
wherein the laser beam in the first condition has a first energy density, a first wavelength, and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 18 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 19 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the catalyst element is selected from the group consisting of Fe, Ni, Co, Ru, Rh, Pd, Os, Ir, Pt, Cu and Au.

### Claim 20 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the first heating treatment is a heating treatment in which heating wire, lamp light source or heated gas is used as a heat source.

### Claim 21 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the gettering site contains one or plural kinds of element selected from the group consisting of He, Ne, Ar, Kr and Xe.

### Claim 22 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the gettering site contains one or plural kinds of element selected from elements belonging to the 15th group in a periodic table.

### Claim 23 (depends on 17)

A method for manufacturing a semiconductor device according to claim 17, the first energy density is 300 to 500 mJ/cm2.

### Claim 24

A method for manufacturing a semiconductor device comprising:
forming a semiconductor film on an insulating surface;
crystallizing the semiconductor film;
forming an oxide film on the semiconductor film;
radiating the crystallized semiconductor film with a laser beam in a first condition to improve a crystal characteristic of the crystallized semiconductor film;
radiating the crystallized semiconductor film with a laser beam in a second condition to eliminate the oxide film; and
after radiating with the laser beam in the second condition, radiating the crystallized semiconductor film with a laser beam in a third condition to level a surface of the crystallized semiconductor film,
wherein radiating with the laser beams in the first to third conditions is performed successively under an atmosphere comprising gas selected from the group consisting of hydrogen and inert gas;
wherein the laser beam in the first condition has a first energy density, a first wavelength, and a first pulse width;
wherein the laser beam in the second condition has a second energy density lower than the first energy density, a second wavelength and a second pulse width shorter than the first wavelength and the first pulse width, respectively; and
wherein the laser beam in the third condition has a third energy density which is higher than the first energy density by 30 to 60 mJ/cm2.

### Claim 25 (depends on 24)

A method for manufacturing a semiconductor device according to claim 24, the oxide film is formed by contacting the surface of the semiconductor film with a solution or gas containing ozone.

### Claim 26 (depends on 24)

A method for manufacturing a semiconductor device according to claim 24, the inert gas is one of nitrogen, argon, helium, neon, krypton and xenon.

### Claim 27 (depends on 24)

A method for manufacturing a semiconductor device according to claim 24, the first energy density is 300 to 500 mJ/cm2.