# US 2002/0160542 A1 · FeRAM having BLT ferroelectric layer and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160542 A1
- Document ID: US20020160542A1
- Status: Published application
- Kind: A1
- Application number: 10/133,505
- Filed: 2002-04-26
- Published: 2002-10-31
- Earliest claimed: 2001-04-27
- Assignees: Hynix Semiconductor Inc.
- Inventors: Nam-Kyeong Kim; Seung-Jin Yeom; Woo-Seok Yang; Soon-Young Kweon
- Web page: https://patentgrep.com/patent/US20020160542A1

## CPC

- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A ferroelectric memory device and a method for manufacturing the same is disclosed. Because a (BixLay)Ti3O12 (BLT) layer, which can be crystallized in relatively low temperature, is used in a capacitor, the electrical characteristics of the ferroelectric capacitor can be improved. The method for manufacturing ferroelectric memory device includes the steps of forming a first conductive layer for a bottom electrode on a semiconductor substrate, forming the (BixLay)Ti3O12 ferroelectric layer, wherein ‘x’ representing atomic concentration of Bi ranges from about 3.25 to about 3.35 and ‘y’ representing atomic concentration of La ranges from about 0.70 to about 0.90 and forming a second conductive layer for a top electrode on the (BixLay)Ti3O12 ferroelectric layer.

## Claims

### Claim 1

A method for manufacturing ferroelectric memory device, comprising:
a) forming a first conductive layer for a bottom electrode on a semiconductor substrate;
b) forming a (BixLay)Ti3O12 ferroelectric layer, wherein ‘x’ representing atomic concentration of Bi ranging from about 3.25 to about 3.35 and ‘y’ representing atomic concentration of La ranges from about 0.70 to about 0.90; and
c) forming a second conductive layer for a top electrode on the (BixLay)Ti3O12 ferroelectric layer.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the method further comprises:
d) performing a thermal treatment to align a crystal direction on the side of the (BixLay)Ti3O12 ferroelectric layer, wherein the angle between the crystal direction of the bottom and top electrodes ranges from 0° to 90° alter the thermal treatment.

### Claim 3 (depends on 2)

The method as recited in claim 2, wherein the step a) comprises:
a1) further forming a conductive oxide layer with Irx or RuOx; and
a2) forming a metal layer selected form the group consisting of Pt, Ru, Ir, W and WN on the conductive oxide layer.

### Claim 4 (depends on 3)

The method recited in claim 3, wherein the step b) comprises:
b1) forming the (BixLay)Ti3O12 ferroelectric layer on the first conductive layer;
b2) performing a thermal treatment for nucleation at temperature ranging from about 400° C. to about 800° C.; and
b3) performing a thermal treatment for crystallization of the (BixLay)Ti3O12 ferroelectric layer at temperature ranging from about 500° C. to about 675° C.

### Claim 5 (depends on 4)

The method as recited in claim 4, wherein the (BixLay)Ti3O12 ferroelectric layer is formed by a technique selected from the group consisting of spin-on, PVD (Physical Vapor Deposition), CVD (Chemical Vapor Deposition), ALD (Atomic Layer Deposition), MOD (Metal Organic Deposition) or PECVD (Plasma Enhanced Chemical Vapor Deposition).

### Claim 6 (depends on 4)

The method as recited in claim 4, wherein the (BixLay)Ti3O12 ferroelectric layer is formed by the PECVD technique at a temperature ranging from about 400° C. to about 700° C.

### Claim 7 (depends on 4)

The method as recited in claim 4, wherein the step b1) comprises:
b4) forming a (BixLay)Ti3O12 material of liquid state on the substrate using the spin-on technique;
b5) removing solvent contained in the (BixLay)Ti3O12 material by a thermal treatment at temperature ranging from about 100° C. to 200° C.; and
b6) removing organic matter contained in the (BixLay)Ti3O12 material by a thermal treatment at temperature ranging from about 200° C. to about 350° C.

### Claim 8 (depends on 4)

The method as recited in claim 4, wherein the thermal treatment for nucleation is performed by increasing temperature at speed ranging from about 50° C./sec to about 300° C./sec in an ambient atmosphere selected from the group consisting of N2, NH3, O2, N2O and mixed O2 and N2.

