# US 2002/0160217 A1 · Method for producing biaxially stretched film made of ethylene-vinyl alcohol copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0160217 A1
- Document ID: US20020160217A1
- Status: Published application
- Kind: A1
- Application number: 10/073,988
- Filed: 2002-02-14
- Published: 2002-10-31
- Earliest claimed: 2001-02-23
- Assignees: Kuraray Co., Ltd.
- Inventors: Kazuhisa Okada; Nariaki Fujii
- Web page: https://patentgrep.com/patent/US20020160217A1

## CPC

- B32B 27/08: of synthetic resin
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 38/0036: {Heat treatment (for heating or cooling of layers during lamination B32B37/06, B32B37/08)}
- B32B 38/1825: {characterised by the control or constructional features of devices for tensioning, stretching or registration}
- C08J 5/18: Manufacture of films or sheets
- B29L 2031/712: {Containers; Packaging elements or accessories, Packages (closures therefor B29L2031/56; ink or toner cartridges B29L2031/7678; squeeze tubes B29L2023/20; suitcases B29L2031/7418)}
- B32B 2329/04: Polyvinylalcohol
- C08J 2329/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- Y10S 428/91: Product with molecular orientation
- Y10T 428/31928: Ester, halide or nitrile of addition polymer
- Y10T 428/31935: Ester, halide or nitrile of addition polymer
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a biaxially stretched film is provided, in which the method comprises, stretching a film made mainly of an ethylene-vinyl alcohol copolymer having an ethylene content of 15 to 70 mol % and a saponification degree of 80 mol % or more under heating; cooling the film; and subjecting the cooled film to a heat treatment; wherein a heating temperature during the stretching is 60 to 160° C., a cooling temperature is a temperature 30 to 100° C. lower than the heating temperature during the stretching, and a temperature for the heat treatment is 150 to 190° C. The thus obtained biaxially stretched film of the present invention has a small bowing coefficient.

## Claims

### Claim 1

A method for producing a biaxially stretched film comprising:
stretching a film made mainly of an ethylene-vinyl alcohol copolymer having an ethylene content of 15 to 70 mol % and a saponification degree of 80 mol % or more under heating,
cooling the film, and
subjecting the cooled film to a heat treatment,
wherein a heating temperature during the stretching is 60 to 160° C., a cooling temperature is a temperature 30 to 100° C. lower than the heating temperature during the stretching, and a temperature for the heat treatment is 150 to 190° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the stretching is simultaneous biaxial stretching.

### Claim 3 (depends on 1, 2)

The method of claim 1 or 2, wherein preheating is performed at 60 to 160° C. before the stretching.

### Claim 4 (depends on 1, 2, 3)

The method of any one of claims 1 to 3, wherein a stretching ratio in a longitudinal direction is 2.5 to 4.5, a stretching ratio in a transverse direction is 2.5 to 4.5, and an area stretching ratio is 7 to 15 in the biaxially stretched film.

### Claim 5 (depends on 1, 2, 3, 4)

The method of any one of claims 1 to 4, wherein a bowing coefficient of the biaxially stretched film is 15% or less.

### Claim 6 (depends on 1, 2, 3, 4, 5)

An ethylene-vinyl alcohol copolymer biaxially stretched film produced by the method of any one of claims 1 to 5, wherein the film has a dry heat shrinkage coefficient in a longitudinal direction of 4.0% or less.

### Claim 7 (depends on 6)

A laminate comprising a layer made of the ethylene-vinyl alcohol copolymer biaxially stretched film of claim 6 and a layer made of another thermoplastic resin.

### Claim 8 (depends on 7)

The laminate of claim 7, wherein the thermoplastic resin is a polyolefin.