# US 2002/0160614 A1 · Method of forming an interlayer dielectric film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160614 A1
- Document ID: US20020160614A1
- Status: Published application
- Kind: A1
- Application number: 10/082,019
- Filed: 2002-02-20
- Published: 2002-10-31
- Earliest claimed: 2001-02-22
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Young-Joo Cho; Eun-Kee Hong; Ju-Bum Lee
- Web page: https://patentgrep.com/patent/US20020160614A1

## CPC

- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6516: {of treatments performed after formation of the materials}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6689: {the compound being a silazane}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In a method for forming an interlayer dielectric film, an insulating film is deposited on a semiconductor substrate that has a metal wiring pattern. The insulating film is polished by CMP until exposing an upper portion of the wiring pattern. A spin on glass composition, which includes polysilazane, is coated over the polished insulating material and exposed portions of the wiring pattern to form a film. The film is then pre-baked in a temperature range of 50 to 350° C., and then hard-baked in a temperature range of 300 to 500° C. After the hard-baking, the film is then heat-treated in an oxidation atmosphere. With the hard-baking, gasses of the coating of film may be removed so that the amount of gas generated during a subsequent anneal or heat-treating process may be reduced. Accordingly, particle contaminants may be reduced by such process in addition to providing a means for reduced risk of crack formation.

## Claims

### Claim 1

A method of forming an interlayer, the method comprising:
preparing a substrate with a wiring pattern;
forming an insulating film on the substrate;
chemical mechanical polishing the insulating film and exposing an upper portion of the wiring pattern;
coating the polished insulation and exposed portion of the wiring pattern with spin on glass composition to form a film;
the coating using polysilazane in the spin on glass composition;
pre-baking the film in a temperature range of 50 to 350° C.;
after the pre-baking, hard-baking the film in a temperature range of 300 to 500° C.; and
heat-treating the film in an oxidation atmosphere.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the forming the insulating film comprises forming at least one of a BPSG film, a HDP oxide film and an SOG oxide layer from a spin on glass composition having polysilazane.

### Claim 3 (depends on 2)

The method as claimed in claim 2, further comprising using at least one of a SiO2, CeO2, Al2O3 or Mn2O3 based slurry in the chemical mechanical polishing.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the coating uses a spin on glass composition comprising about 3 to 15 weight percent of perhydropolysilazane having a structure of —(SiH2NH)n (n being a positive number), an average molecular weight of about 4000 to 8000 and a molecular weight dispersion degree of about 3.0 to 4.0.

### Claim 5 (depends on 4)

The method of claim 4, in which the coating further comprises using about 97 to 85 weight percent solvent in the spin on glass composition.

### Claim 6 (depends on 4)

The method as claimed in claim 4, wherein the coating uses a spin on glass composition that comprises a viscosity of about 1 to 10 mPa s and shear rate of 54 to 420 (1/s).

### Claim 7 (depends on 4)

The method as claimed in claim 4, in which the coating establishes the spin on glass composition with a contact angle less than 4 degrees with respect to an underlayer.

### Claim 8 (depends on 4)

The method as claimed in claim 4, wherein the coating further comprises using a spin-on-glass composition that comprises at least one of the impurities from the group consisting of B, F, P, B and C.

### Claim 9 (depends on 4)

The method as claimed in claim 4, wherein the coating further comprises using a spin-on-glass composition that comprises a compound having at least one of the elements from the group consisting of B, F, P, B, C and O.

### Claim 10 (depends on 4)

The method as claimed in claim 4, wherein the solvent of the spin-on-glass composition comprises at least one of xylene or dibutylether.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein the heat-treating comprises establishing a temperature in a range of about 600 to 1200° C.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein the heat-treating lasts for a duration of about 10 to 120 minutes and uses an oxidation atmosphere selected from the group consisting of an oxygen atmosphere, a vapor atmosphere and a mixed atmosphere of vapor and oxygen.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the film is formed with a thickness of about 500 to 10000 Å.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the hard-baking exposes the film to an oxidation atmosphere selected from the group consisting of an oxygen atmosphere, a vapor atmosphere and a mixed atmosphere of vapor and oxygen for a duration of about 10 to 120 minutes.

### Claim 15 (depends on 1)

The method as claimed in claim 1, wherein the hard-baking exposes the film to an inert atmosphere for a duration of about 10 to 120 minutes.

### Claim 16 (depends on 15)

The method as claimed in claim 15, in which the hard-baking comprises baking the substrate in a vacuum for a duration of about 10 to 120 minutes.

### Claim 17 (depends on 15)

The method as claimed in claim 15, in which the hard-baking further comprises establishing a vacuum for the inert atmosphere.

