# US 2002/0157806 A1 · Process for producing vanadium alloy foil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0157806 A1
- Document ID: US20020157806A1
- Status: Published application
- Kind: A1
- Application number: 10/076,356
- Filed: 2002-02-19
- Published: 2002-10-31
- Earliest claimed: 2001-02-19
- Assignees: Fukuda Metal Foil & Powder Co., Ltd.
- Inventors: Motonori Nishida; Akira Takagi; Toshiki Ohnishi; Osamu Kajita
- Web page: https://patentgrep.com/patent/US20020157806A1

## CPC

- B22D 11/06: into moulds with travelling walls, e.g. with rolls, plates, belts, caterpillars
- C22B 34/22: Obtaining vanadium
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

The invention provides a process for producing vanadium alloy foil suitable as a membrane in a hydrogen-refining unit. A vanadium alloy comprising 5 to 25% by weight of at least one selected from the group consisting of Ni, Co, Mo, Fe and Ag, 0.01 to 5% by weight of at least one selected from the group consisting of Ti, Zr and Y, and the balance being V is used. A melt of the vanadium alloy is prepared by use of a crucible 1 having slit 3 in the bottom, a roll 2 comprising a cylinder whose central axis is arranged to be parallel to the slit is rotated, the melt is jetted from the slit 3 to the roll surface 5, the melt is jetted from the slit 3 is rapidly cooled, and the vanadium alloy solidified on the roll surface 5 is continuously exfolitated from the roll surface 5 to obtain the foil.

## Claims

### Claim 1

A process for producing foil of a vanadium alloy comprising 5 to 25% by weight of at least one selected from the group consisting of Ni, Co, Mo, Fe and Ag, 0.01 to 5% by weight of at least one selected from the group consisting of Ti, Zr and Y, and the balance being V, which comprises the steps of:
preparing a melt of the vanadium alloy by use of a crucible having a slit in the bottom,
rotating a roll comprising a cylinder whose central axis is arranged to be parallel to the slit,
jetting the melt from the slit to the roll surface of the rotating roll and rapidly cooling the melt jetted from the slit, and
continuously removing the vanadium alloy solidified on the roll surface from the roll surface to give foil of the vanadium alloy.

### Claim 2 (depends on 1)

The process according to claim 1, wherein said vanadium alloy further comprises 0.01 to 1% by weight of Si and/or B.

### Claim 3 (depends on 1)

The process according to claim 1, wherein said vanadium alloy further comprises 0.01 to 5% by weight of at least one selected from the group consisting of Ru, Rh, Pd, Os, Ir, Pt, Au, Cu, Cr and W.

### Claim 4 (depends on 1)

The process according to claim 1, wherein said vanadium alloy further comprises 0.01 to 5% by weight of at least one selected from the group consisting of In, Sn and Bi.

### Claim 5 (depends on 1)

The process according to claim 1, wherein said roll is rotated such that said roll surface is moved at a rate of 450 to 20000 m/min.

### Claim 6 (depends on 1)

The process according to claim 1, wherein said foil having an amorphous crystal structure is produced.