# US 2002/0100998 A1 · Plastic closure with compression molded barrier liner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0100998 A1
- Document ID: US20020100998A1
- Status: Published application
- Kind: A1
- Application number: 10/068,744
- Filed: 2002-02-05
- Published: 2002-08-01
- Earliest claimed: 1997-12-24
- Assignees: Owens-Illinois Closure Inc.
- Inventors: Mark R. Hock; David B. Riffer
- Web page: https://patentgrep.com/patent/US20020100998A1

## CPC

- B29C 43/18: incorporating preformed parts or layers, e.g. compression moulding around inserts or for coating articles {(B29C43/206 takes precedence)}
- B65D 41/045: {Discs (B65D41/0457 takes precedence)}
- C09K 3/10: {Materials in mouldable or extrudable form} for sealing or packing joints or covers (filling pastes C09D5/34)
- B29C 43/184: {shaped by the compression of the material during moulding}
- B29L 2031/565: {for containers}
- C09K 2200/047: Amides, imides, imines, N-oxides
- C09K 2200/062: Polyethylene
- C09K 2200/0622: Polyvinylalcohols, polyvinylacetates
- Y10S 215/02: Coatings and laminations for making of bottle caps
- Y10T 428/1379: Contains vapor or gas barrier, polymer derived from vinyl chloride or vinylidene chloride, or polymer containing a vinyl alcohol unit
- Y10T 428/1383: Vapor or gas barrier, polymer derived from vinyl chloride or vinylidene chloride, or polymer containing a vinyl alcohol unit is sandwiched between layers [continuous layer]
- Y10T 428/1386: Natural or synthetic rubber or rubber-like compound containing
- Y10T 428/214: End closure
- Y10T 428/215: Seal, gasket, or packing
- Y10T 428/24132: including grain, strips, or filamentary elements in different layers or components parallel
- Y10T 428/31913: Monoolefin polymer
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A plastic closure that includes a cap having a base with a peripheral skirt defining a cap interior and threads on the skirt for securing the closure to a container. A liner is secured to the interior of the cap, preferably by compression molding in situ. The liner preferably consists essentially of a blend of matrix polymer material, particulate barrier polymer material and compatibilizer material. The heat and pressure of compression forms the particles of barrier polymer material into platelets that are oriented essentially parallel to the plane of the closure base.

## Claims

### Claim 1

A method of making a plastic closure that comprises the steps of:
(a) providing a plastic cap that includes a base and a peripheral skirt defining a cap interior,
(b) placing within said cap interior, on said base, a mold charge that includes a blend of matrix polymer material and barrier polymer material, and
(c) compression molding said mold charge in situ within said cap interior against said base to form a liner having said barrier polymer material in the form of discrete overlapping platelets within said matrix polymer material and oriented essentially parallel to said base.

### Claim 2 (depends on 1)

The method set forth in claim 1 wherein said step (b) is such that said mold charge includes a blend of said matrix polymer material, said barrier polymer material, and a compatibilizer resin material to promote adhesion between said matrix polymer material and said platelets.

### Claim 3 (depends on 2)

The method set forth in claim 2 wherein said mold charge consists essentially of said matrix polymer material, said barrier polymer material and said compatibilizer resin material.

### Claim 4 (depends on 3)

The method set forth in claim 3 wherein the amount of said barrier polymer material is in the range of about 20% to 60% by weight, said compatibilizer resin material is in the range of about 1% to 10% by weight, with the balance consisting of said matrix polymer material.

### Claim 5 (depends on 1)

The method set forth in claim 1 further including, prior to said step (b):
(d) extruding mold charge material having said matrix and barrier polymer materials therein, and
(e) severing said mold charge from said material extruded in said step (d) for placement in said cap in said step (b).

### Claim 6 (depends on 1)

The method set forth in claim 1 wherein said matrix polymer material is selected from the group consisting of thermoplastic elastomers, soft olefin polymers, and mixtures thereof.

### Claim 7 (depends on 6)

The method set forth in claim 6 wherein said matrix polymer material is a thermoplastic elastomer having a Shore A hardness of 45 to 95 and flexural modulus of 30,000 to 100,000 psi.

