# US 2002/0058723 A1 · Contact lens having improved dimensional stability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0058723 A1
- Document ID: US20020058723A1
- Status: Published application
- Kind: A1
- Application number: 09/875,046
- Filed: 2001-06-07
- Published: 2002-05-16
- Earliest claimed: 1995-04-14
- Assignees: Benz Research and Development Corporation
- Inventors: Patrick H. Benz; Jose A. Ors
- Web page: https://patentgrep.com/patent/US20020058723A1

## CPC

- G02B 1/043: {Contact lenses}
- C08F 220/20: of polyhydric alcohols or phenols {, e.g. 2-hydroxyethyl (meth)acrylate or glycerol mono-(meth)acrylate}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A contact lens and a contact lens blank having increased dimensional stability are constructed from a copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate, wherein the copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate has either an absolute water balance ratio greater than 8 or a relative water balance ratio greater than 2 relative to a polymer of 2-hydroxyethyl methacrylate.

## Claims

### Claim 1

A soft contact lens having increased dimensional stability, consisting essentially of a copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate and wherein said copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate has an absolute water balance ratio greater than 8.

### Claim 2 (depends on 1)

The soft contact lens having increased dimensional stability according to claim 1, wherein said 2,3-dihydroxypropyl methacrylate is purified by distillation prior to incorporation in said copolymer.

### Claim 3 (depends on 1)

The soft contact lens having increased dimensional stability according to claim 1, wherein 2,3--dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 10:90 to 99:1.

### Claim 4 (depends on 3)

The soft contact lens having increased dimensional stability according to claim 3, wherein 2,3--dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 20:80 to 90:10.

### Claim 5 (depends on 4)

The soft contact lens having increased dimensional stability according to claim 4, wherein 2,3--dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 40:60 to 90:10.

### Claim 6 (depends on 1)

The soft contact lens having increased dimensional stability according to claim 1, wherein said soft contact lens is a spheric lens.

### Claim 7 (depends on 1)

The soft contact lens having increased dimensional stability according to claim 1, wherein said soft contact lens is a toric lens.

### Claim 8 (depends on 1)

The soft contact lens having increased dimensional stability according to claim 1, wherein said soft contact lens is a multifocal lens.

### Claim 9

A process for forming a soft contact lens having increased dimensional stability comprising:
(A) providing a polymerization reaction mixture which consists essentially of 2,3-dihydroxypropyl methacrylate as a monomer with 2-hydroxyethyl methacrylate as a comonomer;
(B) polymerizing said reaction mixture to form a copolymer;
(C) mechanically forming an optical contact lens from said polymer; and
(D) hydrating said lens subsequent to mechanical formation
to furnish a soft contact lens having an absolute water balance ratio greater than 8.

### Claim 10 (depends on 9)

The process for forming a soft contact lens having increased dimensional stability according to claim 9, wherein said 2,3-dihydroxypropyl methacrylate is purified by distillation prior to incorporation in said copolymer.

### Claim 11 (depends on 9)

The process for forming a soft contact lens having increased dimensional stability according to claim 9, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 10:90 to 99:1.

### Claim 12 (depends on 11)

The process for forming a soft contact lens having increased dimensional stability according to claim 11, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 20:80 to 90:10.

### Claim 13 (depends on 11)

The process for forming a soft contact lens having increased dimensional stability according to claim 11, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 40:60 to 90:10.

### Claim 14 (depends on 9)

The process for forming a soft contact lens having increased dimensional stability according to claim 9, wherein said soft contact lens is a spheric lens.

### Claim 15 (depends on 9)

The process for forming a soft contact lens having increased dimensional stability according to claim 9, wherein said soft contact lens is a toric lens.

### Claim 16 (depends on 9)

The process for forming a soft contact lens having increased dimensional stability according to claim 9, wherein said soft contact lens is a multifocal lens.

### Claim 17

A soft contact lens blank having increased dimensional stability, consisting essentially of a copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate and wherein said copolymer of 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate has a relative water balance ratio greater than 2 relative to a polymer of 2-hydroxyethyl methacrylate.

