# US 2002/0160265 A1 · Negative electrode for lithium secondary battery and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160265 A1
- Document ID: US20020160265A1
- Status: Published application
- Kind: A1
- Application number: 10/046,697
- Filed: 2002-01-17
- Published: 2002-10-31
- Earliest claimed: 2001-01-17
- Assignees: Sanyo Electric Co., Ltd.
- Inventors: Takuya Hashimoto; Atsushi Fukui; Hiroshi Nakamura; Shin Fujitani
- Web page: https://patentgrep.com/patent/US20020160265A1

## CPC

- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- C22C 21/00: Alloys based on aluminium
- C22C 45/08: with aluminium as the major constituent
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/38: of elements or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/40: Alloys based on alkali metals
- H01M 4/624: {Electric conductive fillers}
- H01M 4/626: {Metals}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- B22F 2009/041: {by mechanical alloying, e.g. blending, milling}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 2200/02: Amorphous
- H01M 4/0483: {by methods including the handling of a melt (H01M4/0438, take precedence)}
- H01M 10/052: Li-accumulators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A negative electrode for lithium secondary battery characterized in that the electrode is obtained by sintering a mixture of an active material alloy and a binder disposed on a current collector, or a mixture of an active material alloy, conductive metal powder and a binder disposed on a current collector, and the active material alloy after sintered is substantially amorphous.

## Claims

### Claim 1

A negative electrode for lithium secondary battery, said negative electrode being obtained by sintering a mixture of an active material alloy and a binder arranged on a current collector made of metallic foil, or sintering a mixture of an active material alloy, conductive metal powder and a binder arranged on a current collector made of metallic foil,
wherein said active material alloy after said sintering process is substantially amorphous.

### Claim 2 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said active material alloy contains Si.

### Claim 3 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said active material alloy contains Al, Si and transition metal.

### Claim 4 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said sintering process is performed by heat treatment in a non-oxidizing atmosphere at a temperature lower than the crystallization temperature of said active material alloy.

### Claim 5 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said metallic foil has a surface roughness Ra of 0.2 μm or more.

### Claim 6 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said metallic foil is an electrolytic copper foil or a metallic foil having an electrolytic copper layer on its surface.

### Claim 7 (depends on 1)

The negative electrode for lithium secondary battery according to claim 1, wherein said conductive metal powder is copper or copper alloy powder.

### Claim 8

A manufacturing method of a negative electrode for lithium secondary battery, comprising the steps of:
disposing a mixture of an active material alloy which is substantially amorphous and a binder, or a mixture of said active material alloy, conductive metal powder and a binder, on a current collector made of metallic foil; and
sintering said mixture under a condition such that said active material alloy is substantially amorphous after sintered.

### Claim 9 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said sintering is performed by heat treatment in a non-oxidizing atmosphere at a temperature lower than the crystallization temperature of said active material alloy.

### Claim 10 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said active material alloy, or said active material alloy and said conductive metal powder are mixed with a solution of said binder to obtain slurry, and the obtained slurry is applied onto said current collector and then dried, and thereby, said mixture is disposed on the current collector.

### Claim 11 (depends on 10)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 10, wherein said mixture is rolled together with said current collector after said application and drying process.

### Claim 12 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said active material alloy contains Si.

### Claim 13 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said active material alloy contains Al, Si and transition metal.

### Claim 14 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said metallic foil has a surface roughness Ra of 0.2 μm or more.

### Claim 15 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said metallic foil is an electrolytic copper foil or a metallic foil having an electrolytic copper layer on its surface.

### Claim 16 (depends on 8)

The manufacturing method of a negative electrode for lithium secondary battery according to claim 8, wherein said conductive metal powder is copper or copper alloy powder.

### Claim 17 (depends on 1)

A lithium secondary battery comprising; the negative electrode according to claim 1, a positive electrode and a non-aqueous electrolyte.

### Claim 18 (depends on 8)

A lithium secondary battery comprising; the negative electrode manufactured by the method according to claim 8, a positive electrode and a non-aqueous electrolyte.