# US 2002/0164417 A1 · Method of repairing a ceramic coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0164417 A1
- Document ID: US20020164417A1
- Status: Published application
- Kind: A1
- Application number: 10/120,417
- Filed: 2002-04-12
- Published: 2002-11-07
- Earliest claimed: 2001-04-21
- Assignees: ALSTOM Technology Ltd
- Inventors: Abdus S. Khan; John Fernihough; Maxim Konter
- Web page: https://patentgrep.com/patent/US20020164417A1

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 41/5042: {Zirconium oxides or zirconates; Hafnium oxides or hafnates}
- C04B 41/87: Ceramics
- C23C 24/08: by application of heat or pressure and heat (C23C24/04 takes precedence)
- F01D 5/288: {Protective coatings for blades}
- F05D 2230/80: Repairing, retrofitting or upgrading methods
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

It is a method of repairing a ceramic coating of an article after use of this article in a high temperature environment disclosed. The ceramic coating is removed locally at spalled areas, at the areas where the ceramic coating is removed locally a mixture including a powder of zirconia stabilized with one or a combination of yttria, calcia, scandia, magnesia, ceria and oxides of the rare earth group, and hydrated metallic halides as a binder is applied and the applied ceramic powder is dried.

## Claims

### Claim 1

A method of repairing a ceramic coating of an article after damage due to the transport after manufacture or use of this article in a high temperature environment, wherein
a. remnants of the ceramic coating adjacent to and inside of the areas of spallation are removed,
b. the areas of spallation are prepared for local coating application by conventional means such as chemical treatment, grit blasting or abrasive cleaning,
c. on the areas of spallation is applied a mixture including a powder of zirconia stabilized with one or a combination of yttria, calcia, scandia, magnesia, ceria and oxides of the rare earth group, and hydrated metallic halides as a binder, after which
d. the applied mixture of ceramic powder and binder is dried.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the mixture of stabilized zirconia powder and hydrated metallic halides as a binder is prepared as a slurry with water alone or with water in combination with alcohol using hydrated aluminum chlorides before applying to the mentioned areas.

### Claim 3 (depends on 2)

The method of claim 2, wherein
the slurry is dried at a temperature between 20° C. and 100° C. and finally heat-treated at 55° to 750° C.

### Claim 4 (depends on 2)

The method of claim 2, wherein
hollow zirconia spheres are included in the mixture of stabilized zirconia powder and hydrated metallic hydrides.

### Claim 5 (depends on 1)

The method of claim 1, wherein
the hydrated metallic halide binder consists of one or a combination of hydrated metallic halide components such as hydrated aluminum chloride and/or hydrated halides of magnesium, calcium, yttrium, zirconium, strontium, barium, including other hydrated halides of the rare earth group or group 11 alkaline halides.

### Claim 6 (depends on 1)

The method of claim 1, wherein
the sizes of individual powder particles of the stabilized zirconia powder ranges from 5 to 150 μm.

### Claim 7 (depends on 1)

The method of claim 1, wherein
the mixture of stabilized zirconia powder and hydrated metallic hydrides is applied by painting, slurry spraying, or as a paste.

### Claim 8 (depends on 1)

The method of claim 1, wherein
the article is a blade or a vane or any other part of a gas turbine engine consisting of a nickel or cobalt base alloy exposed to a high temperature environment coated with TBC.