# US 2002/0058759 A1 · Rubber composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0058759 A1
- Document ID: US20020058759A1
- Status: Published application
- Kind: A1
- Application number: 09/947,525
- Filed: 2001-09-07
- Published: 2002-05-16
- Earliest claimed: 2000-09-08
- Assignees: Jsr Corporation
- Inventors: Katsumi Oka; Toshihiro Nishimura; Fumio Tsutsumi; Yutaka Abe
- Web page: https://patentgrep.com/patent/US20020058759A1

## CPC

- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/06: having improved processability or containing aids for moulding methods
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A rubber composition comprising (a) a low molecular weight copolymer rubber which is an ethylene/α-olefin/non-conjugated diene copolymer rubber having a limiting viscosity [η] of 0.4-1.6 dl/g measured in decalin at 135° C., and an ethylene content of 40-60 wt % and (b) a high molecular weight copolymer rubber which is an ethylene/α-olefin/non-conjugated diene copolymer rubber having a Mooney viscosity (ML1+4,100° C.) of 60-150, an ethylene content of 60-80 wt %, and an iodine number of 5-35, wherein the difference between the iodine number of the low molecular weight copolymer rubber (a) and the iodine number of the high molecular weight copolymer rubber (b) is 5 or less and the ratio by weight of the low molecular weight copolymer rubber (a) and the high molecular weight copolymer rubber (b) is 50/50 to 80/20, the rubber composition having a Mooney viscosity (ML1+4,100° C.) of 20-50. The rubber composition exhibits superior roll processability and extrusion processability, excellent surface appearance and adhesiveness, can be processed easily, and produces vulcanized rubber exhibiting excellent mechanical characteristics and good low and high temperature properties.

## Claims

### Claim 1

A rubber composition comprising (a) a low molecular weight copolymer rubber which is an ethylene/α-olefin/non-conjugated diene copolymer rubber having a limiting viscosity [η] of 0.4-1.6 dl/g measured in decalin at 135° C., and an ethylene content of 40-60 wt % and (b) a high molecular weight copolymer rubber which is an ethylene/α-olefin/non-conjugated diene copolymer rubber having a Mooney viscosity (ML1+4, 100° C.) of 60-150, an ethylene content of 60-80 wt %, and an iodine number of 5-35, wherein the difference between the iodine number of the low molecular weight copolymer rubber (a) and the iodine number of the high molecular weight copolymer rubber (b) is 5 or less and the ratio by weight of the low molecular weight copolymer rubber (a) and the high molecular weight copolymer rubber (b) is 50/50 to 80/20, the rubber composition having a Mooney viscosity (ML1+4, 100° C.) of 20-50.

### Claim 2 (depends on 1)

The rubber composition according to claim 1, wherein the difference between the iodine number of the low molecular weight copolymer rubber (a) and the iodine number of the high molecular weight copolymer rubber (b) is 3 or less.

### Claim 3 (depends on 1)

The rubber composition according to claim 1, wherein the α-olefin in the low molecular weight copolymer rubber (a) or the high molecular weight copolymer rubber (b) is one or more α-olefins selected from the group consisting of propylene, 1-butene, 1-pentene, 1-hexene, 4-methyl-1-pentene, 1-heptene, 1-octene, 1-decene, 1-dodecene, 1-tetradecene, 1-hexadecene, and 1-eicosene.

### Claim 4 (depends on 1)

The rubber composition according to claim 1, wherein the α-olefin in the low molecular weight copolymer rubber (a) or the high molecular weight copolymer rubber (b) is propylene, 1-butene, or 1-octene.

### Claim 5 (depends on 1)

The rubber composition according to claim 1, wherein the non-conjugated diene in the low molecular weight copolymer rubber (a) or the high molecular weight copolymer rubber (b) is one or more non-conjugated dienes selected from the group consisting of 5-ethylidene-2-norbornene, 5-propylidene-2-norbornene, dicyclopentadiene, 5-vinyl-2-norbornene, 5-methylene-2-norbornene, 5-isopropylidene-2-norbornene, norbornadiene, 1,4-hexadiene, 4-methyl-1,4-hexadiene, 5-methyl-1,4-hexadiene, 5-methyl-1,5-heptadiene, 6-methyl-1,5-heptadiene, 6-methyl-1,7-octadiene, and 7-methyl-1,6-octadiene.

### Claim 6 (depends on 1)

The rubber composition according to claim 1, wherein the non-conjugated diene in the low molecular weight copolymer rubber (a) or the high molecular weight copolymer rubber (b) is 1,4-hexadiene, dicyclopentadiene, or 5-ethylidene-2-norbornene.

### Claim 7 (depends on 1)

A vulcanized rubber product obtained by vulcanizing the rubber composition of claim 1 using sulfur, a sulfur compound, or an organic peroxide.

### Claim 8 (depends on 7)

A vulcanized rubber product according to claim 7, wherein sulfur or a sulfur compound is used in an amount from 0.1 to 10 parts by weight for 100 parts by weight of the copolymer rubber.

### Claim 9 (depends on 1, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70)

A rubber composition comprising 30-80 wt % of the rubber composition of claim 1 and 20-70 wt % of an ethylene/α-olefin/non-conjugated diene copolymer rubber (c) having a Mooney viscosity (ML1+4, 100° C.) of 30-90, an ethylene content of 45-60 wt %, and an iodine number of 5-35, provided the total of the rubber composition and the ethylene/α-olefin/non-conjugated diene copolymer rubber (c) is 100 wt %.

### Claim 10 (depends on 9)

The rubber composition according to claim 9, wherein the ethylene/α-olefin/non-conjugated diene copolymer rubber (c) is a commonly used EPDM rubber.