# US 2002/0058402 A1 · Method of forming an etch stop layer during manufacturing of a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0058402 A1
- Document ID: US20020058402A1
- Status: Published application
- Kind: A1
- Application number: 09/812,347
- Filed: 2001-03-20
- Published: 2002-05-16
- Earliest claimed: 2000-11-16
- Assignees: Advanced Micro Device, Inc.
- Inventors: Karsten Wieczorek; Frederick N. Hause; Manfred Horstmann
- Web page: https://patentgrep.com/patent/US20020058402A1

## CPC

- H10D 30/0212: {using self-aligned silicidation}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10W 20/065: {by making at least a portion of the conductive part non-conductive, e.g. by oxidation}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In manufacturing a semiconductor device, an etch stop layer is formed on a cobalt silicide layer during a heat treatment when the cobalt and silicon are transformed in a low resistance phase of cobalt silicide. During a predefined time period, oxygen is added to an inert gas ambient and leads to the formation of silicon oxide on the cobalt silicide. Thus, the present invention avoids a deposition step which would otherwise be necessary for forming the silicon oxide layer on top of the cobalt suicide.

## Claims

### Claim 1

A method of forming an etch stop layer during the manufacturing of a semiconductor device, comprising the steps of:
providing a substrate having a surface in and on which the semiconductor device is to be formed;
forming at least one electrically-conductive region in the substrate, the electrically-conductive region comprising silicon;
forming a contact portion in at least a portion of the electrically-conductive region, the contact portion comprising a metal and silicon, the metal and the silicon partially forming a metal silicon compound;
starting a heat treatment in an inert gas ambient for transforming the metal and the silicon to a low resistance metal silicide phase; and
adding oxygen to the inert gas ambient in the course of the heat treatment so as to form on the metal silicide compound a silicon oxide layer, wherein the silicon oxide layer is usable as an etch stop layer for further processing during the manufacture of the semiconductor device.

### Claim 2 (depends on 1)

The method of claim 1 in which said metal is cobalt.

### Claim 3 (depends on 1)

The method of claim 1 further comprising depositing a dielectric layer over the substrate by means of low pressure chemical vapor deposition, wherein the dielectric layer comprises as a sub-layer a silicon nitride layer formed on said silicon oxide layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising etching an opening in the dielectric layer at the position of the electrically-conductive region, wherein said sub-layer acts as an etch stop.

### Claim 5 (depends on 4)

The method of claim 4, further comprising etching said sub-layer, wherein said silicon oxide layer acts as an etch stop.

### Claim 6 (depends on 5)

The method of claim 5, further comprising selectively removing said silicon oxide layers so as to expose the metal silicide.

### Claim 7 (depends on 1)

The method of claim 1, wherein said silicon oxide layer is formed to a predefined thickness that is controlled by a parameter of said heat treatment process, said parameter comprises at least one of a time interval of adding the oxygen, a concentration of the oxygen and temperature during the heat treatment.

### Claim 8 (depends on 1)

The method of claim 1, wherein said oxygen is added during the last 5-45 seconds of said heat treatment.

### Claim 9 (depends on 8)

The method of claim 8, wherein the temperature during the interval when said oxygen is added is higher than 950° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the step of forming a contact region comprises:
depositing a refractory metal on the electrically-conductive region; and
performing a rapid thermal annealing step at a first temperature;
wherein said heat treatment is carried out as a rapid thermal annealing step at a second temperature, the second temperature being higher than the first temperature.

### Claim 11 (depends on 1)

The method of claim 1, wherein depositing said dielectric layer is carried out as a batch process so as to process a plurality of said substrates simultaneously.

### Claim 12 (depends on 1)

The method of claim 1, wherein said semiconductor device to be manufactured is a MIS transistor device.

### Claim 13 (depends on 1)

The method of claim 1, wherein at least one dimension of the electrically-conductive region in a plane parallel to said surface is less than 1 μm.

### Claim 14 (depends on 13)

The method of claim 13, wherein at least said one dimension is less than 0.18 μm.