# US 2002/0117731 A1 · Method for forming layer for trench isolation structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0117731 A1
- Document ID: US20020117731A1
- Status: Published application
- Kind: A1
- Application number: 10/083,756
- Filed: 2002-02-25
- Published: 2002-08-29
- Earliest claimed: 2001-02-23
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Do-Hyung Kim; Sung-Eui Kim
- Web page: https://patentgrep.com/patent/US20020117731A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a thermal oxide layer on the surface of a semiconductor substrate exposed during a semiconductor fabricating process. The thermal oxide layer is to be thin to minimize silicon substrate defects caused by volume expansion. A chemical vapor deposition (CVD) layer is then formed on the thin thermal oxide layer, creating a required thickness. The thin thermal oxide layer and the CVD material layer are formed in the same CVD apparatus. As a result, a process can be simplified and a particle-leading pollution can be prevented.

## Claims

### Claim 1

A method for forming an oxide layer in an integrated circuit device process, comprising:
growing a thermal oxide layer on a surface of a semiconductor substrate in a chemical vapor deposition (CVD) apparatus; and
forming a CVD material layer on the thermal oxide layer in the CVD apparatus.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermal oxide layer is formed to a thickness of approximately 20 Å to 100 Å.

### Claim 3 (depends on 1)

The method of claim 1, wherein the CVD material layer is formed of a material selected from the group consisting of silicon oxide, aluminum oxide, zirconium oxide, and tantalum oxide.

### Claim 4 (depends on 1)

The method of claim 1, further comprising: forming another material layer on the CVD material layer in the CVD apparatus.

### Claim 5 (depends on 1)

The method of claim 1, wherein growing a thermal oxide layer comprises using O2, N2O or a combination thereof for an oxidizing ambient.

### Claim 6 (depends on 1)

The method of claim 1, wherein growing a thermal oxide layer is carried out at a temperature of approximately 750° C. to 1000° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein growing a thermal oxide layer is carried out at a temperature of approximately 750° C. to 1000° C. and forming a CVD material layer is carried out at a temperature of approximately 700° C. to 850° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the surface of the semiconductor substrate comprises a bottom and a sidewall of a trench formed by etching the substrate to a predetermined depth; and
wherein the thermal oxide layer is formed to a thickness of approximately 20 Å to 100 Å, and the CVD material layer is formed to a thickness of approximately 50 Å to 400 Å.

### Claim 9 (depends on 8)

The method of claim 8, wherein the CVD material layer is formed of a material selected from the group consisting of silicon oxide, aluminum oxide, zirconium oxide, and tantalum oxide.

### Claim 10 (depends on 8)

The method of claim 8, wherein growing a thermal oxide layer uses O2, N2O or a combination thereof as a source gas at a temperature of approximately 750° C. to 1000° C., and forming a CVD material layer is carried out using N2O and SiH4 as source gases at a temperature of approximately 700° C. to 850° C.

### Claim 11 (depends on 8)

The method of claim 8, further comprising: forming a nitride liner layer on the CVD material layer in the CVD apparatus to a thickness of approximately 30 Å to 100 Å, and forming a trench filling layer on the nitride liner layer in the CVD apparatus to a thickness of approximately 3000 Å to 10000 Å.

### Claim 12

A method of forming an oxide layer in an integrated circuit device process, comprising:
forming a thermal oxide layer on an exposed single crystalline silicon substrate in a chemical vapor deposition (CVD) apparatus; and
forming a CVD material layer on the thermal oxide layer in the CVD apparatus.

### Claim 13 (depends on 12)

The method of claim 12, wherein forming a thermal oxide layer is carried out at a temperature of approximately 750° C. to 1000° C., and forming a CVD material layer is carried out at a temperature of approximately 700° C. to 850° C.

### Claim 14 (depends on 13)

The method of claim 13, wherein O2, N2O or combination thereof is used as a source gas for forming a thermal oxide layer, and N2O and SiH4 are used as a source gas for forming a CVD material layer.

### Claim 15

A method of forming a layer for an integrated circuit device, comprising:
forming a trench in a single crystalline silicon substrate by etching;
forming a thermal oxide layer on a surface of the trench;
forming a conformal liner material layer on the thermal oxide layer; and
forming a nitride liner layer on the conformal liner material layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the thermal oxide layer is formed to a thickness of 20 Å to 100 Å.

### Claim 17 (depends on 15)

The method of claim 15, wherein the liner material layer is formed to a thickness of 50 Å to 400 Å.

### Claim 18 (depends on 15)

The method of claim 15, wherein the liner material layer is made of a material selected from the group consisting of silicon dioxide, aluminum trioxide, zirconium oxide, and tantalum pentoxide.

### Claim 19 (depends on 15)

The method of claim 15, wherein the thermal oxide layer, the liner material layer, and the nitride liner layer are formed in the same chemical vapor deposition (CVD) apparatus.

### Claim 20 (depends on 19)

The method of claim 19, wherein the thermal oxide layer is formed using O2, N2O or a combination thereof as a source gas at a temperature of approximately 750° C. to 1000° C., and the liner material layer is a high temperature oxide layer formed using N2O and SiH4 as a source gas at a temperature of approximately 700° C. to 850° C.

### Claim 21 (depends on 20)

The method of claim 20, further comprising: forming a trench isolation material on the nitride liner layer in the same CVD apparatus to fill the trench.

### Claim 22

A method of forming an isolation trench, comprising,
etching a single crystalline silicon substrate to form a trench therein; and
forming all layers, formed in the trench, in the trench in the same chemical vapor deposition (CVD) apparatus.

### Claim 23 (depends on 22)

The method of claim 22, wherein said all layers include a thermal oxide layer formed directly following formation of the trench, a liner material barrier layer formed on the thermal oxide layer, a nitride liner layer formed on the liner material barrier layer, and a trench isolation material layer formed on the nitride liner layer to fill the trench.

### Claim 24 (depends on 23)

The method of claim 23, wherein the thermal oxide layer is formed to a thickness of 20 Å to 100 Å, and the liner material barrier layer is formed to a thickness of 50 Å to 400 Å.

### Claim 25 (depends on 23)

The method of claim 23, wherein the thermal oxide layer is formed using O2, N2O or a combination thereof as a source gas at a temperature of approximately 750° C. to 1000° C., and the liner material layer is a higher temperature oxide layer formed using N2O and SiH4 as a source gas at a temperature of approximately 700° C. to 850° C.

### Claim 26 (depends on 23)

The method of claim 23, wherein the liner material layer is made of a material selected from the group consisting of silicon oxide, aluminum oxide, zirconium oxide, and tantalum oxide.

### Claim 27

A trench isolation structure comprising:
a trench for device isolation formed in a semiconductor substrate to a predetermined depth;
a thermal oxide layer formed on a bottom and a sidewall of the trench to a thickness of 20 Å to 100 Å;
a chemical vapor deposition (CVD) material barrier layer formed on the thermal oxide layer to a thickness of 50 Å to 400 Å;
a nitride liner layer formed on the CVD material barrier layer; and
a trench isolation material layer formed on the nitride liner layer to fill up the trench.

### Claim 28 (depends on 27)

The trench isolation structure of claim 27, wherein thermal oxide layer and the CVD material barrier layer are formed in the same CVD apparatus, and the CVD material barrier layer is made of aluminum oxide.