# US 2002/0153061 A1 · Method and apparatus for producing compact of rare earth alloy powder and rare earth magnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0153061 A1
- Document ID: US20020153061A1
- Status: Published application
- Kind: A1
- Application number: 10/166,250
- Filed: 2002-06-11
- Published: 2002-10-24
- Earliest claimed: 1999-10-25
- Assignees: Sumitomo Special Metals Co., Ltd.
- Inventors: Tsutomu Harada; Hitoshi Morimoto; Atsuo Tanaka
- Web page: https://patentgrep.com/patent/US20020153061A1

## CPC

- H01F 1/0576: {pressed, e.g. hot working}
- B22F 3/02: Compacting only
- B22F 3/03: Press-moulding apparatus therefor
- B30B 11/008: {Applying a magnetic field to the material}
- H01F 41/0273: {Imparting anisotropy (methods and devices for magnetising permanent magnets H01F13/003)}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B30B: PRESSES IN GENERAL (producing ultra-high pressure or ultra-high pressure and high temperature to effect modifications of a substance, e.g. for making artificial diamonds B01J3/00 ){(compressing means for refuse receptacles B65F1/1405)}

## Abstract

A method for producing a compact of rare earth alloy powder of the present invention includes: a powder-filling step of filling rare earth allow powder in a cavity formed by inserting a lower punch into a through hall of a die of a powder compacting machine; and a compression step of pressing the rare earth alloy powder while applying a magnetic field, the steps being repeated a plurality of times. When the (n+1)th (n is an integer equal to or more than 1) stage compression step is to be carried out, the top surface of a compact produced in the n-th stage compression step is placed at a position above the bottom surface of a magnetic portion of a die.

## Claims

### Claim 1

A method for producing a compact of rare earth alloy powder comprising:
a first step of filling the rare earth alloy powder in a cavity of a compacting machine, said machine comprising a lower punch and an upper punch,
a second step of pressing the rare earth alloy powder while applying a magnetic field to the rare earth alloy powder and detecting a pressure applied to the rare earth alloy powder in the cavity by a pressure sensor; and
a step of repeating the first step and the second step to produce the compact of the rare earth alloy powder;
wherein the relative position of the upper punch and the lower punch is controlled according to the pressure detected by the pressure sensor.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the compacting machine further comprises a die including a nonmagnetic portion and a magnetic portion placed on the nonmagnetic portion, the die having a through hole; and a magnetic core having an outer circumference facing an inner wall of the through hole,
wherein the lower punch is inserted from below into a space formed between the inner wall of the through hole and the outer circumference of the magnetic core, and the upper punch is inserted from above into the space formed between the inner wall of the through hole and the outer circumference of the magnetic core,
wherein when an (n+1)th stage second step is to be carried out, where n is an integer equal to or greater than 1, a top surface of a compact produced in an n-th stage second step is placed at a position above a bottom surface of the magnetic portion of the die.

### Claim 3 (depends on 2)

A method according to claim 2, wherein in the (n+1)th stage second step, the level difference between the top surface of the compact produced in the n-th stage compression step and the bottom surface of the magnetic portion of the die is 3 mm or more.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the density of the compact produced in the second step is adjusted by controlling the pressure applied to the rare earth alloy powder.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the intensity of the magnetic field in the cavity is 0.4 MA/m or more.

### Claim 6 (depends on 1)

A method according to claim 1, wherein a lubricant is added to the rare earth alloy powder.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the amount of the rare earth alloy powder filled in the cavity is larger in an n-th stage first step than in an (n+1)th stage first step, where n is an integer equal to or greater than 1.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the rare earth alloy powder is made of a R-T-(M)-B alloy, where R denotes a rare earth element containing at least one of the element selected from the group consisting of Y, La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu; T denotes Fe or a mixture of Fe and Co; M denotes an additive element; and B denotes boron.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the compact is formed in a cylindrical shape, and the magnetic field is a radial magnetic field.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the density of the compact produced in an n-th stage compression step is 3.5 g/cm3 or more.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the rare earth alloy powder is filled in the cavity from a feeder box storing the rare earth alloy powder therein.

### Claim 12 (depends on 1)

A method according to claim 1, wherein the rare earth alloy powder is produced by a strip casting method.

### Claim 13 (depends on 1)

A method for manufacturing a rare earth magnet comprising sintering a compact produced by the method for producing a compact of rare earth alloy powder according to claim 1, to obtain a permanent magnet.

### Claim 14

A method for producing a compact of rare earth alloy powder comprising:
forming a first cavity defined by a die and a lower punch;
filling rare earth alloy powder in the first cavity;
compressing the powder filled in the first cavity until a pressure applied to the powder in the first cavity reaches a first predetermined value;
forming a second cavity on the compressed powder by relative movement of the die and the lower punch after compressing the powder filled in the first cavity;
filling rare earth alloy powder in the second cavity; and
compressing the powder filled in the second cavity until a pressure applied to the powder in the second cavity reaches a second predetermined value.

### Claim 15 (depends on 14)

A method according to claim 14, further comprising a step of storing the position of a top surface of the compact produced in the first cavity, wherein the second cavity is formed by the relative movement of the die and the lower punch based on the position of the top surface of the compact.

### Claim 16 (depends on 14)

A method according to claim 14, wherein the first cavity and the second cavity are of a cylindrical shape.

### Claim at position 17

17 A rare earth magnet manufactured by repeating a plurality of times a powder-filling step comprising filling rare earth alloy powder in a cavity and a compression step comprising pressing the rare earth alloy powder while applying a magnetic field,
wherein the surface magnetic flux density at a boundary of an upper compact produced in an (n+1)th stage compression step, where n is an integer equal to or greater than 1, and a lower compact produced in an n-th stage compression step is 65% or more of the maximum value greater than 0.2 T of the surface magnetic flux density at the other portions of the compact.