# US 2002/0160592 A1 · Method for forming ultra-shallow junctions using laser annealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160592 A1
- Document ID: US20020160592A1
- Status: Published application
- Kind: A1
- Application number: 10/016,534
- Filed: 2001-12-10
- Published: 2002-10-31
- Earliest claimed: 2001-04-30
- Assignees: Hynix Semiconductor Inc.
- Inventors: Yong Sun Sohn
- Web page: https://patentgrep.com/patent/US20020160592A1

## CPC

- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10D 64/662: {the conductor further comprising additional layers, e.g. multiple silicon layers having different crystal structures}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming an ultra-shallow junction using laser annealing wherein an amorphous carbon layer is used as an energy absorber layer comprises the steps of preparing a silicon substrate having isolation layers; forming a gate having a stacked structure of a gate insulating layer, a polysilicon layer and a metal layer on the silicon substrate; forming a sacrificial spacer on the sidewalls of the gate; forming source and drain regions on the silicon substrate regions at both sides of the gate including on the sacrificial spacer; removing the sacrificial spacer; doping impurities to form source/drain extension doping layers on the silicon substrate regions at both sides of the gate; depositing sequentially a reaction preventing layer and an amorphous carbon layer as a laser absorber layer on the resulting structure; forming source/drain extension doping layers on inner sides of the source and drain regions by performing laser annealing in an atmosphere of inert gas or under vacuum; and removing the amorphous carbon layer.

## Claims

### Claim 1

A method for forming an ultra-shallow junction using laser annealing comprising the steps of:
preparing a silicon substrate having isolation layers;
forming a gate having a stacked structure of a gate insulating layer, a polysilicon layer and a metal layer on the silicon substrate;
forming a sacrificial spacer on the sidewalls of the gate;
forming source and drain regions on the silicon substrate regions at both sides of the gate, including on the sacrificial spacer;
removing the sacrificial spacer;
doping impurities to form a source/drain extension doping layer on the silicon substrate regions at both sides of the gate;
depositing sequentially a reaction preventing layer and an amorphous carbon layer as a laser absorber layer on the resulting structure;
forming source/drain extension doping layers on inner sides of the source and drain regions by performing laser annealing in an atmosphere of essentially inert gas or under vacuum; and
removing the amorphous carbon layer.

### Claim 2 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein after the formation of the gate and before the formation of the sacrificial spacer, a thin oxide film is formed on the side of the polysilicon layer by performing selective oxidation processes and a silicon nitride layer is deposited as an etching preventing layer on the resulting structure.

### Claim 3 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the step for formation of the source and drain regions comprises doping of N type or P type dopants on the silicon substrate at both sides of the gate and performing a rapid thermal treatment.

### Claim 4 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the sacrificial spacer is removed by performing an etching process using HF solution.

### Claim 5 (depends on 2)

The method for forming an ultra-shallow junction using laser annealing according to claim 2, wherein after the sacrificial spacer is removed and before impurities are doped to form the source/drain extension doping layers, the silicon nitride layer formed on the silicon substrate is removed.

### Claim 6 (depends on 5)

The method for forming an ultra-shallow junction using laser annealing according to claim 5, wherein the silicon nitride layer is removed using an anisotropy etching process.

### Claim 7 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the step for doping impurities to form the source/drain extension doping layers comprises ion-implantation of N type or P type dopants in low energy or plasma doping.

### Claim 8 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the reaction preventing layer is a silicon oxide layer.

### Claim 9 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the amorphous carbon layer is deposited to a thickness of 200 to 400 Å.

### Claim 10 (depends on 1)

The method for forming an ultra-shallow junction using laser annealing according to claim 1, wherein the amorphous carbon layer is removed by etching process using O2 plasma.

### Claim 11

The method for forming an ultra-shallow junction using laser annealing comprising the steps of:
preparing a silicon substrate having trench type isolation layers to define an active region;
forming a gate having a stacked structure of a gate insulating layer, a polysilicon layer, a diffusion preventing layer, a metal layer and a hard mask layer on the active region of silicon substrate;
forming a thin oxide layer on the surface of the silicon substrate and on side of polysilicon layer by performing selective oxidation processes; depositing a thin silicon nitride layer as an etching preventing layer on the resulting structure;
forming a sacrificial spacer on sidewall of gate having the silicon nitride layer thereon;
forming source/drain regions on the silicon substrate at both sides of gate including the sacrificial spacer;
removing the sacrificial spacer, the silicon nitride layer and the oxide layer formed on the surface of the silicon substrate;
doping impurities in low energy to form source/drain extension doping layers on the silicon substrate at both sides of the gate;
depositing a silicon oxide layer as a reaction preventing layer and an amorphous carbon layer as a laser absorber layer on the resulting structure;
forming source/drain extension doping layers on inner sides of the source and drain regions by performing laser annealing in an atmosphere of inert gas or under vacuum; and
removing the amorphous carbon layer using an O2 plasma etching process.