### Claim 18 (depends on 1)

The method as claimed in claim 1, further comprising:
determining an upper limit for the thickness of the film of spin on glass by which it may be hard-backed without crack formation;
determining if a thickness of the film exceeds the upper limit; and
decreasing a thickness of the film to below the upper limit dependent upon the thickness determination.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the decreasing the thickness of the film uses at least one of a chemical mechanical polishing or an etch back process.

### Claim 20

A method of forming an interlayer dielectric, comprising:
forming insulating material on a semiconductor substrate;
polishing the insulating material using a chemical mechanical polishing process and exposing an upper portion of a conductive pattern of the semiconductor substrate;
coating the polished insulating material and the upper portion of the conductive pattern with a spin on glass composition and forming a film, the coating using polysilazane in the spin on glass composition;
pre-baking the film at a temperature below 500° C.;
determining if a thickness of the film exceeds a crack free thickness limit;
decreasing a thickness of the film dependant on the determining; and
heat-treating the film in an oxidation atmosphere.

### Claim 21

A method of processing a semiconductor substrate, comprising:
forming insulating material on a semiconductor substrate having a conductive pattern and step;
chemical mechanical polishing the insulating material and exposing an upper portion of the conductive pattern;
coating the insulating material and the exposed upper portion of the conductive pattern with spin on glass composition to form a film;
using polysilazane in the spin on glass composition;
pre-baking the film in a predetermined first temperature range for a first duration;
hard-baking the film in a predetermined second temperature range for a second duration, the predetermined second temperature range higher than the first; and
heat-treating the film for a third duration in an oxidation atmosphere of a predetermined third temperature range, the predetermined third temperature range higher than the second.

### Claim 22

A method of forming an interlayer dielectric film, the method comprising:
coating a spin on glass composition on a semiconductor substrate that has been formed with a conductive pattern step, the coating using polysilazane in the spin on glass composition;
curing the spin on glass composition to form a film;
outgassing the film, the outgassing comprises releasing silane gas; and
annealing and oxidizing the film.

### Claim 23 (depends on 22)

The method as claimed in claim 22, in which the coating uses a spin on glass composition comprising about 20 to 30 weight percent of perhydropolysilazane and about 80 to 70 weight percent of a solvent, the perhydropolysilazane having a structure of —(SiH2NH)n (n being a positive number), an average molecular weight of about 4000 to 8000 and a molecular weight dispersion degree of about 3.0 to 4.0.

### Claim 24 (depends on 23)

The method as claimed in claim 23, in which the spin on glass composition further comprises a constant viscosity of about 1 to 10 (mPa s) at a shear rate of about 54 to 420 (1/s).

### Claim 25 (depends on 23)

The method as claimed in claim 23, in which the coating establishes the spin on glass composition with a contact angle less than about 4 degrees with respect to an underlayer.

### Claim 26 (depends on 23)

The method as claimed in claim 23, wherein the spin on glass composition comprises at least one impurity compound comprising at least one element of the group consisting of B, F, P, B, C and O.

### Claim 27 (depends on 23)

The method as claimed in claim 23, wherein the solvent comprises at least one of xylene or dibutylether.

### Claim 28 (depends on 22)

The method as claimed in claim 22, wherein the annealing uses temperatures in a range of about 600 to 1200° C.

### Claim 29 (depends on 28)

The method as claimed in claim 28, in which the annealing comprises exposing the film to an oxidation atmosphere comprising at least one of oxygen and vapor for a duration of 10 to 120 minutes.

### Claim 30 (depends on 22)

The method as claimed in claim 22, in which the curing comprises pre-baking the semiconductor substrate through multiple stages of different temperatures.

### Claim 31 (depends on 30)

A method according to claim 30, in which the pre-baking uses a temperature range of S0 to 350° C. for the multiple stages.

### Claim 32 (depends on 30)

The method as claimed in claim 30, wherein the outgassing comprises hard-baking the film in a temperature range of about 300 to 500° C.

### Claim 33 (depends on 32)

The method as claimed in claim 32, wherein the hard-baking comprises exposing the film to an atmosphere that comprises at least one of vapor and oxygen for a duration of about 10 to 120 minutes.

### Claim 34 (depends on 32)

The method as claimed in claim 32, wherein the hard-baking is carried out for a duration of about 10 to 120 minutes in an inert atmosphere.

### Claim 35 (depends on 34)

A method according to claim 34, in which the hard-baking uses nitrogen in the inert atmosphere.

### Claim 36 (depends on 35)

A method according to claim 35, in which the hard-baking further comprises removing gases from a chamber to establish a vacuum for the inert atmosphere.