# US 2002/0058425 A1 · Method of structuring a photoresist layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0058425 A1
- Document ID: US20020058425A1
- Status: Published application
- Kind: A1
- Application number: 09/999,323
- Filed: 2001-10-31
- Published: 2002-05-16
- Earliest claimed: 2000-10-31
- Assignees: Infineon Technologies AG
- Inventors: Ernst-Christian Richter; Michael Sebald
- Web page: https://patentgrep.com/patent/US20020058425A1

## CPC

- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/0392: {the macromolecular compound being present in a chemically amplified positive photoresist composition}
- H10P 76/204: {of organic photoresist masks}
- G03F 7/0046: {with perfluoro compounds, e.g. for dry lithography (G03F7/0048 takes precedence)}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method structures a chemical amplification photoresist layer, in which a photoresist layer of the chemically amplified type is brought into contact, before or after the exposure for structuring, with a base which is capable of diffusing into the photoresist layer. As a result of this treatment with the base, greater steepness and less roughness of the resist profiles are achieved in the subsequent development step.

## Claims

### Claim 1

A method of structuring a photoresist layer, which comprises:
providing a substrate;
applying a photoresist layer at least partially to the substrate; the photoresist layer including a film-forming polymer having molecular groups convertible into alkali-soluble groups at a given temperature by acid-catalyzed cleavage reactions, and including a photosensitive acid generator for liberating an acid when exposed to light in a defined wavelength range;
partially exposing the photoresist layer to light in the defined wavelength range;
contacting the photoresist layer with a base over a specific period;
allowing the base to diffuse into the photoresist layer; heating the photoresist layer to the given temperature to cause the cleavage reaction catalyzed by the photolytically produced acid; and
developing the photoresist layer.

### Claim 2 (depends on 1)

The method according to claim 1, whrein the contacting step comprises covering the photoresist layer with a liquid including the base in order to contact the photoresist layer with the base.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the contacting step comprises exposing the photoresist layer to a gas including the base in order to contact the photoresist layer with the base.

### Claim 4 (depends on 3)

The method according to claim 3, which further comprises including in the gas an inert carrier gas selected from the group consisting of noble gases and nitrogen.

### Claim 5 (depends on 4)

The method according to claim 4, which further comprises selecting the noble gases from the group consisting of helium and argon.

### Claim 6 (depends on 1)

The method according to claim 1, which further comprises utilizing an amine as the base.

### Claim 7 (depends on 6)

The method according to claim 6, which further comprises selecting the amine from the group consisting of ammonia, methylamine, ethylamine, dimethylamine, diethylamine, hexylamine, tripentylamine, 1,5-diaminopentane, N-methyl-2-pyrrolidone, and 1,1,1,3,3,3-hexamethyldisilazane.

### Claim 8 (depends on 1)

The method according to claim 1, which further comprises using as the base a salt having the general structure according to formula I
4
in which R1, R2, R3, and R4, independently of one another, are selected from the group consisting of hydrogen, methyl, ethyl, propyl, and butyl.

### Claim 9 (depends on 1)

The method according to claim 1, which further comprises using tetramethylammonium hydroxide as the base.

### Claim 10 (depends on 1)

The method according to claim 1, which comprises heating the photoresist layer to a temperature between 80 and 250° C.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the photosensitive acid generator liberates an acid when exposed to UV light having a wavelength of from 150 to 300 nm, and the partially exposing of the photoresist layer is to light having a wavelength of from 150 to 300 nm.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the photosensitive acid generator liberates an acid when exposed to UV light having a wavelength of from 300 to 450 nm, and the partially exposing of the photoresist layer is to light having a wavelength of from 300 to 450 nm.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the photosensitive acid generator liberates an acid when exposed to UV light having a wavelength of from 350 to 450 nm, and the partially exposing of the photoresist layer is to light having a wavelength of from 350 to 450 nm.

### Claim 14 (depends on 1)

The method according to claim 1, which further comprises adapting the polymer to have an adapted absorption in the wavelength range of from 150 to 450 nm, so that the photosensitive acid generator can be photochemically activated.

### Claim 15 (depends on 1)

The method according to claim 1, which further comprises selecting the photosensitive acid generator from the group consisting of onium compounds, nitrobenzyl esters, sulfones, phosphates, N-hydroximidosulfonates, and diazonaphthoquinones.

### Claim 16 (depends on 15)

The method according to claim 15, which further comprises selecting the onium compounds from the group consisting of diphenyliodonium triflate and trisulfonium nonasulfate.

