# US 2002/0152951 A1 · Method of epitaxially growing device structures with submicron group III nitride layers utilizing HVPE

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0152951 A1
- Document ID: US20020152951A1
- Status: Published application
- Kind: A1
- Application number: 10/113,692
- Filed: 2002-03-28
- Published: 2002-10-24
- Earliest claimed: 2001-03-30
- Assignees: Technologies and Devices International, Inc.
- Inventors: Denis V. Tsvetkov; Andrey E. Nikolaev; Vladimir A. Dmitriev
- Web page: https://patentgrep.com/patent/US20020152951A1

## CPC

- C30B 25/16: Controlling or regulating (controlling or regulating in general G05)
- C23C 16/303: {Nitrides}
- C23C 16/4488: {by in situ generation of reactive gas by chemical or electrochemical reaction}
- C23C 16/45514: {Mixing in close vicinity to the substrate}
- C30B 25/02: Epitaxial-layer growth
- C30B 25/08: Reaction chambers; Selection of materials therefor
- C30B 25/14: Feed and outlet means for the gases; Modifying the flow of the reactive gases
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B 29/403: {AIII-nitrides}
- C30B 29/406: {Gallium nitride}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2901: {Materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10P 14/3444: {P-type}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method and apparatus for fabricating thin Group III nitride layers as well as Group III nitride layers that exhibit sharp layer-to-layer interfaces are provided. According to one aspect, an HVPE reactor includes one or more gas inlet tubes adjacent to the growth zone, thus allowing fine control of the delivery of reactive gases to the substrate surface. According to another aspect, an HVPE reactor includes both a growth zone and a growth interruption zone. According to another aspect, an HVPE reactor includes a slow growth rate gallium source, thus allowing thin layers to be grown. Using the slow growth rate gallium source in conjunction with a conventional gallium source allows a device structure to be fabricated during a single furnace run that includes both thick layers (i.e., utilizing the conventional gallium source) and thin layers (i.e., utilizing the slow growth rate gallium source).

## Claims

### Claim 1

A method of epitaxially growing a Group III nitride semiconductor device in a single epitaxial growth run, the method utilizing HVPE techniques and comprising the steps of:
locating a first gallium (Ga) source in a source boat within a first source zone of an HVPE reactor, said first Ga source having a first exposed surface area;
locating a second Ga source in a quartz channel within a second source zone of said HVPE reactor, said Ga source having a second exposed surface area, wherein said second exposed surface area is less than said first exposed area;
locating a substrate within a growth zone of said HVPE reactor, wherein said growth zone is maintained at a first temperature;
heating said first Ga source to a second temperature;
heating said second Ga source to a third temperature;
introducing a halide reaction gas into said first source zone to form a first gallium chloride compound;
transporting said first gallium chloride compound to said growth zone;
transporting a reaction gas to said growth zone, said reaction gas containing nitrogen (N);
reacting said first gallium chloride compound with said reaction gas to achieve a first epitaxial growth rate of greater than 0.1 microns per hour;
growing a first Group III nitride layer to a thickness of greater than 5 microns;
transferring said substrate to a growth interruption zone maintained at a fourth temperature, wherein said fourth temperature is within 50° C. of said first temperature;
directing an inert gas in a flow direction that substantially prevents said first gallium chloride compound and said reaction gas from entering said growth interruption zone;
purging said growth zone;
introducing said halide reaction gas into said second source zone to form a second gallium chloride compound;
transporting said second gallium chloride compound to said growth zone;
reacting said second gallium chloride compound with said reaction gas to achieve a second epitaxial growth rate of less than 0.1 microns per hour; and
growing a second Group III nitride layer to a thickness of less than 0.02 microns.

### Claim 2 (depends on 1)

The method of claim 1, further comprising the step of discontinuing said step of transporting said first gallium chloride compound to said growth zone, said discontinuing step performed after said step of transferring said substrate to said growth interruption zone.

### Claim 3 (depends on 1)

The method of claim 1, further comprising the step of discontinuing said step of transporting said first gallium chloride compound to said growth zone, said discontinuing step performed prior to said step of transferring said substrate to said growth interruption zone.

### Claim 4 (depends on 1)

The method of claim 1, further comprising the steps of:
discontinuing said steps of transporting said first gallium chloride compound and said reaction gas to said growth zone, said discontinuing step performed after said step of transferring said substrate to said growth interruption zone; and
transporting said reaction gas to said growth zone prior to said step of reacting said second gallium chloride compound with said reaction gas.

### Claim 5 (depends on 1)

The method of claim 1, further comprising the steps of:
discontinuing said steps of transporting said first gallium chloride compound and said reaction gas to said growth zone, said discontinuing step performed prior to said step of transferring said substrate to said growth interruption zone; and
transporting said reaction gas to said growth zone prior to said step of reacting said second gallium chloride compound with said reaction gas.

