# US 2002/0160307 A1 · Optical disk and method of fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160307 A1
- Document ID: US20020160307A1
- Status: Published application
- Kind: A1
- Application number: 10/133,959
- Filed: 2002-04-26
- Published: 2002-10-31
- Earliest claimed: 2001-04-30
- Assignees: LG Electronics Inc.
- Inventors: Tae Hee Jeong; Hun Seo
- Web page: https://patentgrep.com/patent/US20020160307A1

## CPC

- G11B 7/266: {Sputtering or spin-coating layers (sputtering in general C23C14/24; spin-coating in general B05D1/005)}
- G11B 7/24: Record carriers characterised by shape, structure or physical properties, or by the selection of the material (characterised by the arrangement of information on the carrier G11B7/007)
- G11B 7/243: comprising inorganic materials only, e.g. ablative layers
- G11B 7/252: of layers other than recording layers
- G11B 7/2542: consisting essentially of organic resins
- G11B 7/258: of reflective layers
- G11B 7/2534: polycarbonates [PC]
- G11B 7/257: of layers having properties involved in recording or reproduction, e.g. optical interference layers or sensitising layers or dielectric layers, which are protecting the recording layers
- G11B 7/2585: based on aluminium
- G11B 7/259: based on silver
- G11B 2007/24306: {transition metal elements of groups 3-10}
- G11B 2007/2431: {group 13 elements (B, Al, Ga, In)}
- G11B 2007/24312: {group 14 elements (e.g. Si, Ge, Sn)}
- G11B 2007/24314: {group 15 elements (e.g. Sb, Bi)}
- G11B 2007/24316: {group 16 elements (i.e. chalcogenides, Se, Te)}
- G11B 2007/2432: {Oxygen}
- Y10T 428/21: Circular sheet or circular blank
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An optical disk and a method of fabricating the optical disk capable of improving the signal quality and the productivity are disclosed. The optical disk includes a plurality of reflective layers stacked on a substrate, amorphous layers formed among the reflective layers which include a small amount of oxide therein, a recording layer, formed on the reflective layer, for recording information, and a cover layer formed on the recording layer.

## Claims

### Claim 1

An optical disk comprising:
a substrate;
a plurality of reflective layers stacked on the substrate;
amorphous layers formed among the reflective layers;
a recording layer, formed on the reflective layer, for recording information; and
a cover layer formed on the recording layer.

### Claim 2 (depends on 1)

The optical disk as claimed in claim 1, wherein the reflective layer is made of a mixture obtained by adding an oxide to any one selected from the group consisting of Al, Al alloy, Ag, and Ag alloy.

### Claim 3 (depends on 2)

The optical disk as claimed in claim 2, wherein the oxide is SiO2.

### Claim 4 (depends on 2)

The optical disk as claimed in claim 2, wherein the adding ratio of the oxide is in the range of 0.1˜10 mol %.

### Claim 5 (depends on 1)

The optical disk as claimed in claim 1, wherein the thickness of the reflective layer is in the range of 100˜1000 Å.

### Claim 6 (depends on 1)

The optical disk as claimed in claim 1, wherein the amorphous layer is made of a material selected from the group consisting of Si-oxide, Al-oxide, Ti-oxide, Cr-oxide, and ZnS—siO2.

### Claim 7 (depends on 1)

The optical disk as claimed in claim 1, wherein the amorphous layer is made of either of a Ge—Sb—Te type alloy thin film and an Ag—In—Sb—Te type alloy thin film.

### Claim 8 (depends on 1)

The optical disk as claimed in claim 1, wherein the thickness of the amorphous layer is in the range of 10˜50 Å.

### Claim 9 (depends on 1)

The optical disk as claimed in claim 1, wherein the recording layer is made of either of a Sb—Te—Ge alloy and an Ag—In—Sb—Te type alloy, and its thickness is in the range of 100˜300 Å.

### Claim 10 (depends on 1)

The optical disk as claimed in claim 1, further comprising upper and lower dielectric layers formed on upper and lower parts of the recording layer, respectively.

### Claim 11 (depends on 10)

The optical disk as claimed in claim 10, wherein the upper and lower dielectric layers are made of one selected from the group consisting of ZnS—SiO2, SiO2, SiN, (ZrxCe1-x)yO1-y, AlN, and Al2O3.

### Claim 12 (depends on 10)

The optical disk as claimed in claim 10, wherein the thickness of the upper dielectric layer is in the range of 100˜300 Å, and the thickness of the lower dielectric layer is in the range of 500˜3000 Å.

### Claim 13 (depends on 1)

The optical disk as claimed in claim 1, wherein the cover layer is made of an UV curing resin, and its thickness is in the range of 0.09˜0.12 mm.

### Claim 14

A method of fabricating an optical disk comprising the steps of:
forming by turns a first reflective layer and an amorphous layer on a substrate;
forming a second reflective layer on the amorphous layer;
forming by turns an upper dielectric layer, a recording layer, and a lower dielectric layer on a recording layer; and
forming a cover layer on the lower dielectric layer.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the step of forming by turns the first reflective layer and the dielectric layer on the substrate is repeatedly performed.

### Claim 16 (depends on 14)

The method as claimed in claim 14, wherein the first and second reflective layers are formed by simultaneously sputtering a metal and an oxide.

### Claim 17 (depends on 16)

The method as claimed in claim 16, wherein the sputtering is performed using a target in which the metal and the oxide are mixed together.

### Claim 18 (depends on 17)

The method as claimed in claim 17, wherein the target in which the metal and the oxide are mixed is either of an Al—SiO2 target and an Ag—SiO2 target.

### Claim 19 (depends on 16)

The method as claimed in claim 16, wherein the sputtering is performed using a metal target and an oxide target.

### Claim 20 (depends on 19)

The method as claimed in claim 19, wherein the metal target is any one of an Al target and an Ag target, and the oxide target is a SiO2 target.