# US 2002/0117470 A1 · Method for controlling the sheet resistance of thin film resistors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0117470 A1
- Document ID: US20020117470A1
- Status: Published application
- Kind: A1
- Application number: 09/793,252
- Filed: 2001-02-26
- Published: 2002-08-29
- Earliest claimed: 2001-02-26
- Assignees: TRW Inc.
- Inventors: Michael D. Lammert
- Web page: https://patentgrep.com/patent/US20020117470A1

## CPC

- H01C 17/2404: {by charged particle impact, e.g. by electron or ion beam milling, sputtering, plasma etching}
- H01C 17/24: by removing or adding resistive material (H01C17/23, H01C17/232, H01C17/235 take precedence)
- H10D 1/474: {comprising refractory metals, transition metals, noble metals, metal compounds or metal alloys, e.g. silicides}
- H01C: RESISTORS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for controlling the sheet resistance of thin film resistors. The sheet resistance can be inexpensively controlled within a tight tolerance by determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate, depositing the resistor material on the substrate using a deposition process which is consistent enough to achieve a target sheet resistance within a first specified tolerance, the resistor material being deposited to achieve a target sheet resistance which is equal to the desired final value minus the first specified tolerance, and removing a small amount of material from the surface of the deposited thin film resistor material by etching or ion bombardment to raise the sheet resistance to the desired final value within a second specified tolerance characteristic of the removing process where the second specified tolerance is less than the first specified tolerance.

## Claims

### Claim 1

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising, after said depositing, measuring the sheet resistance of said deposited thin film resistor material, determining the thickness of said deposited thin film resistor material, calculating the thickness of said deposited thin film resistor material needed to be removed to raise the sheet resistance thereof to said desired final value, and calculating the time for performing said removing process to remove said calculated thickness based on a measured removal rate for said removing process.

### Claim 3 (depends on 2)

The method according to claim 2, wherein said determining the thickness of said deposited thin film resistor material is accomplished by measuring the deposited thin film resistor material.

### Claim 4 (depends on 2)

The method according to claim 2, wherein said determining the thickness of said deposited thin film resistor material is accomplished by calculation using said measured sheet resistance and a reference characteristic for said material relating thickness and sheet resistance.

### Claim 5

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material uniformly from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance.

### Claim 6

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance,
removing a small amount of material uniformly from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance, and
patterning a thin film resistor from said thin film resistor material on said substrate.

### Claim 7 (depends on 6)

The method according to claim 6, wherein said patterning is done before the sheet resistance is raised to said desired final value.

### Claim 8 (depends on 6)

The method according to claim 6, wherein said patterning is done after the sheet resistance is raised to said desired final value.

### Claim 9

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate,
depositing said thin film resistor material on said substrate using a deposition process selected from the group consisting of evaporation and sputter deposition which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance.

### Claim 10 (depends on 1)

The method according to claim 1, wherein said small amount of material is removed uniformly from said surface of the deposited thin film resistor material in a time within the range of from about 10 seconds to several minutes.

### Claim 11

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a GaAs integrated circuit substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance.

### Claim 12

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on an InP integrated circuit substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material from the surface of the deposited thin film resistor material by one of an etching and ion bombardment removing process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, said second specified tolerance being less than said first specified tolerance.

### Claim 13

A method for controlling the sheet resistance of thin film resistors, comprising:
determining a desired final value for the sheet resistance of thin film resistor material to be deposited on a substrate,
depositing said thin film resistor material on said substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to said desired final value minus said first specified tolerance, and
removing a small amount of material from the surface of the deposited thin film resistor material by an Argon sputter etching process to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said etching process, said second specified tolerance being less than said first specified tolerance.

### Claim 14

A method for controlling the sheet resistance of thin film resistors, comprising:
depositing a thin film resistor material on a substrate using a deposition process which is consistent enough to achieve a target sheet resistance for the deposited thin film resistor material within a first specified tolerance, said thin film resistor material being deposited by said deposition process to achieve a target sheet resistance which is equal to a desired final value for the sheet resistance minus said first specified tolerance,
measuring the sheet resistance of said deposited thin film resistor material,
determining the thickness of said deposited thin film resistor material,
calculating the thickness of said deposited thin film resistor material needed to be removed to raise the sheet resistance thereof to said desired final value,
calculating the time for performing one of an etching and ion bombardment removing process to remove said calculated thickness based on a measured removal rate for said removing process, and
performing said removing process for said calculated time to remove said calculated thickness of said deposited resistor material needed to be removed to raise the sheet resistance to said desired final value within a second specified tolerance characteristic of said removing process, where said second specified tolerance is less than said first specified tolerance.