# US 2002/0119324 A1 · Charging member, charging device and manufacture of charging roller

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0119324 A1
- Document ID: US20020119324A1
- Status: Published application
- Kind: A1
- Application number: 09/984,709
- Filed: 2001-10-31
- Published: 2002-08-29
- Earliest claimed: 2000-11-02
- Assignees: Bridgestone Corporation
- Inventors: Hiroshi Harashima; Shohei Morikawa; Tomoyuki Yusa; Yasushi Inoue; Takeshi Murayama
- Web page: https://patentgrep.com/patent/US20020119324A1

## CPC

- G03G 15/0233: {Structure, details of the charging member, e.g. chemical composition, surface properties}
- Y10T 428/31554: Next to second layer of polyamidoester
- Y10T 428/31587: Hydrocarbon polymer [polyethylene, polybutadiene, etc.]
- Y10T 428/31598: Next to silicon-containing [silicone, cement, etc.] layer
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In order to obtain a charging member which is free of problems such as bleeding of a conductive agent and environment dependency, has little voltage dependency, and can be preferably used in a charging system of impressing only a DC voltage, there is provided a charging member comprising an elastic layer, a resistance regulation layer provided on the elastic layer, and a skin layer provided on the resistance regulation layer, wherein the resistance regulation layer is formed by use of a resin composition prepared by blending an ion conductive substance having a molecular weight of 30 to 800 as a conductive agent into a low-resistance resin matrix having a resistance of 1×104 to 1×1010 Ω·cm. In the case of obtaining a charging roller by dipping rollers in a coating material to form coating films on the surfaces of the rollers, {circle over (1)} the temperature of the coating material at the time of a dipping treatment is appropriately controlled, {circle over (2)} the temperatures of the rollers at the time of the dipping treatment are appropriately controlled, or {circle over (3)} air-blowing conditions in blowing air to the rollers to dry the coating films are appropriately controlled, whereby a charging roller with high quality can be obtained securely and stably without generating problems on a production basis such as liquid sag of the coating material and unevenness of coating film thickness.

## Claims

### Claim 1

A charging member for charging a body to be charged by bringing said charging member into contact with said body to be charged and impressing a voltage between said charging member and said body to be charged, wherein
said charging member comprises an elastic layer, a resistance regulation layer provided on said elastic layer, and a skin layer provided on said resistance regulation layer, and said resistance regulation layer is formed from a resin composition prepared by blending an ion conductive substance having a molecular weight of 30 to 800 as a conductive agent in a low-resistance resin matrix having a resistance of 1×104 to 1×1010 Ω·cm.

### Claim 2 (depends on 1)

A charging member as set forth in claim 1, wherein said ion conductive substance is blended in an amount of 1 to 10 parts by weight per 100 parts by weight of said low-resistance resin matrix.

### Claim 3 (depends on 1)

A charging member as set forth in claim 1, wherein said low-resistance resin matrix is one or at least two selected from the group consisting of urethane resin, acrylurethane resin and acrylic resin.

### Claim 4 (depends on 1)

A charging member as set forth in claim 1, wherein said ion conductive substance is one or at least two selected from the group consisting of cationic surface active agents, anionic surface active agents and nonionic surface active agents.

### Claim 5 (depends on 1)

A charging member as set forth in claim 1, wherein said resistance regulation layer is formed by applying a coating solution prepared by dispersing or dissolving said low-resistance resin matrix and said ion conductive substance.

### Claim 6 (depends on 5)

A charging member as set forth in claim 5, wherein said low-resistance resin matrix is a water-based resin, and said resistance regulation layer is formed by applying a water-based coating solution.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

A charging device comprising a charging member for charging a body to be charged by making contact with said body to be charged, and voltage impressing means for impressing a DC voltage between said body to be charged and said charging member, wherein a charging member as set forth in any one of claims 1 to 6 is used as said charging member.

