# US 2002/0119311 A1 · Polyester fiber excellent in workability and process for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0119311 A1
- Document ID: US20020119311A1
- Status: Published application
- Kind: A1
- Application number: 09/899,239
- Filed: 2001-07-06
- Published: 2002-08-29
- Earliest claimed: 1997-11-26
- Assignees: Asahi Kasei Kabushiki Kaisha
- Inventors: Katsuhiro Fujimoto; Jinichiro Kato
- Web page: https://patentgrep.com/patent/US20020119311A1

## CPC

- D06M 15/53: Polyethers (polyacetals D06M15/39)
- D01F 6/62: from polyesters
- D06M 7/00: {Treating fibres, threads, yarns, fabrics, or fibrous goods made of other substances with subsequent freeing of the treated goods from the treating medium, e.g. swelling, e.g. polyolefins (D06M10/00 takes precedence; treating fibres or filaments made of glass, mineral -, or slag wool C03C; carbon fibres D01F11/10)}
- D06M 13/02: with hydrocarbons
- D06M 13/224: Esters of carboxylic acids; Esters of carbonic acid
- D06M 2200/40: Reduced friction resistance, lubricant properties; Sizing compositions
- Y10T 428/2913: Rod, strand, filament or fiber
- Y10T 428/2969: Polyamide, polyimide or polyester
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.: 0.18≦Q/R≦0.45 (1) The polyester fiber of the present invention is a poly(trimethylene terephthalate) fiber which has an elongation, a thermal stress and a boil-off shrinkage in appropriate ranges, and the woven or knitted fabric prepared therefrom shows inhibition of an excessive thermal shrinkage during processing and manifests a low elastic modulus and a soft hand touch. Accordingly, the polyester fiber of the present invention is suitable for use in innerwear, outerwear, sportswear, legwear, lining cloths, swimwear and the like. In addition, the polyester fiber can be stably manufactured in high productivity by a process in which spinning and drawing are consecutively conducted to prevent the undrawn yarn from aging.

## Claims

### Claim 1

A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
0.18≦Q/R≦0.45 (1)

### Claim 2 (depends on 1)

The polyester fiber according to claim 1, wherein the peak value of a thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 3

A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C., and being wound into a cheese-like package:
0.18≦Q/R≦0.45 (1)

### Claim 4 (depends on 3)

The polyester fiber according to claim 3, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 5

A cheese-like package which is formed by winding a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
0.18≦Q/R≦0.45 (1)
and which shows a bulging rate of 10% or less.

### Claim 6 (depends on 5)

The cheese-like package according to claim 5, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 7

A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of a thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):
0.18≦Q/R≦0.45 (1) 0.2≦S/T≦0.85 (2)
wherein T is the peak value (g/d) of a thermal stress, and S is a thermal stress (g/d) at 100° C.

### Claim 8 (depends on 7)

The polyester fiber according to claim 7, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 9

A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of the thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):
0.18≦Q/R≦0.45 (1) 0.2≦S/T≦0.85 (2)
wherein T is a peak value (g/d) of a thermal stress, and S is a thermal stress (g/d) at 100° C., and being wound into a cheese-like package.

### Claim 10 (depends on 9)

The polyester fiber according to claim 9, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 11

A cheese-like package which is formed by winding a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of the thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2), and which shows a bulging rate of 10% or less:
0.18≦Q/R≦0.45 (1) 0.2≦S/T≦0.85 (2)
wherein T is a peak value (g/d) of a thermal stress, and S is a thermal stress (g/d) at 100° C.

### Claim 12 (depends on 11)

The cheese-like package according to claim 11, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 13

A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solid filaments, winding the solidified filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.

### Claim 14

A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising passing molten filaments extruded from a spinning nozzle through a retarded cooling zone 2 to 80 cm long provided directly below the spinning nozzle and held at atmospheric temperatures of 30 to 200° C., whereby rapid cooling of the filaments is suppressed, rapidly cooling the molten filaments to be changed into solidified filaments, winding the solidified filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.

### Claim 15

A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solidified filaments, winding the solid filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, cooling the fiber with a third roll, and winding the fiber on a winder having a peripheral speed lower than that of the second roll.

### Claim 16

A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solidified filaments, imparting a finishing agent to the fiber, whereby the lubricant amount becomes from 0.2 to 3% by weight, winding the solid filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.

### Claim 17

A fabric partly or entirely formed with a polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
0.18≦Q/R≦0.45 (1)

### Claim 18 (depends on 17)

The fabric according to claim 17, wherein the peak value of the thermal stress is from 0.1 to 0.25 g/d, and the elongation is from 35 to 50%.

### Claim 19

A fabric partly or entirely formed with a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of a thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):
0.18≦Q/R≦0.45 (1) 0.2≦S/T≦0.85 (2)
wherein T is a peak value (g/d) of a thermal stress, and S is a thermal stress (g/d) at 100° C.

### Claim 20 (depends on 19)

The fabric according to claim 19, wherein the peak value of the thermal stress of the fiber used is from 0.1 to 0.25 g/d, and the elongation is from 35% to 50%.