### Claim 9 (depends on 4)

The method as recited in claim 4, wherein the thermal treatment for crystallization of the (BixLay)Ti3O12 ferroelectric layer is performed at an atmospheric pressure condition in an ambient atmosphere selected from the group consisting of O2, N2O and mixed O2 and N2.

### Claim 10

A ferroelectric memory device, comprising:
a semiconductor substrate;
a transistor comprising a gate insulating layer, a gate electrode formed on the semiconductor substrate and a doped region formed in the semiconductor substrate at an end of the gate electrode;
a plug engaging to the doped region of the transistor; and
a capacitor including a bottom electrode formed on the plug, a (BixLay)Ti3O12 ferroelectric layer formed on the bottom electrode and a top electrode formed on the ferroelectric layer.

### Claim 11 (depends on 10)

The ferroelectric memory device as recited in claim 10, wherein ‘x’ representing atomic concentration of Bi ranges from about 3.25 to about 3.35 and ‘y’ representing atomic concentration of La ranges from about 0.70 to about 0.90.

### Claim 12 (depends on 11)

The ferro electric memory device as recited in claim 11, an angle between a crystal direction on a side of the (BixLay)Ti3O12 ferroelectric layer and the bottom and top electrodes ranges from 0° to 90°.

### Claim 13 (depends on 12)

The ferroelectric memory device as recited in claim 12, wherein the bottom electrode comprises:
a first bottom electrode formed with a conductive oxide layer on the plug; and
a second bottom electrode formed with a metal layer on the first bottom electrode.

### Claim 14 (depends on 12)

The ferroelectric memory device as recited in claim 12, wherein the first bottom electrode is formed with IrOx or RuOx.

### Claim 15 (depends on 12)

The ferroelectric memory device as recited in claim 12, wherein the second bottom electrode is formed with a material selected from the group consisting of Pt, Ru, Ir, W and WN.

### Claim 16 (depends on 10)

The ferroelectric memory device as recited in claim 10, wherein the device further comprises an Ohmic contact layer and a barrier metal layer between the plug and the bottom electrode.

### Claim 17

A method for manufacturing ferroelectric memory device, comprising:
a) forming a first conductive layer for a bottom electrode on a semiconductor substrate;
b) forming a (BixLay)Ti3O12 ferroelectric layer, wherein ‘x’ representing atomic concentration of Bi ranges from about 3.25 to about 3.35 and ‘y’ representing atomic concentration of La ranges from about 0.70 to about 0.90;
c) forming a second conductive layer for a top electrode on the (BixLay)Ti3O12 ferroelectric layer;
d) patterning the second conductive layer, the (BixLay)Ti3O12 ferroelectric layer and the first conductive layer, wherein the edge of the (BixLay)Ti3O12 ferroelectric layer is exposed;
e) performing a thermal treatment to align a crystal direction on the side of the (BixLay)Ti3O12 ferroelectric layer, wherein the angle between the crystal direction of the bottom and top electrodes ranges from 0° to 90° alter the thermal treatment.

### Claim 18 (depends on 17)

The method recited in claim 17, wherein the step comprises:
b1) forming the (BixLay)Ti3O12 ferroelectric layer on the first conductive layer;
b2) performing a thermal treatment for nucleation at temperature ranging from about 400° C. to about 800° C.; and
b3) performing a thermal treatment for crystallization of the (BixLay)Ti3O12 ferroelectric layer at temperature ranging from about 500° C. to about 675° C.

### Claim 19 (depends on 4)

The method as recited in claim 4, wherein the (BixLay)Ti3O12 ferroelectric layer is formed by the PECVD technique at a temperature ranging from about 400° C. to about 700° C.

### Claim 20 (depends on 18)

The method as recited in claim 18, wherein the step b1) comprises:
b4) forming a (BixLay)Ti3O12 material of liquid state on the substrate using the spin-on technique;
b5) removing solvent contained in the (BixLay)Ti3O12 material by a thermal treatment at temperature ranging from about 100° C. to about 200° C.; and
b6) removing organic matter contained in the (BixLay)Ti3O12 material by a thermal treatment at temperature ranging from about 200° C. to about 350° C.