### Claim 8

A method of manufacturing a charging roller comprising a step of dipping a roller in a coating material to form a coating film on the surface of the roller, wherein the dipping treatment is conducted while said coating material is kept at a substantially constant predetermined temperature in the range of 25 to 35° C.

### Claim 9 (depends on 8)

A method of manufacturing a charging roller as set forth in claim 8, wherein said coating material is a water-based coating material.

### Claim 10 (depends on 9)

A method of manufacturing a charging roller as set forth in claim 9, wherein said coating material is a water-based coating material of any of urethane coating material, acrylic coating material and emulsion coating material.

### Claim 11 (depends on 8)

A method of manufacturing a charging roller as set forth in claim 8, wherein the temperature of said coating material is controlled to be within ±1° C. of a predetermined temperature in the range of 25 to 35° C.

### Claim 12 (depends on 8)

A method of manufacturing a charging roller as set forth in claim 8, wherein said roller subjected to said dipping treatment is a roller provided with an elastic layer composed of a solid rubber or a solid or foamed urethane rubber.

### Claim 13 (depends on 8)

A method of manufacturing a charging roller as set forth in claim 8, wherein in the case of successively repeating said dipping treatment of dipping one or a plurality of rollers in said coating material under predetermined raising and lowering process conditions so as thereby to successively subject a multiplicity of said rollers to said dipping treatment, the temperature of said coating material is always kept to be substantially constant during when said dipping treatment is repeated.

### Claim 14

A method of manufacturing a charging roller comprising a step of simultaneously dipping a plurality of rollers in a coating material to thereby form a coating on the surface of each roller, wherein the temperatures of said plurality of rollers immediately before dipping are kept to be substantially uniform over all said rollers.

### Claim 15 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein the distribution of temperature in the circumferential direction of each roller is substantially uniform.

### Claim 16 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein in the case of a treatment of dipping a plurality of rollers hung in vertical direction in a coating material, the distribution of temperature at the same height of all of said hung rollers is controlled to be substantially constant.

### Claim 17 (depends on 14, 15, 16)

A method of manufacturing a charging roller as set forth in any of claims 14 to 16, wherein the dispersion of temperature of said rollers is controlled to be within ±1° C. of the average value.

### Claim 18 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein said coating material is a water-based coating material.

### Claim 19 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein said coating material is a water-based coating material of any of urethane coating material, acrylic coating material and emulsion coating material.

### Claim 20 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein said rollers subjected to said dipping treatment each comprise an elastic layer composed of a solid or foamed rubber or urethane.

### Claim 21 (depends on 14)

A method of manufacturing a charging roller as set forth in claim 14, wherein said rollers subjected to said dipping treatment are uniformly preheated at a predetermined temperature of not lower than 30° C.

### Claim 22

A method of manufacturing a charging roller comprising a step of dipping rollers in a coating material to form a coating film on the surface of each roller, wherein said plurality of rollers provided on their surfaces with said coating films by the dipping operation are hung in substantially vertical direction, and air is blown from the lower side to the upper side of said rollers to thereby dry said coating films.

### Claim 23 (depends on 22)

A method of manufacturing a charging roller as set forth in claim 22, wherein air is so blown that the air velocity of the wind colliding on each roller is substantially uniform.

### Claim 24 (depends on 22)

A method of manufacturing a charging roller as set forth in claim 22, wherein air is so blown that the air velocity of wind flowing along the outer peripheral surfaces of said rollers at an arbitrary position in the axial direction of said individual rollers is substantially uniform at any position on the circumferences of said rollers.

### Claim 25 (depends on 23, 24)

A method of manufacturing a charging roller as set forth in claim 23 or 24, wherein the variation of the air velocity is within ±0.1 m/s.

### Claim 26 (depends on 22)

A method of manufacturing a charging roller as set forth in claim 22, wherein the air velocity is substantially constant at a predetermined velocity of not greater than 1.5 m/s.