### Claim 18 (depends on 17)

The soft contact lens blank having increased dimensional stability according to claim 17, wherein said 2,3-dihydroxypropyl methacrylate is purified by distillation prior to incorporation in said copolymer.

### Claim 19 (depends on 17)

The soft contact lens blank having increased dimensional stability according to claim 17, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 10:90 to 99:1.

### Claim 20 (depends on 19)

The soft contact lens blank having increased dimensional stability according to claim 19, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 20:80 to 90:10.

### Claim 21 (depends on 20)

The soft contact lens blank having increased dimensional stability according to claim 20, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 40:60 to 90:10.

### Claim 22 (depends on 17)

The soft contact lens blank having increased dimensional stability according to claim 17, wherein said soft contact lens is a spheric lens.

### Claim 23 (depends on 17)

The soft contact lens blank having increased dimensional stability according to claim 17, wherein said soft contact lens is a toric lens.

### Claim 24 (depends on 17)

The soft contact lens blank having increased dimensional stability according to claim 17, wherein said soft contact lens is a multifocal lens.

### Claim 25

A process for forming a soft contact lens blank having increased dimensional stability comprising:
(A) providing a polymerization reaction mixture which consists essentially of 2,3-dihydroxypropyl methacrylate as a monomer with 2-hydroxyethyl methacrylate as a comonomer;
(B) polymerizing said reaction mixture to form a copolymer; and
(C) mechanically forming an optical contact lens blank from said polymer
to furnish a soft contact lens blank having a relative water balance ratio greater than 2 relative to a polymer of 2-hydroxyethyl methacrylate.

### Claim 26 (depends on 25)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 25, wherein said 2,3-dihydroxypropyl methacrylate is purified by distillation prior to incorporation in said copolymer.

### Claim 27 (depends on 25)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 25, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 10:90 to 99:1.

### Claim 28 (depends on 27)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 27, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 20:80 to 90:10.

### Claim 29 (depends on 28)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 28, wherein-2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 40:60 to 90:10.

### Claim 30 (depends on 25)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 25, wherein said soft contact lens is a spheric lens.

### Claim 31 (depends on 25)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 25, wherein said soft contact lens is a toric lens.

### Claim 32 (depends on 25)

The process for forming a soft contact lens blank having increased dimensional stability according to claim 25, wherein said soft contact lens is a multifocal lens.

### Claim 33

A process for forming a molded or partially molded soft contact lens having increased dimensional stability, comprising the steps of:
(A) providing a polymerization reaction mixture which consists essentially of 2,3-dihydroxypropyl methacrylate as a monomer with 2-hydroxyethyl methacrylate as a comonomer;
(B) polymerizing said reaction mixture in a mold to form a copolymer optical contact lens or partial contact lens; and
(C) hydrating said lens subsequent to said forming step
to furnish a soft contact lens having an absolute water balance ratio greater than 8.

### Claim 34 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein said 2,3-dihydroxypropyl methacrylate is purified by distillation prior to incorporation in said copolymer.

### Claim 35 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 10:90 to 99:1.

### Claim 36 (depends on 35)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 35, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 20:80 to 90:10.

### Claim 37 (depends on 35)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 35, wherein 2,3-dihydroxypropyl methacrylate and 2-hydroxyethyl methacrylate are present in a molar ratio of from 40:60 to 90:10.

### Claim 38 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein said soft contact lens is a spheric lens.

### Claim 39 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein said soft contact lens is a toric lens.

### Claim 40 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein said soft contact lens is a multifocal lens.

### Claim 41 (depends on 33)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 33, wherein said polymerizing step completely forms an optical contact lens.

### Claim 42 (depends on 41)

The process for forming a molded or partially molded soft contact lens having increased dimensional stability according to claim 41, wherein said polymerizing step partially forms an optical contact lens, said process further comprising the step of mechanically forming a remainder of said optical contact lens.