# US 2002/0119654 A1 · Method for dual-damascene patterning of low-k interconnects using spin-on distributed hardmask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0119654 A1
- Document ID: US20020119654A1
- Status: Published application
- Kind: A1
- Application number: 09/795,417
- Filed: 2001-02-28
- Published: 2002-08-29
- Earliest claimed: 2001-02-28
- Assignees: International Business Machines Corporation
- Inventors: Ann Rhea-Helene Fornof; Stephen McConnell Gates; Jeffrey Curtis Hedrick; Satyanarayana V. Nitta; Sampath Purushothaman; Christy Sensenich Tyberg
- Web page: https://patentgrep.com/patent/US20020119654A1

## CPC

- H10W 20/071: {of dielectric parts thereof}
- H10P 50/73: {using masks for insulating materials}
- H10P 95/08: {Planarisation of organic insulating materials}
- H10W 20/087: {involving multiple stacked pre-patterned masks}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A cost effective and simple method of patterning interconnect structures is provided in which spun-on materials are used as the hard mask. The use of spun-on materials for the hard mask ensures that the process is carried out in a single tool and it permits the use of a single curing step which is not typically employed in prior art patterning processes wherein CVD hard masks are employed. The effective dielectric constant of the resultant structure is not significantly increased since the use of spin coating allows for selection of a polish stop layer (formed on a surface of a low-k dielectric) that has substantially the same dielectric constant as the underlying dielectric. In the present invention, the hard mask employed includes at least two spun-on dielectric materials that have different etch rates.

## Claims

### Claim 1

A method of forming a patterned interconnect structure comprising the steps of:
(a) spin-on coating a dielectric material having a dielectric constant of about 3.5 or less on the surface of a substrate;
(b) forming a hard mask comprising at least a polish stop layer and a patterning layer on a surface of said dielectric material, wherein said polish stop layer and said patterning layer have different etching rates and are both formed by spin-on coating, said polish stop layer has a dielectric constant that is compatible with said dielectric material and has an etch selectivity to said dielectric material, and said patterning layer has an etch selectivity to said polish stop layer;
(c) curing said hard mask and said dielectric material;
(d) forming an opening in said hard mask so as to expose a portion of said dielectric material;
(e) etching said exposed portion of said dielectric material so as to form a trench in said dielectric material;
(f) filling said trench with at least a conductive metal; and
(g) planarizing said conductive metal stopping on the uppermost surface of said polish stop layer.

### Claim 2 (depends on 1)

The method of claim 1 wherein said dielectric material has a dielectric constant of from about 1.4 to about 3.8.

### Claim 3 (depends on 1)

The method of claim 1 wherein said dielectric material is an organic-containing polymeric material.

### Claim 4 (depends on 3)

The method of claim 3 wherein said organic-containing polymeric material is porous.

### Claim 5 (depends on 3)

The method of claim 3 wherein said organic-containing polymeric material comprises C, O and H.

### Claim 6 (depends on 3)

The method of claim 3 wherein said organic-containing polymeric material is an aromatic thermosetting polymeric resin.

### Claim 7 (depends on 1)

The method of claim 1 wherein an adhesion promoter is formed on said substrate prior to step (a).

### Claim 8 (depends on 7)

The method of claim 7 wherein said adhesion promoter comprises an alkoxysilane.

### Claim 9 (depends on 7)

The method of claim 7 wherein said adhesion promoter is formed by spin-on coating.

### Claim 10 (depends on 1)

The method of claim 1 wherein said substrate is a dielectric material, a buried barrier layer, a metal wiring layer or a semiconductor wafer.

### Claim 11 (depends on 1)

The method of claim 1 wherein said spun-on dielectric is hot plate baked prior to step (b).

### Claim 12 (depends on 11)

The method of claim 11 wherein said hot plate baking is carried out at temperature of from about 90° to about 500° C. for a time period of from about 10 to about 600 seconds.

### Claim 13 (depends on 1)

The method of claim 1 wherein polish stop layer is an inorganic-containing dielectric.

### Claim 14 (depends on 13)

The method of claim 13 wherein said inorganic dielectric has a dielectric constant comprises Si, O and H, and optionally C.

### Claim 15 (depends on 1)

The method of claim 1 wherein said polish stop layer has a low chemical mechanical polishing (CMP) rate in a metal CMP process.

### Claim 16 (depends on 1)

The method of claim 1 wherein said patterning layer is composed of an organic-containing dielectric.

### Claim 17 (depends on 1)

The method of claim 1 wherein said polish stop layer and said patterning layer are subjected to separate hot plate bake processes after formation of each layer.

### Claim 18 (depends on 1)

The method of claim 1 wherein said curing step is carried out by a hot plate bake process.

### Claim 19 (depends on 1)

The method of claim 1 wherein said curing step is carried out by furnace heating.

### Claim 20 (depends on 1)

The method of claim 1 wherein step (d) includes two separate and distinct lithography and etching processes.

### Claim 21 (depends on 1)

The method of claim 1 wherein step (e) includes etching in oxygen or a reducing gas atmosphere.

### Claim 22 (depends on 1)

The method of claim 1 wherein said trench is a via opening, a line opening or both.

### Claim 23 (depends on 1)

The method of claim 1 wherein a liner material is formed in said trench prior to filling.

### Claim 24 (depends on 23)

The method of claim 23 wherein said liner is composed of TaN, TiN, Ta, Ti, W, WN, Cr, Nb or mixtures thereof.

### Claim 25 (depends on 1)

The method of claim 1 wherein said conductive metal is composed of Al, Cu, W, Ag or alloys thereof.

### Claim 26 (depends on 25)

The method of claim 25 wherein said conductive metal is Cu.

### Claim 27 (depends on 1)

The method of claim 1 wherein step (g) includes chemical-mechanical polishing.