# US 2002/0055261 A1 · Method of manufacturing semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0055261 A1
- Document ID: US20020055261A1
- Status: Published application
- Kind: A1
- Application number: 09/996,918
- Filed: 2001-11-30
- Published: 2002-05-09
- Earliest claimed: 1998-03-30
- Assignees: Hitachi, Ltd.
- Inventors: Akio Nishida; Kikuo Kusukawa; Toshiaki Yamanaka; Natsuki Yokoyama; Shinichiro Kimura; Norio Suzuki; Osamu Tsuchiya; Atsushi Ogishima
- Web page: https://patentgrep.com/patent/US20020055261A1

## CPC

- H10B 12/09: {with simultaneous manufacture of the peripheral circuit region and memory cells}
- H10D 84/0135: {Manufacturing their gate conductors}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10B 12/315: {with the capacitor higher than a bit line}
- H10P 95/062: {involving a dielectric removal step}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In a method of manufacturing a semiconductor device having a memory mat portion in which an active region and a field region are formed densely, after a polishing stopper film is deposited on a semiconductor substrate, there are formed grooves by etching a polishing stopper film of a field region and the semiconductor substrate. Then, after an insulating film is deposited so as to fill the grooves, then insulating film is partly removed from the memory mat portion by etching. Under this state, the insulating film is chemically mechanically polished until the polishing stopper film is exposed. The film thickness of the polishing stopper film on the active region can be reduced, and an electrical element isolation characteristic of the field region can be improved. At the same time, upon chemical mechanical polishing, a silicon substrate can be prevented from being exposed at the central portion of the memory mat portion and the insulating film can be prevented from being left on the silicon nitride film near the outer periphery, thereby making it possible to form elements having uniform electrical characteristics on all active regions of the memory mat portion.

## Claims

### Claim 1

A method of manufacturing semiconductor devices having a memory mat region, comprising the steps of:
depositing a polishing stopper film on a semiconductor substrate;
forming grooves in a field region by etching said polishing stopper film and said semiconductor substrate;
depositing an insulating film so as to fill said grooves;
partially removing said insulating film from said memory mat region by etching; and
chemically mechanically polishing said insulating film until said polishing stopper film is exposed.

### Claim 2 (depends on 1)

A method according to claim 1, wherein corners of said insulating film surrounding said memory mat region and a plurality of pillars of said insulating film are formed within said memory mat region in the process in which said insulating film is partially removed by etching.

### Claim 3 (depends on 2)

A method according to claim 2, wherein said corners and said pillars are formed in such a manner that a volume of said insulating film that should be polished in the outside of said memory mat region and volumes of said corners and said pillars become equal to each other.

### Claim 4 (depends on 1)

A method according to claim 1, wherein said polishing stopper film is a silicon nitride film.

### Claim 5 (depends on 1)

A method according to claim 1, wherein said insulating film is a silicon oxide film.

### Claim 6 (depends on 5)

A method according to claim 5, wherein said insulating film is deposited by CDV using O3-TEOS.

### Claim 7 (depends on 5)

A method according to claim 5, wherein said insulating film is deposited by HDP.

### Claim 8

A semiconductor device manufacturing method comprising the steps of:
forming a thermal oxide film on a semiconductor substrate surface;
depositing a silicon nitride film on said thermal oxide film;
patterning said silicon nitride film in accordance with an active region;
etching said thermal oxide film and said silicon substrate with said patterned silicon nitride film used as a mask to form grooves in a field region;
depositing an insulating film;
partly etching said insulating film within said memory mat region so as to leave pillars of said insulating film in said memory mat region;
exposing said patterned silicon nitride film by chemical mechanical polishing;
removing said exposed silicon nitride film; and
forming an element on an active region by removing said thermal oxide film from said active region.

### Claim 9 (depends on 8)

A method according to claim 8, wherein said insulating film is a silicon oxide film.

### Claim 10 (depends on 9)

A method according to claim 9, wherein said insulating film is deposited by CVD using O3-TEOS.

### Claim 11 (depends on 9)

A method according to claim 9, wherein said insulating film is deposited by HDP.

### Claim 12

A method of manufacturing a semiconductor device having a memory mat region, comprising the steps of:
forming a gate insulating film on an active region of a semiconductor substrate;
depositing a material film of a gate electrode on said semiconductor substrate;
depositing a polishing stopper film on said material film;
forming a plurality of gate electrodes by patterning a laminated film of said material film and said polishing stopper film;
forming source-drain regions on both sides of said gate electrode of said active region;
forming side wall films on side surfaces of said gate electrode;
depositing an interlayer insulator so as to fill a space between said gate electrodes;
partly removing said interlayer insulator from said memory mat region by etching; and
chemically mechanically polishing said interlayer insulator until said polishing stopper film is exposed.