### Claim 6 (depends on 1)

The method of claim 1, further comprising the steps of:
locating said substrate within said growth interruption zone prior to said steps of transporting said first gallium chloride compound and said reaction gas to said growth zone;
stabilizing the reaction between said reaction gas and said first gallium chloride compound; and
transferring said substrate from said growth interruption zone to said growth zone after completion of said stabilizing step.

### Claim 7 (depends on 6)

The method of claim 6, wherein said stabilizing step is performed for at least three minutes.

### Claim 8 (depends on 1)

The method of claim 1, further comprising the step of maintaining said third temperature to within 25° C. of said first temperature.

### Claim 9 (depends on 1)

The method of claim 1, further comprising the step of maintaining said third temperature to within 10° C. of said first temperature.

### Claim 10 (depends on 1)

The method of claim 1, further comprising the step of maintaining said third temperature to within 5° C. of said first temperature.

### Claim 11 (depends on 1)

The method of claim 1, further comprising the step of maintaining said third temperature to within 1° C. of said first temperature.

### Claim 12 (depends on 1)

The method of claim 1, wherein said flow direction of said inert gas directing step is substantially orthogonal to a source flow direction.

### Claim 13 (depends on 1)

The method of claim 1, wherein said flow direction of said inert gas directing step is substantially opposite to a source flow direction.

### Claim 14 (depends on 1)

The method of claim 1, wherein said flow direction of said inert gas directing step is angled at a growth surface of said substrate

### Claim 15 (depends on 1)

The method of claim 1, further comprising the steps of:
locating a first supplemental Group III metal in a third source zone of said HVPE reactor;
heating said first supplemental Group III metal to a fifth temperature;
introducing said halide reaction gas into said third source zone to form a first supplemental Group III metal halide compound; and
transporting said first supplemental Group III metal halide compound to said growth zone, wherein said first Group III nitride layer is comprised of said Ga, said first supplemental III metal and nitrogen, and wherein said first Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound and said first supplemental Group III metal halide compound.

### Claim 16 (depends on 15)

The method of claim 15, wherein said first supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 17 (depends on 15)

The method of claim 15, further comprising the steps of:
locating a second supplemental Group III metal in a fourth source zone of said HVPE reactor;
heating said second supplemental Group III metal to a sixth temperature;
introducing said halide reaction gas into said fourth source zone to form a second supplemental Group III metal halide compound; and
transporting said second supplemental Group III metal halide compound to said growth zone, wherein said first Group III nitride layer is comprised of said Ga, said first supplemental Group III metal, said second supplemental Group III metal and nitrogen, and wherein said first Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound, said first supplemental Group III metal halide compound and said second supplemental Group III metal halide compound.

### Claim 18 (depends on 17)

The method of claim 17, wherein said second supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 19 (depends on 17)

The method of claim 17, further comprising the steps of:
locating a third supplemental Group III metal in a fifth source zone of said HVPE reactor;
heating said third supplemental Group III metal to a seventh temperature;
introducing said halide reaction gas into said fifth source zone to form a third supplemental Group III metal halide compound; and
transporting said third supplemental Group III metal halide compound to said growth zone, wherein said first Group III nitride layer is comprised of said Ga, said first supplemental Group III metal, said second supplemental Group III metal, said third supplemental Group III metal and nitrogen, and wherein said first Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound, said first supplemental Group III metal halide compound, said second supplemental Group III metal halide compound and said third supplemental Group III metal halide compound.

### Claim 20 (depends on 19)

The method of claim 19, wherein said third supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 21 (depends on 1)

The method of claim 1, further comprising the steps of:
locating a first supplemental Group III metal in a third source zone of said HVPE reactor;
heating said first supplemental Group III metal to a fifth temperature;
introducing said halide reaction gas into said third source zone to form a first supplemental Group III metal halide compound; and
transporting said first supplemental Group III metal halide compound to said growth zone, wherein said second Group III nitride layer is comprised of said Ga, said first supplemental III metal and nitrogen, and wherein said second Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound and said first supplemental Group III metal halide compound.

### Claim 22 (depends on 21)

The method of claim 21, wherein said first supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 23 (depends on 21)

The method of claim 21, further comprising the steps of:
locating a second supplemental Group III metal in a fourth source zone of said HVPE reactor;
heating said second supplemental Group III metal to a sixth temperature;
introducing said halide reaction gas into said fourth source zone to form a second supplemental Group III metal halide compound; and
transporting said second supplemental Group III metal halide compound to said growth zone, wherein said second Group III nitride layer is comprised of said Ga, said first supplemental Group III metal, said second supplemental Group III metal and nitrogen, and wherein said second Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound, said first supplemental Group III metal halide compound and said second supplemental Group III metal halide compound.