### Claim 8 (depends on 6)

The method set forth in claim 6 wherein said matrix polymer material is a thermoplastic elastomer selected from the group consisting of styrene block copolymers and elastomeric alloys.

### Claim 9 (depends on 6)

The method set forth in claim 6 wherein said matrix polymer material includes a olefin polymer that is selected from the group consisting of metallocene-made polyethylene, ethylene-propylene rubbers, ethylene copolymers, and mixtures thereof.

### Claim 10 (depends on 1)

The method set forth in claim 1 wherein said barrier polymer material is selected from the group consisting of EVOH, nylon, acrylonitrile copolymers, blends of EVOH and amorphous nylon, blends of EVOH and an ionomer, acrylonitrile, cyclic olefin copolymers, and blends thereof.

### Claim 11 (depends on 1)

The method set forth in claim 1 wherein said step (b) is such that said mold charge includes compatibilizer material selected from the group consisting of maleic anhydride grafted polymers, ethylene vinyl acetate grafted polymers, ethylene methyl acrylate, ionomers and blends thereof.

### Claim 12 (depends on 1)

The method set forth in claim 1 wherein said barrier polymer material comprises EVOH and said matrix polymer material comprises EVA or polypropylene/butyl rubber.

### Claim 13 (depends on 1)

The method set forth in claim 1 wherein said platelets are substantially uniformly distributed throughout said liner.

### Claim 14 (depends on 1)

The method set forth in claim 1 wherein said liner contains lubricant in the amount of about 0.5% to 2.0% by weight.

### Claim 15 (depends on 14)

The method set forth in claim 14 wherein said lubricant is in the amount of a bout 1% by weight.

### Claim 16 (depends on 14)

The method set forth in claim 14 wherein said lubricant is selected from the group consisting of fatty acid amides, fatty acid esters, microcrystalline waxes, polyethylene glycols, primary amides, secondary amides, secondary-bis amides, and blends thereof.

### Claim 17

A method of making a plastic closure that comprises the steps of:
(a) extruding plastic mold charge material that consists essentially of a blend of matrix polymer material, barrier polymer material and compatibilizer resin material to promote adhesion between said matrix and barrier polymer materials by reactive bonds or non-reactive adhesion mechanisms,
(b) severing a mold charge pellet from the mold charge material extruded in said step (a),
(c) providing a plastic cap that includes a base and a peripheral skirt defining a cap interior,
(d) placing said mold charge pellet within said cap interior, and
(e) compression molding said mold charge pellet against said base to form a liner on said base having said barrier polymer material dispersed as overlapping platelets within said matrix polymer material and oriented essentially parallel to said base.

### Claim 18 (depends on 17)

The method set forth in claim 17 wherein said matrix polymer material is selected from the group consisting of thermoplastic elastomers, soft olefin polymers, and mixtures thereof.

### Claim 19 (depends on 18)

The method set forth in claim 18 wherein said matrix polymer material is a thermoplastic elastomer having a Shore A hardness of 45 to 95 and flexural modulus of 30,000 to 100,000 psi.

### Claim 20 (depends on 18)

The method set forth in claim 18 wherein said matrix polymer material is a thermoplastic elastomer selected from the group consisting of styrene block copolymers and elastomeric alloys.

### Claim 21 (depends on 18)

The method set forth in claim 18 wherein said matrix polymer material includes a olefin polymer that is selected from the group consisting of metallocene-made polyethylene, ethylene-propylene rubbers, ethylene copolymers, and mixtures thereof.

### Claim 22 (depends on 17)

The method set forth in claim 17 wherein said barrier polymer material is selected from the group consisting of EVOH, nylon, acrylonitrile copolymers, blends of EVOH and amorphous nylon, blends of EVOH and an ionomer, acrylonitrile, cyclic olefin copolymers, and blends thereof.

### Claim 23 (depends on 17)

The method set forth in claim 17 wherein said step (a) is such that said mold charge includes compatibilizer resin material selected from the group consisting of maleic anhydride grafted polymers, ethylene vinyl acetate grafted polymers, ethylene methyl acrylate, ionomers and blends thereof.

### Claim 24 (depends on 17)

The method set forth in claim 17 wherein said barrier polymer material comprises EVOH and said matrix polymer material comprises EVA or polypropylene/butyl rubber.

