# US 2002/0160236 A1 · Transparent electroconductive film and process for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160236 A1
- Document ID: US20020160236A1
- Status: Published application
- Kind: A1
- Application number: 10/103,120
- Filed: 2002-03-22
- Published: 2002-10-31
- Earliest claimed: 2001-03-27
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Takeshi Hattori; Kunio Saegusa; Yozo Shigesato
- Web page: https://patentgrep.com/patent/US20020160236A1

## CPC

- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

There are provided: (1) a process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering simultaneously: (i) a target (A) for sputtering, which comprises In, Sb and O, and whose atomic ratio of Sb/In is from 0.9 to 1.1, and (ii) a target (B) for sputtering, which comprises Sb, (2) a transparent eletroconductive film, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 0.8 to 1.5, and (3) a target for sputtering, which contains In. Sb and O, and whose atomic ratio of Sb/In is from 1.2 to 2.0.

## Claims

### Claim 1

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering simultaneously:
(i) a target (A) for sputtering, which comprises In, Sb and O, and whose atomic ratio of Sb/In is from 0.9 to 1.1, and
(ii) a target (B) for sputtering, which comprises Sb.

### Claim 2 (depends on 1)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 1, wherein a ratio of an area of the target (A) for sputtering to that of the target (B) for sputtering is 1:0.001 to 0.1.

### Claim 3 (depends on 1)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 1, which further comprises the step of calcining at a temperature ranging from 500° C. to 1100° C. after the step of sputtering.

### Claim 4 (depends on 1)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 1, wherein an atomic ratio of Sb/In in the InSbO4-containing transparent electroconductive film is from 0.8 to 1.5.

### Claim 5

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering simultaneously:
(i) a target (A) for sputtering, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 0.9 to 1.1,
(ii) a target (B) for sputtering, which contains Sb, and
(iii) at least one target (C) for sputtering selected from the group consisting of Sn, SnO2, Hf and HfO2.

### Claim 6 (depends on 5)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 5, wherein a ratio of an area of the target (A) for sputtering to that of the target (B) for sputtering is 1:0.001 to 0.1.

### Claim 7 (depends on 5)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 5, which further comprises the step of calcining at a temperature ranging from 500° C. to 1100° C. after the step of sputtering.

### Claim 8 (depends on 5)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 5, wherein an atomic ratio of Sb/In in the InSbO4-containing transparent electroconductive film is from 0.8 to 1.5.

### Claim 9

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering simultaneously:
(i) a target (D) for sputtering, which contains In, Sb, O and at least one element selected from the group consisting of Sn and Hf, and whose atomic ratio of Sb/In is from 0.9 to 1.1, and
(ii) a target (B) for sputtering, which contains Sb.

### Claim 10 (depends on 9)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 9, wherein a ratio of an area of the target (D) for sputtering to that of the target (B) for sputtering Is 1:0.001 to 0.1.

### Claim 11 (depends on 9)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 9, which further comprises the step of calcining at a temperature ranging from 500° C. to 1100° C. after the step of sputtering.

### Claim 12 (depends on 9)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 9, wherein an atomic ratio of Sb/In In the InSbO4-containing transparent electroconductive film is from 0.8 to 1.5.

### Claim 13

A transparent eletroconductive film, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 0.8 to 1.5.

### Claim 14

A transparent electroconductive film, which contains In, Sb, O and at least one element selected from the group consisting of Sn and Hf, and whose atomic ratio of Sb/In is from 0.8 to 1.5.

### Claim 15

A target for sputtering, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 1.2 to 2.0.

### Claim 16

A target for sputtering, which contains In, Sb, O and at least one element selected from the group consisting of Sn and Hf, and whose atomic ratio of Sb/In is from 1.2 to 2.0.

### Claim 17

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering a target (E) for sputtering, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 1.2 to 2.0.

### Claim 18 (depends on 17)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 17, which further comprises the step of calcining at an ultimate maximum temperature ranging from 500° C. to 1100° C. after the step of sputtering.

### Claim 19

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering simultaneously:
(i) a target (E) for sputtering, which contains In, Sb and O, and whose atomic ratio of Sb/In is from 1.2 to 2.0, and
(ii) at least one target (C) for sputtering selected from the group consisting of Sn, SnO2, Hf and HfO2.

### Claim 20 (depends on 19)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 19, which further comprises the step of calcining at an ultimate maximum temperature ranging from 500° C. to 1100° C. after the step of sputtering.

### Claim 21

A process for producing an InSbO4-containing transparent electroconductive film, which comprises the step of sputtering a target (F) for sputtering, which contains In, Sb, O and at least one element selected from the group consisting Sn and Hf, and whose atomic ratio of Sb/In is from 1.2 to 2.0.

### Claim 22 (depends on 21)

The process for producing an InSbO4-containing transparent electroconductive film according to claim 21, which further comprises the step of calcining at an ultimate maximum temperature ranging from 500° C. to 110° C. after the step of sputtering.