### Claim 17 (depends on 15)

The method according to claim 15, which further comprises using 4-nitrobenzyl-9,10-dimethoxyanthracene 2-sulfonate as the nitrobenzyl ester.

### Claim 18 (depends on 15)

The method according to claim 15, which further comprises using phenylacyl phenyl sulfone as the sulfone.

### Claim 19 (depends on 15)

The method according to claim 15, which further comprises using triaryl phosphates as the phosphate.

### Claim 20 (depends on 15)

The method according to claim 15, which further comprises using N-hydroxyphthalimidomethanesulfonate as the N-hydroximidosulfonates.

### Claim 21 (depends on 15)

The method according to claim 15, which further comprises using 1-oxo-2-diazonaphthoquinone 5-arylsulfonate as the diazonaphthoquinones.

### Claim 22 (depends on 1)

The method according to claim 1, which further comprises selecting molecular groups in the polymer capable of participating in the acid-catalyzed cleavage reactions from the group of carboxylic esters consisting of tert-alkyl carboxylates, tetrahydrofuranyl carboxylates, and tetrahydropyranyl carboxylates.

### Claim 23 (depends on 1)

The method according to claim 1, which further comprises selecting the molecular groups in the polymer capable of participating in the acid-catalyzed cleavage reactions from the group of ethers consisting of tert-alkyl ethers, tetrahydrofuranyl ether, and tetrahydropyranyl ether.

### Claim 24 (depends on 23)

The method according to claim 23, which further comprises using tert-butyl ether as the tert-alkyl ether.

### Claim 25 (depends on 1)

The method according to claim 1, which further comprises selecting as the molecular groups in the polymer capable of participating in the acid-catalyzed cleavage reactions from the group consisting of cyclic ketals., acyclic ketals, cyclic acetals, and acyclic acetals.

### Claim 26 (depends on 1)

The method according to claim 1, wherein the molecular groups in the polymer capable of participating in the acid-catalyzed cleavage reactions have a structure according to formula II
5
in which R7 is selected from the group consisting of tert-alkyl groups, tetrahydrofuranyl, tetrahydropyranyl, tert-butoxycarbonyloxy, acetal groups, and groups having a structure according to formula III, IV, and V
6
R1, R2, and R3, independently of one another, being selected from the group consisting of methyl, ethyl, propyl, and butyl; and R4, R5 and R6, independently of one another, being selected from the group consisting of hydrogen, methyl, ethyl, propyl, and butyl, and only R4 or R5 may be hydrogen and R6 is not hydrogen.

### Claim 27 (depends on 26)

The method according to claim 26, wherein the tert-alkyl groups are tert-butyl.

### Claim 28 (depends on 26)

The method according to claim 26, wherein R1, R2, and R3 are methyl.

### Claim 29 (depends on 1)

The method according to claim 1, which further comprises including anhydride structures in the film-forming polymer.

### Claim 30 (depends on 1)

The method according to claim 1, which further comprises including succinic anhydride structures in the film-forming polymer.

### Claim 31 (depends on 1)

The method according to claim 1, which further comprises:
formulating the photoresist layer by preparing a solution including a solvent, the film-forming polymer, and the photosensitive acid generator;
applying the solution to the substrate; and
then at least partly evaporating the solvent.

### Claim 32 (depends on 31)

The method according to claim 31, which further comprises selecting the solvent from the group consisting of 1-methoxy-2-propyl acetate, cyclopentanone, cyclohexanone, butyrolactone, ethyl acetate, and mixtures of at least two of the abovementioned solvents.

### Claim 33 (depends on 31)

The method according to claim 31, which further comprises heating the to temperatures between 60 and 160° C. during the evaporating of the solvent.

### Claim 34 (depends on 31)

The method according to claim 31, which further comprises:
including from 1 to 50% by weight of film-forming polymer;
including from 0.01 to 10% by weight of photosensitive acid generator; and
including from 50 to 99% by weight of solvent.

### Claim 35 (depends on 34)

The method according to claim 34, which further comprises including from 3 to 20% total by weight of film-forming polymer.

### Claim 36 (depends on 34)

The method according to claim 34, which further comprises including from 0.1 to 1% total by weight of photosensitive acid generator.

### Claim 37 (depends on 34)

The method according to claim 34, which further comprises including from 88 to 96% total by weight of solvent.

### Claim 38 (depends on 1)

The method according to claim 1, which further comprises using a solution of 2.38% by weight of tetramethylammonium hydroxide in water for developing the photoresist resist layer.