# US 2002/0117086 A1 · Low shrinkage, high strength cellular lightweight concrete

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0117086 A1
- Document ID: US20020117086A1
- Status: Published application
- Kind: A1
- Application number: 10/050,248
- Filed: 2002-01-16
- Published: 2002-08-29
- Earliest claimed: 2000-12-19
- Inventors: Caijun Shi; Yanzhong Wu; Monte Riefler
- Web page: https://patentgrep.com/patent/US20020117086A1

## CPC

- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 2111/34: Non-shrinking or non-cracking materials
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

An economical structural cellular lightweight concrete with a density of from about 45 lb/ft3 to about 90 lb/ft3 and a strength from about 1,000 psi to about 6,000 psi after 28 days of curing at room temperature and with minimal shrinkage on drying, is described. The concrete comprises cement, lightweight aggregate with a density from about 25 lb/ft3 to about 60 lb/ft3, fiber, superplastizer, gas and/or foaming agents, and a shrinkage reducing agent. The concrete can be manufactured using facilities for conventional concrete even with a portion of Portland cement replaced by industrial by-products or recycled materials such as blast furnace slag, coal fly ash and recycled glasses. The preferred procedure for making the lightweight concrete is also described. The products made with the lightweight concrete have much better ductility and construction capabilities than conventional concrete products.

## Claims

### Claim 1

A cellular structural lightweight concrete comprising, by weight:
a) about 30% to about 45% cementing material;
b) about 20% to about 55% aggregate;
c) about 0.02% to 5% fiber;
d) a lime containing material;
e) a shrinkage reducing agent;
f) about 0.001% to 1.0% of a gas-forming agent or a foaming agent; and,
g) about 12% to 30% water.

### Claim 2 (depends on 1)

The concrete of claim 1 having a dry density from about 45 lb/ft3 to about 90 lb/ft3.

### Claim 3 (depends on 1)

The concrete of claim 1 wherein a compressive strength of the concrete is from about 1,000 psi to about 6,000 psi after 28 days of curing at room temperature.

### Claim 4 (depends on 1)

The concrete of claim 1 wherein the cementing material includes Portland cement.

### Claim 5 (depends on 1)

The concrete of claim 1 wherein the cementing material has either cementitious or pozzolanic properties and is selected from the group consisting of coal fly ash, natural pozzolan, ground blast furnace slag, ground steel slag, silica fume, and mixtures thereof.

### Claim 6 (depends on 1)

The concrete of claim 1 wherein the aggregate is selected from the group consisting of volcanic ash, pumice, scoria, tuff, and expanded, palletized or sintered blast furnace slag, clay, diatomite, fly ash, shale, perlite, vermiculite, slate, and mixtures thereof.

### Claim 7 (depends on 1)

The concrete of claim 1 wherein the aggregate includes both fine and coarse aggregate.

### Claim 8 (depends on 1)

The concrete of claim 1 wherein the aggregate has a density between 25 lb/ft3 to 60 lb/ft3.

### Claim 9 (depends on 1)

The concrete of claim 1 wherein the lime containing material is selected from the group consisting of quick lime, hydrated lime, and any material containing at least 50% free CaO.

### Claim 10 (depends on 1)

The concrete of claim 1 wherein the shrinkage reducing agent is selected from the group consisting of at least one alkyl ether oxyalkylene adduct represented by the formula: RO (AO)nH, wherein A is a C2-4 alkylene radical, O is an oxygen atom, R is a tertiary alkyl group and n is an integer from 1 to 3, and an oxyalkylene glycol represented by the formula: HO(AO)mH, wherein A is a C2-4 alkylene radical, O is an oxygen atom, and m is an integer of 1 to 3.

### Claim 11 (depends on 1)

The concrete of claim 1 wherein the shrinkage reducing agent comprises an alkyl ether oxyalkylene adduct and a tertiary alkyl group in a weight ratio of about 1:1.

### Claim 12 (depends on 1)

The concrete of claim 1 wherein the shrinkage reducing agent is present in a concentration about 0.01% to about 3%, by weight.

### Claim 13 (depends on 1)

The concrete of claim 1 wherein the gas-forming agent is selected from the group consisting of aluminum powder, zinc powder, magnesium powder, aluminum sulfate, and mixtures thereof.

### Claim 14 (depends on 1)

The concrete of claim 1 wherein the foaming agent is an alkaline salt selected from the group consisting of natural wood resins, fatty acids, sulfonated organic compounds, and mixtures thereof.

### Claim 15 (depends on 1)

The concrete of claim 1 further including fibers selected from the group consisting of nylon fibers, polypropylene fibers, carbon fibers, cellulose fibers, and mixtures thereof.

### Claim 16 (depends on 15)

The concrete of claim 15 wherein the fiber is present in a concentration of about 0.02% to about 5%, by weight.