### Claim 12 (depends on 11)

The method for forming an ultra-shallow junction using laser annealing according to claim 11, wherein the sacrificial spacer is removed by an etching process using HF solution and the silicon nitride layer is removed by an anisotropy etching process.

### Claim 13 (depends on 11)

The method for forming an ultra-shallow junction using laser annealing according to claim 11, wherein the step for doping impurities to form the source/drain extension doping layers comprises ion implantation of N type or P type dopants in low energy or plasma doping.

### Claim 14 (depends on 11)

The method for forming an ultra-shallow junction using laser annealing according to claim 11, wherein the amorphous carbon layer is deposited to a thickness of 200 to 400 Å.

### Claim 15

A method for forming an ultra-shallow junction using laser annealing comprising the steps of:
preparing a silicon substrate having isolation layers thereon;
forming a gate having a stacked structure of a gate insulating layer, a polysilicon layer and a metal layer on the silicon substrate;
forming source/drain extension doping layers on the silicon substrate regions at both sides of the gate;
forming a spacer on sidewalls of the gate;
doping impurities on the silicon substrate at both sides of the gate including the spacer to form source and drain regions;
depositing a reaction preventing layer and an amorphous carbon layer as an energy absorber layer on the resulting structure;
forming source and drain regions on the silicon substrate at both sides of gate including the spacer by performing a laser annealing in an atmosphere of inert gas or under vacuum; and
removing the amorphous carbon layer.

### Claim 16 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein after the formation of the gate and before the formation of the source/drain extension doping layers, thin oxide layers are formed on the surface of the silicon substrate and on sidewall of the polysilicon layer by performing selective oxidation processes.

### Claim 17 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein after formation of the source/drain extension doping layers and before formation of the spacer, a silicon nitride layer is deposited as an etching preventing layer on the resulting structure.

### Claim 18 (depends on 17)

The method for forming an ultra-shallow junction using laser annealing according to claim 17, wherein in the formation of the spacer, the silicon nitride layer formed on the surface of the silicon substrate is removed.

### Claim 19 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein the formation of the source/drain extension doping layers comprises ion implantation of N type or P type dopants in low energy or plasma doping on the silicon substrate at both sides of the gate and performing a rapid thermal treatment.

### Claim 20 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein the reaction preventing layer is a silicon oxide layer.

### Claim 21 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein the amorphous carbon layer is deposited to a thickness of 200 to 400 Å.

### Claim 22 (depends on 15)

The method for forming an ultra-shallow junction using laser annealing according to claim 15, wherein the amorphous carbon layer is removed by an etching process using O2 plasma.

### Claim 23

A method for forming an ultra-shallow junction using laser annealing comprising the steps of:
preparing a silicon substrate having trench type isolation layers to define an active region;
forming a gate having a stacked structure of a gate insulating layer, a polysilicon layer, a diffusion preventing layer, a metal layer and a hard mask layer on the active region of the silicon substrate;
forming source/drain extension doping layer by doping impurities on silicon substrate at both sides of the gate and by performing a rapid thermal treatment;
depositing a thin silicon nitride layer as an etching preventing layer on the resulting structure;
forming a spacer on sidewall of the gate and on the silicon nitride layer deposited thereon;
doping impurities to form source and drain regions on the silicon substrate at both sides of the gate including the spacer;
depositing a silicon oxide layer as a reaction preventing layer and an amorphous carbon layer as an energy absorber layer on the resulting structure;
forming source and drain regions on the silicon substrate at both sides of the gate including the spacer by performing laser annealing in an atmosphere of inert gas or under vacuum; and
removing the amorphous carbon layer using O2 plasma etching.

### Claim 24 (depends on 23)

The method for forming an ultra-shallow junction using laser annealing according to claim 23, wherein after the formation of the gate and before the formation of the source/drain extension doping layers, thin oxide layers are formed on the surface of the silicon substrate and on the sidewalls of the polysilicon layer by selective oxidation processes.

### Claim 25 (depends on 24)

The method for forming an ultra-shallow junction using laser annealing according to claim 24, wherein in the formation of the spacer, the silicon nitride formed on the surface of the silicon substrate is removed.

### Claim 26 (depends on 24)

The method for forming an ultra-shallow junction using laser annealing according to claim 24, wherein the amorphous carbon layer is deposited to a thickness of 200 to 400 Å.