Abrasive tape, process for producing it, and coating agent for abrasive tape
AssigneeDai Nippon Printing Co., Ltd.
InventorsKazuhito Fujii, Masahisa Yamaguchi, Takaki Miyachi, Kojiro Okawa, Yasuki Suzuura
Life of this patent
Estimating the term…
Abstract
Provided are an abrasive tape suitable for finishing of surfaces or the like of precision components such as optical connector ferrules and semiconductor wafers, and a process for producing it. A coating agent in which abrasive particles having an average particle size in the range of 1 to 200 mμ are dispersed in a binder resin solution. The coating agent is applied, with intervention of a primer layer if necessary, onto a base for abrasive tape to form an abrasive layer, thus obtaining an abrasive tape.
Claims22
An abrasive tape comprising:
- a base for abrasive tape;
- and
- an abrasive layer formed on the base;
- wherein the abrasive layer is formed from a coating agent in which abrasive particles of an average particle size in the range of 10 to 100 mμ are dispersed in a binder resin solution.
A process for producing an abrasive tape, comprising the steps of:
- dispersing abrasive particles of an average particle size in the range of 10 to 100 mμ in a binder resin solution,
- producing aggregates of the abrasive particles in the binder resin solution to obtain a coating agent containing the abrasive particles of particle diameters 50 to 800 mμ, and
- applying the coating agent onto a base for abrasive tape.
An abrasive tape comprising:
- a base for abrasive tape;
- and
- an abrasive layer formed on the base;
- wherein said abrasive layer has abrasive particles of an average particle size in the range of 1 to 200 mμ and a binder for binding the abrasive particles.
A coating agent for production of an abrasive tape, comprising:
- an abrasive particle solution containing abrasive particles of an average particle size in the range of 1 to 200 mμ and a solvent for abrasive particles, and
- a binder resin solution containing a binder and a binder solvent.
A process for producing an abrasive tape, comprising the steps of:
- preparing a base for abrasive tape;
- mixing an abrasive particle solution containing abrasive particles of an average particle size in the range of 1 to 200 mμ and a solvent for abrasive particles, with a binder resin solution containing a binder and a binder solvent to produce a coating agent;
- applying the coating agent onto the base for abrasive tape;
- and
- drying the coating agent thus applied.