### Claim 25 (depends on 17)

The method set forth in claim 17 wherein said barrier polymer material is in the range of about 20% to 60% by weight, said compatibilizer resin material is in the range of about 1% to 10% by weight, with the balance consisting of said matrix polymer material.

### Claim 26 (depends on 17)

The method set forth in claim 17 wherein said platelets are substantially uniformly distributed throughout said liner.

### Claim 27 (depends on 17)

The method set forth in claim 17 wherein said liner contains lubricant in the amount of about 0.5% to 2.0% by weight.

### Claim 28 (depends on 27)

The method set forth in claim 27 wherein said lubricant is in the amount of about 1% by weight.

### Claim 29 (depends on 27)

The method set forth in claim 27 wherein said lubricant is selected from the group consisting of fatty acid amides, fatty acid esters, microcrystalline waxes, polyethylene glycols, primary amides, secondary amides, secondary-bis amides, and blends thereof.

### Claim 30

A method of making a liner for a plastic closure that comprises the steps of:
(a) forming a pellet that consists essentially of a blend of matrix polymer material, barrier polymer material and compatibilizer resin material to promote adhesion between the matrix polymer material and the barrier polymer material, and
(b) compression molding said pellet to form a liner disk within which heat and pressure from compression molding form said barrier polymer material into discrete overlapping platelets that are oriented essentially parallel to the disk.

### Claim 31 (depends on 30)

The method set forth in claim 30 comprising the additional steps of:
(c) providing a closure cap having a base and a peripheral skirt defining a cap interior and means on said skirt for securing the cap to a container, and
(d) securing said liner disk to the interior of said cap.

### Claim 32 (depends on 31)

The method set forth in claim 31 wherein said steps (b) and (d) are carried out simultaneously by compression molding said pellet in situ on said base.

### Claim 33 (depends on 32)

The method set forth in claim 32 wherein said step (a) comprises the step of forming said pellet such that said barrier material is substantially uniformly dispersed as a discontinuous phase of discrete particles within said matrix material.

### Claim 34 (depends on 30)

The method set forth in claim 30 wherein said matrix polymer material is selected from the group consisting of thermoplastic elastomers, soft olefin polymers, and mixtures thereof.

### Claim 35 (depends on 34)

The method set forth in claim 34 wherein said matrix polymer material is a thermoplastic elastomer having a Shore A hardness of 45 to 95 and a flexural modulus of 30,000 to 100,000 psi.

### Claim 36 (depends on 34)

The method set forth in claim 34 wherein said matrix polymer material is a thermoplastic elastomer selected from the group consisting of styrene block copolymers and elastomeric alloys.

### Claim 37 (depends on 34)

The method set forth in claim 34 wherein said matrix polymer material includes an olefin polymer selected from the group consisting of metallocene-made polyethylene, ethylene-propylene rubbers, ethylene copolymers, and mixtures thereof.

### Claim 38 (depends on 30)

The method set forth in claim 30 wherein said barrier polymer material is selected from the group consisting of EVOH, nylon, acrylonitrile copolymers, blends of EVOH and amorphous nylon, blends of EVOH and an ionomer, acrylonitrile, cyclic olefin copolymers, and blends thereof.

### Claim 39 (depends on 30)

The method set forth in claim 30 wherein compatibilizer resin material is selected from the group consisting of maleic anhydride grafted polymers, ethylene vinyl acetate grafted polymers, ethylene methyl acrylate, ionomers and blends thereof.

### Claim 40 (depends on 30)

The method set forth in claim 30 wherein said barrier polymer material comprises EVOH and said matrix material comprises EVA or polypropylene/butyl rubber.

### Claim 41 (depends on 30)

The method set forth in claim 30 wherein said barrier polymer material is in the range of about 20% to 60% by weight, said compatibilizer resin material is in the range of about 1% to 10% by weight, with the balance consisting of said matrix polymer material.

### Claim 42 (depends on 30)

The method set forth in claim 30 wherein said liner has a Shore A hardness of not more than 95.

### Claim 43 (depends on 30)

The method set forth in claim 30 wherein said liner contains lubricant in the amount of about 0.5% to 2.0% by weight.

### Claim 44 (depends on 43)

The method set forth in claim 43 wherein said lubricant is in the amount of about 1% by weight.