### Claim 13 (depends on 12)

A method according to claim 12, wherein corners of said insulating film surrounding said memory mat region and a plurality of pillars of said insulating film are formed within said memory mat region in the process in which said insulating film is partially removed by etching.

### Claim 14 (depends on 13)

A method according to claim 13, wherein said corners and said pillars are formed in such a manner that a volume of said insulating film that should be polished in the outside of said memory mat region and volumes of said corners and said pillars become equal to each other.

### Claim 15 (depends on 12)

A method according to claim 12, wherein the material film of said gate electrode is any one of a laminated film of a polycrystalline silicon film, a polycrystalline silicon film and a metal silicide film or a laminated film of a polycrystalline silicon film and a metal film.

### Claim 16 (depends on 12)

A method according to claim 12, wherein said polishing stopper film is a silicon nitride film.

### Claim 17 (depends on 12)

A method according to claim 12, wherein said insulating film is a silicon oxide film.

### Claim 18 (depends on 17)

A method according to claim 17, wherein said insulating film is deposited by CVD using O3-TEOS.

### Claim 19 (depends on 17)

A method according to claim 17, wherein said insulating film is deposited by HDP.

### Claim 20

A method of manufacturing a DRAM having a memory mat portion and a peripheral circuit portion, comprising the steps of:
forming a thermal oxide film on a semiconductor substrate surface;
depositing a first nitride film on said thermal oxide film;
patterning said first nitride film in accordance with an active region;
etching said thermal oxide film and said silicon substrate with said patterned first silicon nitride film used as a mask to form grooves in a field region;
depositing a first insulating film;
partly etching said first insulating film formed on said memory mat portion in such a manner that a plurality of pillars of said first insulating film are left within said memory mat portion;
exposing said patterned first silicon nitride film by chemical mechanical polishing; and
removing said exposed first silicon nitride film.

### Claim 21 (depends on 20)

A method according to claim 20, wherein a volume of said first insulating film in said peripheral circuit portion and a volume of said first insulating film that should be polished in said memory mat portion become equal to each other in the process in which said first insulating film is etched partly.

### Claim 22 (depends on 20)

A method according to claim 20, further comprising the steps of:
forming a gate insulating film in said active region by removing said thermal oxide film from said active region;
depositing a gate electrode material film on said semiconductor substrate;
depositing a second nitride film on said material film;
forming a plurality of gate electrodes by patterning a laminated film of said material film and said second silicon nitride film in such a manner that two gate electrodes cross at least one active region of said memory mat portion;
forming source-drain regions on both sides of said gate electrode of said active region;
depositing a third silicon nitride film on said semiconductor substrate;
leaving a third silicon nitride film on a side surface of said gate electrode by anisotropy-etching said third silicon nitride film;
depositing a second insulating film;
partly etching said second insulating film on said memory mat portion in such a manner that a plurality of pillars of said second insulating film are left within said memory mat portion;
chemically mechanically polishing said interlayer insulator until said second silicon nitride film on said gate electrode is exposed;
depositing a third insulating film;
forming a plurality of first plugs penetrating said second and third insulating films and which are connected to a source-drain region formed between two gate electrodes of each active region of said memory mat portion;
forming a metal interconnection connected to said first plugs;
depositing a fourth insulating film;
forming a plurality of second plugs penetrating said second, third and fourth insulating films and which are connected to each source-drain region formed on the outside of two gate electrodes of each active region of said memory mat portion; and
forming a capacitor connected to said second plugs.

### Claim 23

A method of manufacturing semiconductor devices having a wide active region and a narrow active region, comprising the steps of:
depositing a silicon nitride film on a semiconductor substrate;
forming grooves by etching said silicon nitride film of a field region and said semiconductor substrate;
depositing an insulating film so as to fill said grooves;
partly removing said insulating film from said wide active region by etching; and
chemically mechanically polishing said insulating film until said silicon nitride film is exposed.

### Claim 24 (depends on 23)

A method according to claim 23, wherein said insulating film is a silicon oxide film.

### Claim 25

A method of manufacturing semiconductor devices having a wide active region and a narrow active region, comprising the steps of:
forming a first thermal oxide film on a semiconductor substrate surface;
depositing a first silicon nitride film on said first thermal oxide film;
forming grooves by etching said first silicon nitride film of a field region, said first thermal oxide film and said semiconductor substrate;
forming a second thermal oxide film within said grooves;
depositing a silicon oxide film;
depositing a second silicon nitride film;
partly etching said silicon oxide film and said silicon nitride film on said wide active region in such a manner that a pillar of a laminated layer of said silicon oxide film and said second silicon nitride film are left within said wide active region;
chemically mechanically polishing said silicon oxide film until said first silicon nitride film is exposed; and
removing said exposed first silicon nitride film.