### Claim 17 (depends on 1)

The concrete of claim 1 further comprising a superplasticizer as a linear polymer containing sulfonic acid groups attached to the polymer backbone at regular intervals.

### Claim 18 (depends on 17)

The concrete of claim 17 wherein the superplastizer is selected from the group consisting of sulfonated melamine-formaldehyde condensates (SMF), sulfonated naphthalene-formaldehyde condensates (SNF), modified lignosulfonates (MLS), polycarboxylate derivatives, and mixtures thereof.

### Claim 19 (depends on 17)

The concrete of claim 17 wherein the superplastizer is present in a concentration of about 0.02% to about 1%, by weight.

### Claim 20

A method for making cellular concrete product using a cellular concrete mixture, comprising the steps of:
a) mixing, by weight, about 30% to about 45% cementing material with about 20% to about 55% aggregate, a lime containing material, about 0.02% to 5% fiber, about 0.01% to about 3% of a shrinkage reducing agent, about 0.001% to 1.0% of a gas-forming agent or foaming agent, and about 12% to 30% water to provide a concrete mixture;
b) pouring the concrete mixture to partially fill the total volume of a form;
c) allowing the poured concrete mixture to expand to the total volume of the form;
d) allowing the expanded concrete to set;
e) curing the set concrete in a moist environment; and
f) utilizing the cured concrete.

### Claim 21 (depends on 20)

The method of claim 20 including providing the concrete having a dry density from about 45 lb/ft3 to about 90 lb/ft3.

### Claim 22 (depends on 20)

The method of claim 20 including providing the concrete having a compressive strength of from about 1,000 psi to about 6,000 psi after about 28 days of curing at room temperature.

### Claim 23 (depends on 20)

The method of claim 20 including providing the cement as Portland cement.

### Claim 24 (depends on 20)

The method of claim 20 including providing the cementing material having either cementitious or pozzolanic properties and being selected from the group consisting of coal fly ash, natural pozzolan, ground blast furnace slag, ground steel slag, silica fume, and mixture thereof.

### Claim 25 (depends on 20)

The method of claim 20 including selecting the aggregate from the group consisting of pumice, scoria, tuff, and expanded blast furnace slag, palletized blast furnace slag, sintered blast furnace slag, clay, diatomite, fly ash, shale, perlite, vermiculate, slate, and mixtures thereof.

### Claim 26 (depends on 20)

The method of claim 20 including providing the lightweight aggregate as either fine or coarse aggregate.

### Claim 27 (depends on 20)

The method of claim 20 including providing the aggregate having a density of from about 25 lb/ft3 to about 60 lb/ft3.

### Claim 28 (depends on 20)

The method of claim 20 including selecting the lime containing material from the group consisting of quick lime, hydrated lime and any material containing at least 50% free CaO.

### Claim 29 (depends on 20)

The method of claim 20 including selecting the shrinkage reducing agent from the group consisting of at least one alkyl ether oxyalkylene adduct represented by the formula: RO(AO)nH, wherein A is a C2-4 alkylene radical, O is an oxygen atom, R is a tertiary alkyl group and n is an integer from 1 to 3, and an oxyalkylene glycol represented by the formula: HO(AO)mH, wherein A is a C2-4 alkylene radical, O is an oxygen atom, and m is an integer of 1 to 3.

### Claim 30 (depends on 20)

The method of claim 20 including providing the shrinkage reducing agent in a concentration from about 0.01% to about 3%, by weight.

### Claim 31 (depends on 20)

The method of claim 20 including selecting the gas forming agent from the group consisting of aluminum powder, zinc powder, magnesium powder, aluminum sulfate, and mixtures thereof.

### Claim 32 (depends on 20)

The method of claim 20 including providing the foaming agent as an alkali salt selected from the group consisting of natural wood resins, fatty acids, sulfonated organic compounds, and mixtures thereof.

### Claim 33 (depends on 20)

The method of claim 20 further including providing the concrete comprising fibers selected from the group consisting of nylon fibers, polypropylene fibers, carbon fibers, cellulose fibers, and mixtures thereof.

### Claim 34 (depends on 33)

The method of claim 33 including providing the fiber in a concentration of about 0.02% to about 5%, by weight.

### Claim 35 (depends on 20)

The method of claim 20 further including mixing a superplasticizer of a linear polymer containing sulfonic acid groups attached to the polymer backbone at regular intervals.

### Claim 36 (depends on 35)

The method of claim 35 including selecting the superplastizer from the group consisting of sulfonated melamine-formaldehyde condensates (SMF), sulfonated naphthalene-formaldehyde condensates (SNF), modified lignosulfonates (MLS), polycarboxylate derivatives, and mixtures thereof into the concrete mixture

### Claim 37 (depends on 35)

The method of claim 35 including providing the superplastizer in a concentration of about 0.02% to about 1%, by weight.