### Claim 24 (depends on 23)

The method of claim 23, wherein said second supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 25 (depends on 21)

The method of claim 21, further comprising the steps of:
locating a third supplemental Group III metal in a fifth source zone of said HVPE reactor;
heating said third supplemental Group III metal to a seventh temperature;
introducing said halide reaction gas into said fifth source zone to form a third supplemental Group III metal halide compound; and
transporting said third supplemental Group III metal halide compound to said growth zone, wherein said second Group III nitride layer is comprised of said Ga, said first supplemental Group III metal, said second supplemental Group III metal, said third supplemental Group III metal and nitrogen, and wherein said second Group III nitride layer is formed by said reaction gas reacting with said gallium chloride compound, said first supplemental Group III metal halide compound, said second supplemental Group III metal halide compound and said third supplemental Group III metal halide compound.

### Claim 26 (depends on 25)

The method of claim 25, wherein said third supplemental Group III metal is selected from the group consisting of aluminum (Al), indium (In) and boron (B).

### Claim 27 (depends on 1)

The method of claim 1, further comprising the step of transporting at least one acceptor impurity metal to said growth zone, wherein said first Group III nitride layer contains said at least one acceptor impurity metal.

### Claim 28 (depends on 27)

The method of claim 27, wherein said first Group III nitride layer has a p-type conductivity.

### Claim 29 (depends on 27)

The method of claim 27, wherein said at least one acceptor impurity metal is selected from the group consisting of magnesium (Mg), zinc (Zn) and magnesium-zinc (MgZn) alloys.

### Claim 30 (depends on 1)

The method of claim 1, further comprising the step of transporting at least one acceptor impurity metal to said growth zone, wherein said second Group III nitride layer contains said at least one acceptor impurity metal.

### Claim 31 (depends on 30)

The method of claim 30, wherein said second Group III nitride layer has a p-type conductivity.

### Claim 32 (depends on 30)

The method of claim 30, wherein said at least one acceptor impurity metal is selected from the group consisting of magnesium (Mg), zinc (Zn) and magnesium-zinc (MgZn) alloys.

### Claim 33 (depends on 1)

The method of claim 1, further comprising the step of transporting at least one donor impurity to said growth zone, wherein said first Group III nitride layer contains said at least one donor impurity.

### Claim 34 (depends on 33)

The method of claim 33, wherein said at least one donor is selected from the group consisting of oxygen (O), germanium (Ge), silicon (Si) and tin (Sn).

### Claim 35 (depends on 1)

The method of claim 1, further comprising the step of transporting at least one donor impurity to said growth zone, wherein said second Group III nitride layer contains said at least one donor impurity.

### Claim 36 (depends on 35)

The method of claim 35, wherein said at least one donor is selected from the group consisting of oxygen (O), germanium (Ge), silicon (Si) and tin (Sn).

### Claim 37 (depends on 1)

The method of claim 1, wherein said thickness of said second Group III nitride layer is less than 0.01 microns.

### Claim 38 (depends on 1)

The method of claim 1, wherein said thickness of said second Group III nitride layer is less than 0.005 microns.

### Claim 39 (depends on 1)

The method of claim 1, further comprising the steps of:
locating a Group V material in a third source zone of said HVPE reactor; and
transporting said Group V material to said growth zone, wherein said first Group III nitride layer is comprised of said gallium, said Group V material and nitrogen.

### Claim 40 (depends on 1)

The method of claim 1, further comprising the steps of:
locating a Group V material in a third source zone of said HVPE reactor; and
transporting said Group V material to said growth zone, wherein said second Group III nitride layer is comprised of said gallium, said Group V material and nitrogen.

### Claim 41 (depends on 1)

The method of claim 1, wherein said second exposed surface area is less than 4 square millimeters.

### Claim 42 (depends on 1)

The method of claim 1, wherein said second exposed surface area is less than 2 square millimeters.

### Claim 43 (depends on 1)

The method of claim 1, wherein said second exposed surface area is less than 1 square millimeter.

### Claim 44 (depends on 1)

The method of claim 1, wherein said second expitaxial growth rate is less than 0.05 microns per hour.

### Claim 45 (depends on 1)

The method of claim 1, wherein said second expitaxial growth rate is less than 0.01 microns per hour.

### Claim 46 (depends on 1)

The method of claim 1, wherein said second expitaxial growth rate is less than 0.005 microns per hour.

### Claim 47 (depends on 1)

The method of claim 1, further comprising the step of growing an additional Group III nitride layer, said additional Group III nitride layer interposed between said substrate and said first Group III nitride layer.